Background: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H Orthodontics composites) and two thickness of the adhesive (1mm, 2mm). The samples were prepared for each composite in which a wire was embedded; then the composite was light cured for 40 seconds and the specimens were stored in artificial saliva at 37°C in the incubator for 24 hours. The ends of the wire were drawn up and tensile force was applied through Tinius-Olsen universal testing machine until the resin failed and the results were recorded in Newton (N). Results: Statistical analysis showed that there was a highly significant difference (P ≤ 0.01) among the mean values of tensile forces of the three types of retainer wires in each thickness of composite with exception of a non significant difference (P > 0.05) between (3 braided) and (8 braided) and a non significant difference (P > 0.05) between (3 braided) and (6 coaxial) in both thickness of composite, a highly significant difference (P ≤ 0.01) between the two thickness of both composite types in each wire type and a highly significant difference (P ≤ 0.01) between the two types of composite in each wire type of both thickness of composite. Conclusion: The result of this study revealed that the 8 braided strands retainer wire shows the highest values of tensile force among the tested retainer wires, the non flowable composite demonstrates a higher tensile force than the flowable composite and increasing the thickness of composite overlying the wire increased the force required to detach the wire from the composite.
Background: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown re
... Show MoreBackground: Type 2 diabetes mellitusand chronic periodontitis hold a close relationship that has been the focus of many researches. Currently there is an appreciation to the role of adipose tissue-derived substances "the adipokines" in immune-inflammatory responses; also, there is an interest in using the simple non-invasive saliva in diagnosing and linking oral and general health problems. The current study aims to determine the periodontal health status in the chronic periodontitis patients with and without poorly or well controlled type 2 diabetes mellitus, measure the salivary levels of two adipokines "leptin and resistin", pH and flow rate and then correlate between these clinical periodontal, biochemical and physical parameters in eac
... Show Moreأن التطور العلمي الحاصل فيما يخص المجال الرياضي أرسى آفاق جديدة لمواكبة التطور الكبير في مجا ل الألعاب والفعاليات الرياضية المختلفة ,و أن تحقيق النتائج الجيدة في فعاليات العاب القوى بشكل عام والثلاثية بشكل خاص في التدريب الرياضي يتطلب إتباع الأساليب العلمية الدقيقة والموضوعية بشكل سليم ومخطط له،فضلا عنة تطبيق نظريات ومنحى جديد لمواكبة الاتجاهات الحديثة في تحقيق النتائج الجيدة للوصول إلى المستويات العالية
... Show MoreIn this paper, we made comparison among different parametric ,nonparametric and semiparametric estimators for partial linear regression model users parametric represented by ols and nonparametric methods represented by cubic smoothing spline estimator and Nadaraya-Watson estimator, we study three nonparametric regression models and samples sizes n=40,60,100,variances used σ2=0.5,1,1.5 the results for the first model show that N.W estimator for partial linear regression model(PLM) is the best followed the cubic smoothing spline estimator for (PLM),and the results of the second and the third model show that the best estimator is C.S.S.followed by N.W estimator for (PLM) ,the
... Show MoreBackground: Masseter muscle is a jaw closing muscle of the mandible involved in Para functional habits; which include lip and cheek chewing, fingernail biting, and teeth clenching or bruxism which can be classified as awake or sleep bruxism. Patients with sleep bruxism are three to four times more likely to experience jaw pain and limitation of movement than people who do not experience sleep bruxism. The aim of this study is to measure the thickness of the masseter muscle in bruxist subjects and compare it with non-bruxist subjects by using sonography. Materials and Method: Forty Iraqi subjects with age ranged (20-40) divided into two groups according to the presence of bruxism. Clinical examination was made and masseter muscle thickness
... Show MoreThis study focused on treating wastewater to remove phosphorus by adsorption onto naturaland local materials. Burned kaolin, porcelinite, bauxite and limestone were selected to be testedas adsorption materials.The adsorption isotherms were evaluated by batch experiments, studyingthe effects of pH, temperature and initial phosphorus concentration. The results showed that at pH6, temperature 20°C and 300 mg/l initial phosphorus concentration; the sorption capacity was0.61, 9, 10 and 13 mg/g at 10 h contact time, for burned kaolin, porcelanite, limestone and bauxiterespectively. As the pH increased from 2 to 10 the removal efficiency for the materials differs inbehaviour. The removal efficiency increased from 40 to 90 % for limestone, and dec
... Show MoreAim: To evaluate the effect of two bonding systems and two curing systems on sealing ability of class V composite restorative materials. Materials and methods: This study was performed in vitro on 40 caries free upper first premolar teeth. The Standardized class V cavity preparation on buccal and lin- gual surfaces of each tooth was done. Then the teeth were randomly divided into two major groups each of twenty. 40 cavities were performed on these teeth and the first group7th generation bonding agent (i Bond) were applied according to the manufacturer instructions and single increment of univer- sal composite (XRV Herculite) from kerr were applied and twenty of the cavities were cured with con- ventional light cure device (astralis-5) and t
... Show More