In this paper, the effect of temperature on the charge transfer rate of dye (N3) in contact with ZnS semiconductors is discussed and studied when electrons move from the excited N3 dye to the conduction band of ZnS based on quantum shift theory. In a heterogeneous system, the energy levels are assumed to be continuous, and the N3-ZnS system is surrounded by a variety of polar solvent media. The transition energy of the N3/ZnS heterojunction was calculated using seven different solvents at room temperature, considering the refractive index and dielectric constant of the solvents and the ZnS semiconductor, respectively. The charge-transport reaction rate was calculated over different temperature ranges (300, 310 and 320 K) to study the influence of temperature on the charge transfer reaction rate. The probability of charge transport is influenced by the transition energy, which depends on the polar medium, and the probability of transfer increases as the transition energy decreases. The charge transfer rate, which is strongly affected by temperature, increases with increasing temperature and vice versa. The dye (N3)/semiconductor (ZnS) heterojunction system has a high probability of charge transport from the excited N3 dye to the conduction band of ZnS with polar morpholine media because the transition energy is lower than the low charge transfer that occurs in the system with polar methanol solvent, which has a large transfer energy. However, the rate increases with increasing temperature and coupling strength
In this study, gold nanoparticle samples were prepared by the chemical reduction method (seed-growth) with 4 ratios (10, 12, 15 and 18) ml of seed, and the growth was stationary at 40 ml. The optical and structural properties of these samples were studied. The 18 ml seed sample showed the highest absorbance. The X- ray diffraction (XRD) patterns of these samples showed clear peaks at (38.25o, 44.5o, 64.4o, and 77.95o). The UV-visible showed that the absorbance of all the samples was in the same range as the standard AuNPs. The field emission-scanning electron microscope (FE-SEM) showed the shape of AuNPs as nanorods and the particle size between 30-50 nm. Rhodamine-610 (RhB) was prepared at 10<
... Show MoreThe present study aimed to identify the therapeutic evaluation of chitosan extracted from the fungus cushroom and pure chitosan on glucose and lipid profile in the blood of 35 male rabbits with hyperlipidemia induced experimentally by cholesterol. The tests included estimation of glucose levels, total cholesterol, triglycerides, high-density lipoproteins, low-density lipoproteins, and very low-density lipoproteins. hyperlipidemia was induced in the male rabbits used in the study which was administered orally with cholesterol 150mg/kg body weight for a week. rabbits were divided into seven groups: control, cholesterol, pure chitosan, mushroom chitosan, cholesterol and pure chitosan, cholesterol and mushroom chitosan and cholestero
... Show MoreCeramic coating compose from a ceramic mixture (MgO, Al2O3) and metall (Al-Ni) were produced by Thermal Spray Technique. The mixed ratio of used materials Al:Ni (50%) and 40% of Al2O3 and 10% MgO. This mixture was spray on a stainless steel substrate of type (316 L) by using thermal spray with flame method and at spraying distances (8, 12, 16 and 20) cm, then the prepared films were treated by laser and thermal treatment. After that performing a hardness and adhesion tests were eximined. The present study shows that the best value of the thermal treatment is 1000 ℃ for 30 mint; the optimum spray distance is 12 cm and most suitable laser is 500 mJ where the microscopic and mechanical character
... Show MoreVibration is a source of energy that can be beneficial or harmful based on the application. Vibration can affect the function of any structure; however, Ceramic matrix composite (CMC) is one of these structures. Whereby less studies have been concentrated on study its function specially when electromagnetic wave (microwave) exposed on its surface to perform its designed function. To address this concept, SiC composite has been fabricated which is designed to have a transparent characteristics to microwave. External vibration had been applied on its surface to monitor how much influence could nanoscale amplitude vibration damage the microwave interaction. The source of vibration was applied from piezoelectric and the vibration was monitored
... Show MoreIn this paper, investigates the biosynthesis of gold nanoparticles (AuNPs) by biochemical method using Myrtus communis leaves extract as reducing agent and Chloroauric acid (HAuCl4) as precursors. X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM) and FTIR were used in addition to UV-visible spectroscopy (UV) in order to characterize the AuNPs. The biosynthesized AuNPs exhibited inhibitory effects on alpha amylase and alkaline phosphatase in sera of patient with type 2 Diabetes Miletus and the sera of healthy control subjects; the inhibition percentage with alpha amylase was 72 % and 45 % for patient and control group respectively. Oral consent obtained from the most of patients and healthy subjects before them being under
... Show MoreThe first studies on shocks and vibrations were carried out at the beginning of the 1930s to improve the behavior of buildings during earthquakes. Vibration tests on aircraft were developed from 1940 to verify the resistance of parts and equipments prior to their first use. Flutter is a well-known example of dynamic aero elasticity, where when oscillation of structure interacted with unsteady aerodynamic forces the flutter will occur. Vibration on any structure without damping means that self-harmonic oscillation will occur, and in most cases the oscillation may start to increase until structural failure. This behavior is very similar to resonance phenomena if only the oscillation is being studied as a vibration case. In vibration suppre
... Show MoreThe work concerned with studying the effect of (SiO2) addition as a
filler on the adhesive properties of (PVA). Samples were prepared as
sheets by using casting method. The mechanical properties showed
that increase in tensile strength from (34MPa) to (68MPa) when
(SiO2) added to (PVA). The adhesive strength showed that joint
properties depend upon specific adhesive characteristic of material
(PVA) and (SiO2\PVA)composites at different concentrations (1.5%,
2.5%, 3.5%, 4.5wt%), the cohesive strength of the adhesive material,
the joint design, and adherent type (Sponge Rubber(SR), Natural
leather (NL), Vulcanized Rubber(VR), and Cartoon). The results
proved the tensile strength increased with (SiO2) ratio, so