Copper zinc tin sulfide selenide, Cu2 ZnSn(S1−x Se x)4 , absorbers are promising earth-abundant and environmentally benign materials for low-cost photovoltaic applications. This study investigates the structural and optical properties of Cu 2 ZnSn(S1−x Se x)4 nanostructured thin films prepared by pulsed laser deposition using melt-quenched targets with selenium compositions x = 0.0–1.0. X-ray diffraction revealed that films with low selenium content remained amorphous, whereas higher selenium incorporation promoted the formation of polycrystalline kesterite–stannite phases with preferred orientations along (112), (200), (220), and (312). The crystallite size increased from 12.3 to 17.9 nm as selenium reached x = 1.0, indicating enhanced crystal growth. Atomic force microscopy showed composition-dependent surface evolution, where average roughness decreased initially, reached a maximum of 88.29 nm at x = 0.6, and then declined, reflecting structural reorganization during phase transition. Optical characterization by UV–Vis–NIR spectroscopy demonstrated high absorption coefficients exceeding 10 4 cm −1 in the visible region, confirming strong light-harvesting capability. The direct optical band gap was tunable between 2.00 and 2.30 eV, with the highest value observed at x = 0.6 due to quantum confinement, nanoscale disorder, and compositional effects. The refractive index, extinction coefficient, and dielectric constants decreased with selenium addition up to x = 0.6, then increased at higher selenium contents, indicating a strong correlation between composition and optical response. The combined results highlight selenium control as an effective route for tailoring phase stability, transparency, and photon management for devices.
In this study the alloys Ge xS1-x with different Ge content (x=0, 0.1,0.2 and 0.3) wt.% have been successfully prepared by evacuated quartz tube under vacuum pressure (10−2Torr), whereas Ge xS1-x thin films were prepared by thermal evaporation technique under vacuum (10−5Torr) with (x=0,0.1,0.2 and 0.3). The optical properties measurements shows that the optical energy gap decrease from (3.4 to 3 eV) with the increase of x content, the optical constants declare significant variation with x content variation.
In this study, the melting-cooling method was used to prepare the chalcogenide compound S60-Se40-X-PbX. Four samples were obtained by partial replacement of Selenium with Lead in the weight ratios x = 0, 10, 20, and 30, respectively. The materials were mixed separately, ground, placed in quartz ampoules, and heated to 500 degrees Celsius. After conducting several operations on the samples, their insulating properties were studied, represented by the real dielectric constant and the imaginary dielectric constant, and the electrical conductivity was measured as a function of the frequency. It was found that partial replacement plays an impo
Superconducting compound Bi2Sr2-xYxCa2Cu3O10+δ were Synthesized by method of solid state reaction, at 1033 K for 160 hours temperature of the sintering at normal atmospheric pressure where substitutions Yttrium oxide with Strontium. When Y2O3 concentration (0.0, 0.1, 0.2, 0.3, 0.4 and 0.5). All specimens of Bi2Sr2Ca2Cu3O10+δ superconducting compounds were examined. The resistivity of electrical was checked by the four point probe technique, It was found th
Zinc-indium-selenide ZnIn2Se4 (ZIS) ternary chalcopyrite thin film on glass with a 500 nm thickness was fabricated by using the thermal evaporation system with a pressure of approximately 2.5×10−5 mbar and a deposition rate of 12 Å/s. The effect of aluminum (Al) doping with 0.02 and 0.04 ratios on the structural and optical properties of film was examined. The utilization of X-ray diffraction (XRD) was employed to showcase the influence of aluminum doping on structural properties. XRD shows that thin ZIS-pure, Al-doped films at RT are polycrystalline with tetragonal structure and preferred (112) orientation. Where the
Bulk AlxSb1-x samples were prepared with different x ratios (0.1, 0.3, 0.5, 0.7 and 0.9) by quenching technique. This was done throughout mixing the aluminum and antimony elements according to the proper atomic weight and put them in an evacuated quartz ampoule which then sealed and heated at 1273 K for five hours and left to cool in air. Thin films of AlxSb1-xwere prepared by using thermal evaporation under vacuum of 10-5 mbar on glass substrates at room temperature with deposition rate (10-15nm/min) at thickness of ∼ 500nm. The structures of AlxSb1-x bulk and thin films have been studied by X–ray diffraction technique. The results showed that all alloys have polycrystalline structures and the p
Thin films of (CuO)x(ZnO)1-x composite were prepared by pulsed laser deposition technique and x ratio of 0≤ x ≤ 0.8 on clean corning glass substrate at room temperatures (RT) and annealed at 373 and 473K. The X-ray diffraction (XRD) analysis indicated that all prepared films have polycrystalline nature and the phase change from ZnO hexagonal wurtzite to CuO monoclinic structure with increasing x ratio. The deposited films were optically characterized by UV-VIS spectroscopy. The optical measurements showed that (CuO)x(ZnO)1-x films have direct energy gap. The energy band gaps of prepared thin films
This work concerned with effect of zinc oxide concentrating on the structural and optical properties of (MgO)1-x(ZnO)x thin films. (MgO)1-x(ZnO)x compounds were produced by mixing the two oxides powders accordance to the atomic ratios and compressed as pellets, these pellets were sintered in an oven at temperature1273K for five hours. Thin films from (MgO)1-x(ZnO)x compounds were obtained using pulsed laser deposition technique using Nd:YAG laser . The results of x-ray diffraction as well as UV-Visible- spectrophotometer measurements transmittance of (MgO)