Background: The type of dental implant surface is one of many factors that determine the success of implant restoration. This study aimed to study the effect of mixture of nano titanium oxide with nanohydroxyapatite coating of screw shaped CPTi dental implant on bond strength at bone implant interface by torque removal test related to two healing periods (2 and 6 weeks). Materials and methods: Dip coating process was performed to get an even coating layer on CPTi screws. X-ray diffraction (XRD) analysis and microscopical examination were performed on the coating surfaces of the CPTi. The tibia of 10 white New Zealand rabbits was chosen as implantation sites. The tibia of each rabbit received two screws, one was coated with mixture of nanoTio2and nanoHA and the other was coated with nanoHA and a total of 40 screws were implanted. Torque removal test was performed to measure bond strength between implant and bone, after 2 and 6 weeks healing periods. . Results: The results revealed, that the mean removal torque recordings for the mixture of nanoTio2and nanoHA coated screws was significantly greatly than the nanoHA covered screws over the two periods of time(2and6 weeks). There was an increase in the torque value with time. Conclusion: Commercially pure titanium implant coated with mixture of nanoTio2andnanoHApresented an increasing bond strength at bone implant interface than nanoHA , after 2 and 6 weeks (20.13±4.4 N.cm , 26.47±4 N.cm. ) in comparison to nanoHA coating after 2 and 6 weeks (15.16±2.5 N.cm , 20.12±2.3 N.cm) .
Background: Several pathologies of the oral cavity have been associated with stress. Dental students need to gain assorted proficiencies as theoretical knowledge, clinical proficiencies, and interpersonal dexterity which is accompanied with high level of stress. Uric acid is the major antioxidant in saliva. The aim of this study is to assess the dental caries experience among dental students with different levels of dental environment stress in relation to physicochemical characteristics of whole unstimulated saliva.
Materials and Methods: the total sample is composed of 300 dental students (73 males, 227 female) aged 22-23 years old, from collage of dentistry / university of Baghdad, from the 4t
... Show MorePMMA (Poly methyl methacrylate) is considered one of the most commonly used materials in denture base fabrication due to its ideal properties. Although, a major problem with this resin is the frequent fractures due to heavy chewing forces which lead to early crack and fracture in clinical use. The addition of nanoparticles as filler performed in this study to enhance its selected mechanical properties. The Nano-additive effect investigated in normal circumstances and under a different temperature during water exposure. First, tests applied on the prepared samples at room temperature and then after exposure to water bath at (20, 40, 60) C° respectively. SEM, PSD, EDX were utilized for samples evaluation in this study. Flexural
... Show MoreABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreIron-Epoxy composite samples were prepared by added
different weight percentages (0, 5, 10, 15, and 20 wt %) from Iron
particles in the range of (30-40μm) as a particle size. The contents
were mixed carefully, and placed a circular dies with a diameter of
2.5 cm. Different mechanical tests (Shore D Hardness, Tensile
strength, and Impact strength ) were carried out for all samples. The
samples were immersed in water for ten weeks, and after two weeks
the samples were take-out and drying to conducting all mechanical
tests were repeated for all samples. The hardness values increased
when the Iron particle concentration increased while the Impact
strength is not affected by the increasing of Iron particles
c
Background: The incorporation of rubber has not been entirely successful because it can have detrimental effects on the transverse Strength and hence the rigidity of the denture base. Materials and methods: Zirconium oxide nanoparticales were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 3% by weight then mixed with powder using conventional procedure.(100) samples were prepared and divided into five groups according to the test performed ,Each group consisted of 20 specimens and these were subdivided into 2 groupsGroup (A): control group (10 specimens of high impact acrylic resin without zirconium oxide) and Group (B):zirconium oxide group(10 specimens of high impac
... Show MoreBackground: The purpose of the current study was to evaluate the efficacy of a new orthodontic bonding system (Beauty Ortho Bond) involving the shear bond strength in dry and wet environments, and adhesion remnant index (ARI) scores evaluation in regard to other bonding systems (Heliosit and Resilience Orthodontic Adhesives). Materials and methods: Sixty defect free extracted premolars were randomly divided into six groups of 10 teeth each, mounted in acrylic resin, three groups for a dry environment and three for a wet one. Shear bond strength test was performed with a cross head speed of 0.5 mm/min, while surfaces of enamel and bracket-adhesive-enamel surfaces were examined with stereomicroscope For ARI scores evaluation. Data were analyz
... Show MoreA simple, fast, inexpensive and sensitive method has been proposed to screen and optimize experimental factors that effecting the determination of phenylephrine hydrochloride (PHE.HCl) in pure and pharmaceutical formulations. The method is based on the development of brown-colored charge transfer (CT) complex with p-Bromanil (p-Br) in an alkaline medium (pH=9) with 1.07 min after heating at 80 °C. ‘Design of Experiments’ (DOE) employing ‘Central Composite Face Centered Design’ (CCF) and ‘Response Surface Methodology’ (RSM) were applied as an improvement to traditional ‘One Variable at Time’ (OVAT) approach to evaluate the effects of variations in selected factors (volume of 5×10-3 M p-Br, heating time, and temperature) on
... Show MoreThis investigation was undertaken to evaluate the effectiveness of using Hydrated lime as a (partial substitute) by weight of filler (lime stone powder) with five consecutive percentage namely (1.0, 1.5, 2.0, 2.5, 3.0) % by means of aggregate treatment, by introducing dry lime on dry and 2–3% Saturated surface aggregate on both wearing and binder coarse. Marshall design method, indirect tensile test and permanent deformation under repeated loading of Pneumatic repeated load system at full range of temperature (20, 40, 60) C0 were examined The study revealed that the use of 2.0% and 1.5 % of dry and wet replacement extend the pavement characteristics by improving the Marshall properties and increasing the TSR%. Finally, increase permanent
... Show MoreThree cultivars of the crop Almash (Green Indian VC6089A10, Green Indian VC6173B1319, and Black Indian Gold Star) were tested in a field experiment during the 2022 growing season in Ramadi, Anbar province, to determine the impact of spraying levels of zinc (0, 25, and 50) mg Zn L-1 and manganese (0, 30, and 60) mg Mn L-1 on some growth characteristics. The experiment was conducted using a randomized complete block design (RCBD) with three replicates, with each treatment being tested in a separate split plot. The study found that there were statistically significant differences between zinc levels, with the level giving 50 mg Zn L-1