Beryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa
... Show MoreThis research was conduct to evaluate the cytotoxic effect of exotoxin A (ETA) produced by Pseudomonas aeruginosa on mice in comparison with (phosphate buffer saline (PBS) as a negative control. The effect of the toxin was measured by employing the cytogenetic analysis which included (the mitotic index (MI), chromosomal aberrations (CAs), micronucleus (MN) and sperm abnormalities) parameters. In order to specify the cytotoxic effect of the toxin, three doses of ETA (125, 250 and 500 ng/ml) were used. Results showed that ETA was found to cause a significant decrease in mitotic index (MI) percentage, while significant increase in micronucleus (MN), chromosomal aberrations (CAs) and sperm abnormalities parameters in compression with control wa
... Show MoreAbstract: In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
Abstract: The aim of this study was to evaluate the effect of bone density value in Hounsfield unit derived from cone beam computed tomography (CBCT), and implant dimensions in relation to implant stability parameters namely the resonance frequency analysis and the insertion torque (IT) value. It included 24 patients who received 42 dental implants (DI). The bone density of the planned implant site was preoperatively measured using cone beam computed tomography. The implant stability was measured using Osstell implant stability quotient (ISQ). The ISQ values were recorded immediately postoperatively and after 16 weeks. The IT value was categorized as 35 N/cm or > 35 N/cm. The mean (standard deviation) primary stability was 79.58 (5.27) ISQ,
... Show MoreThis survey investigates the thermal evaporation of Ag2Se on glass substrates at various thermal annealing temperatures (300, 348, 398, and 448) °K. To ascertain the effect of annealing temperature on the structural, surface morphology, and optical properties of Ag2Se films, investigations and research were carried out. The crystal structure of the film was described by Xray diffraction and other methods.The physical structure and characteristics of the Ag2Se thin films were examined using X-ray and atomic force microscopy (AFM) based techniques. The Ag2Se films surface morphology was examined by AFM techniques; the investigation gave average diameter, surface roughness, and grain size mutation values with increasing annealing temperature
... Show MorePowders for (TiO 2 ) 1−x(MoO 3 ) x composites have been prepared with the use of a dry mix of TiO2 and MoO3 oxides with a variety of compositions (x = 0, 0.2, 0.4, 0.6, 0.8, and 1), then sintering at 1473 K. The materials have been ground and formed into pellets so that they could be used as targets for the pulsed laser deposition (PLD) process, which produced thin flms with a thickness of ≈150 nm on a glass substrate. When MoO3 is added to TiO2 , the crystal size has been observed to decrease from 33.3 to 25.8 nm, yet it after that continued to expand as MoO3 was added. The molybdenum ions were confrmed by XRD patterns, indicating that the substitution regarding Mo+6 ions for Ti +4 ions in TiO2 matrix is what is re
... Show More