Background: The purpose of the current study was to evaluate the efficacy of a new orthodontic bonding system (Beauty Ortho Bond) involving the shear bond strength in dry and wet environments, and adhesion remnant index (ARI) scores evaluation in regard to other bonding systems (Heliosit and Resilience Orthodontic Adhesives). Materials and methods: Sixty defect free extracted premolars were randomly divided into six groups of 10 teeth each, mounted in acrylic resin, three groups for a dry environment and three for a wet one. Shear bond strength test was performed with a cross head speed of 0.5 mm/min, while surfaces of enamel and bracket-adhesive-enamel surfaces were examined with stereomicroscope For ARI scores evaluation. Data were analyzed by one way analysis of variance, least significant difference, student's t-test, and Fisher exact test. Results: The mean shear bond strength showed highest values for Resilience adhesive followed by Beauty Ortho Bond and Heliosit adhesives respectively both in dry and wet environments. Interestingly, there was a non-significant difference (P<0.05) between Resilience and Beauty Ortho Bond adhesives using least significant difference at dry environment. In wet environment the Beauty Ortho Bond showed an acceptable mean shear bond strength value (6.39 Mpa) which is considered as a clinically acceptable value. Adhesive remnant index scores demonstrated a tendency towards score 1 in dry environment, and towards score 3 in wet environment, the scores also showed a non-significant difference (P<0.05) between Resilience and Beauty Ortho Bond adhesives using Fischer exact test. Conclusion: Beauty Ortho Bond is less sensitive to wet environment than Resilience and Heliosit adhesives, therefore it has an advantage during clean up, as it reduces the risk of enamel damage during debonding procedure. Keywords: Beauty Ortho Bond, Shear bond strength, light cured composite.
Orthodontic treatment is widely used to correct irregular teeth and/or jaw discrepancies to improve oral function and facial aesthetics. However, it is frequently associated with enamel damage that include chipping, demineralisation, and white spot formation. So far, current bonding systems that can maintain shear bond strengths (SBS) suitable for clinical performance are unable to limit enamel demineralisation, adhesive remnants and damage caused on removal of brackets after treatment. This study reports a novel “safe enamel etch” clinically viable procedure that was accomplished via application of novel etchant pastes developed with β-tricalcium phosphate and monocalcium phosphate monohydrate
This study aimed to incorporate hydroxyapatite nanoparticles (nHA) or amorphous calcium phosphate nanoparticles (nACP) into a self-etch primer (SEP) to develop a simplified orthodontic bonding system with remineralizing and enamel preserving properties.
nHA and nACP were incorporated into a commercial SEP (Transbond™ plus) in 7% weight ratio and compared with the plain SEP as a control. Shear bond strengths (SBS), enamel damage, and adhesive remnant index (ARI) scores were evaluated at 24 h
This study aimed to incorporate hydroxyapatite nanoparticles (nHA) or amorphous calcium phosphate nanoparticles (nACP) into a self-etch primer (SEP) to develop a simplified orthodontic bonding system with remineralizing and enamel preserving properties.
nHA and nACP were incorporated into a commercial SEP (Transbond™ plus) in 7% weight ratio and compared with the plain SEP as a control. Shear bond strengths (SBS), enamel damage, and adhesive remnant index (ARI) scores were evaluated at 24 h
Objective. This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. Materials and Methods. Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water stora
... Show MoreBackground and objectives: This study aimed at testing the effect of plastic sleeve or barrier, used to cover the guide of the light cure unit to prevent cross-infection, on the shear bond strength and site of bond failure of stainless steel and ceramic orthodontic brackets. Materials and methods: Forty orthodontic brackets; twenty stainless steel and twenty ceramic brackets bonded to forty extracted human maxillary first premolars using light cure adhesive cured with and without the use of a protective plastic barrier on the guide. Comparing the effect of this barrier on the shear bond strength and adhesive remnant index was performed using an independent t-test and Chi-square test. Results: The protective barrier had decreased the shear b
... Show MoreBackground: One of the most important complications of fixed orthodontic treatment is formation of white spots, which are initial carious lesions. Addition of antimicrobial agents into orthodontic adhesive material might be wise solution for prevention of white spots formation. The aim of this study was to evaluate the antibacterial properties of orthodontic adhesive primer against S. Mutans after adding the three different types of nanoparticles (Ag, ZnO, or TiO2). Materials and methods: Discs were prepared using empty insulin syringe approximately 2 mm×2 mm rounded in shape specimens (40 discs) were divided into four groups (ten discs for each group): The first group was the control (made from primer only), the second group (10 dis
... Show MoreBackground This study aimed to develop remineralizing calcium-phosphate (CaP) etchant pastes for enamel conditioning before bracket bonding and evaluate the bonding performance, failure pattern, and enamel surface integrity post bracket debonding in comparison with the conventional phosphoric acid (PA) etchant gel. Material and Methods Micro-sized monocalcium phosphate monohydrate and hydroxyapatite (micro- and nano-sized) powders were mixed with various phosphoric and nitric acid concentrations to develop eight acidic CaP pastes. Ninety extracted human premolars were randomly assigned into eight experimental and one control group (n=10). The developed pastes and control (commercial 37% PA-gel) were applied onto the enamel using the etch-a
... Show MoreThis research which is entitled (Devine Beauty), aims at studying the philosophical and literary extensive visions of Andalusian poets in search of pleasure in the beauty of divine self and its impact on the formation of a philosophical frame of mind. It also attempts to investigate the aesthetic aspects that highlight the prestige and greatness and majesty of that absolute beauty.