ABSTRACT: Thin film of CdS has been deposited onto clean glass substrate by using Spray pyrolysis technique. Results of Morphological (AFM) studied; electrical properties and optical conductivity studied are analysis. AFM results show a crystalline nature of the films. From the conductivity measurement at different temperatures, the activation energy of the films was calculated and found to be between 0.188 - 0.124 eV for low temperature regions, and between 1.67-1.19eV for high temperature regions. Hall measurements of electrical properties at room temperature show that the resistivity and mobility of CdS polycrystalline films deposited at 400 C0, were 3.878x103 . cm and 1.302x104cm2/ (V.s), respectively. The electrical conductivity of the films was found to be in the range of 10-4 −10-6 (. cm)-1 with n type of conduction mechanism, which is suitable as optical windows for efficient solar cells.
Effect of the thermal annealing at 400oC for 2 hours and Argon laser radiation for half hour on the optical properties of AgAlS2 thin films, prepared on glass slides by chemical spray pyrolysis at 360oC with (0.18±0.05) μm thickness .The optical characteristics of the prepared thin films have been investigated by UV/Vis spectrophotometer in the wavelength range (300 – 1100)nm .The films have a direct allow electronic transition with optical energy (Eg) values decreased from (2.25) eV for untreated thin films to (2.10) eV for the annealed films and to (2.00) eV for the radiated films. The maximum value of the refractive index (n) for all thin films are given about (2.6). Also the extinction coefficient (K) and the real and imaginary d
... Show MoreThis research examines the electrical, optical, and structural properties of zinc oxide (ZnO) and tin(IV) oxide (ZnO)1-x (SnO2)x composite thin films made by pulsed laser deposition, as well as the impact of composition concentration. The structural study of (ZnO)1-x (SnO2)x composites and thin films was conducted by X-ray analysis (XRD). Optical properties were investigated by UV–Vis infrared spectroscopy. The structural analysis revealed that all prepared thin-film composites were polycrystalline, exhibiting both hexagonal wurtzite and tetragonal phases for pure ZnO and SnO2, as well as a mixture of both phases for x=0.2 and 0.4. In contrast, the SnO2 phase was predominant for x=0.6 and 0.8. The increase in crystal size in the (
... Show MoreThin films of CdTe were prepared with thickness (500, 1000) nm on the glass substrate by vacuum evaporation technique at room temperature then treated different annealing temperatures (373,473,and 573)K for one hour. Results of the Hall Effect and the electrical conductivity of (I-V) characteristics were measured in darkness and light.at different annealing temperature results show that the thin films have ability to manufacture solar cells, and found that the efficient equal to (2.18%) for structure solar cell (Algrid / CdS / CdTe /glass/ Al) and the efficient equal to (1.12%) for structure solar cell (Algrid / CdS / CdTe /Si/ Al) with thick ness of (1000) nm with CdTe thin films at RT.
In this work, pure and doped Vanadium Pentoxide (V2O5) thin films with different concentration of TiO2 (0, 0.1, 0.3, 0.5) wt were obtained using Pulse laser deposition technique on amorphous glass substrate with thickness of (250)nm. The morphological, UV-Visible and Fourier Transform Infrared Spectroscopy (FT-IR) were studied. TiO2 doping into V2O5 matrix revealed an interesting morphological change from an array of high density pure V2O5 nanorods (~140 nm) to granular structure in TiO2-doped V2O5 thin film .Transform Infrared Spectro
... Show MoreIn this study, high quality ZnO/Ag-NPs thin transparent and conductive film coatings were fabricated
Optical properties of chromium oxide (Cr2O3) thin films which were prepared by pulse laser deposition method, onto glass substrates. Different laser energy (500-900) mJ were used to obtain Cr2O3 thin films with thickness ranging from 177.3 to 372.4 nm were measured using Tolansky method. Then films were annealed at temperature equal to 300 °C. Absorption spectra were used to determine the absorption coefficient of the films, and the effects of the annealing temperature on the absorption coefficient were investigated. The absorption edge shifted to red range of wavelength, and the optical constants of Cr2O3 films increases as the annealing temperature increased to 300 °C. X-ray diffraction (XRD) study reveals that Cr2O3 thin films are a
... Show MoreBulk AlxSb1-x samples were prepared with different x ratios (0.1, 0.3, 0.5, 0.7 and 0.9) by quenching technique. This was done throughout mixing the aluminum and antimony elements according to the proper atomic weight and put them in an evacuated quartz ampoule which then sealed and heated at 1273 K for five hours and left to cool in air. Thin films of AlxSb1-xwere prepared by using thermal evaporation under vacuum of 10-5 mbar on glass substrates at room temperature with deposition rate (10-15nm/min) at thickness of ∼ 500nm. The structures of AlxSb1-x bulk and thin films have been studied by X–ray diffraction technique. The results showed that all alloys have polycrystalline structures and the p