The provision of openings in serviceable reinforced concrete beams may result in a substantial decline in the beam's capacity and integrity, indicating the necessity of opening strengthening. The present study investigates the experimental response of reinforced concrete T-beams with multiple web-strengthened openings disposed in shear span to static and impact loads. Fourteen RC T-beams were tested in two groups, each of seven beams. The first group was tested under static loading up to failure, while the second group was tested under repeated impact loading until the width of shear cracks reached 0.3 mm. The residual static strengths of the beams subjected to impact loading were then determined. The test variables considered were: number of web openings, the method used to strengthen the member at openings and the height of drop during impact tests. All beams were simply supported with load applied at mid – span. Static results indicated that T-beams with four and six un-strengthened web circular openings whose diameter is 48% of the web depth have strength capacities less than those without openings by 30% and 41%, respectively. However, strengthening of webs results in an increase in the strength capacities ranging between 27% and 92%, depending on the type of strengthening. Impact results indicated that the beam with four openings did not show a remarkable increase in the maximum mid-span deflection compared with the solid beam, while that with six openings showed an increase in the maximum mid-span deflections by about 75% greater than the maximum mid-span deflection of the solid beam. Strengthening of specimens could overcome the increase in deflections.
The massive growth of the automotive industry and the development of vehicles use lead to produce a huge amount of waste tire rubber. Rubber tires are non-biodegradable, resulting in environmental problems such as fire risks. In this search, the flexural behavior of steel fiber reinforced self-compacting concrete (SFRSCC) beams containing different percentages and sizes of waste tire rubbers were studied and compared them with the flexural behavior of SCC and SFRSCC. Micro steel fiber (straight type) with aspect ratio 65 was used in mixes. The replacement of coarse and fine aggregate was 20% and 10% with chip and crumb rubber. Also, the replacement of limestone dust and silica fume was 50%, 25%, and 12% with ground rubbe
... Show MoreSewer sediment deposition is an important aspect as it relates to several operational and environmental problems. It concerns municipalities as it affects the sewer system and contributes to sewer failure which has a catastrophic effect if happened in trunks or interceptors. Sewer rehabilitation is a costly process and complex in terms of choosing the method of rehabilitation and individual sewers to be rehabilitated. For such a complex process, inspection techniques assist in the decision-making process; though, it may add to the total expenditure of the project as it requires special tools and trained personnel. For developing countries, Inspection could prohibit the rehabilitation proceeds. In this study, the researchers propos
... Show MoreIncorporating waste byproducts into concrete is an innovative and promising way to minimize the environmental impact of waste material while maintaining and/or improving concrete’s mechanical characteristics and strength. The proper application of sawdust as a pozzolan in the building industry remains a significant challenge. Consequently, this study conducted an experimental evaluation of sawdust as a fill material. In particular, sawdust as a fine aggregate in concrete offers a realistic structural and economical possibility for the construction of lightweight structural systems. Failure under four-point loads was investigated for six concrete-filled steel tube (CFST) specimens. The results indicated that recycled lightweight co
... Show MoreIn this study, the effect of construction joints on the performance of reinforced concrete beams was experimentally investigated. Seven beam specimens, with dimensions of 200×100×1000 mm, were fabricated. The variables were considered including; the location and configuration of the joints. One beam was cast without a joint (Reference specimen), two specimens were fabricated with a one horizontal joint located either at tension, or compression zone. The fourth
beam had two horizontal joints placed at tension, and compression area. The remaining specimens were with one or two inclined joints positioned at the shear span or beam’s mid-span. The specimens were subjected to a monotonic central concentrated loading until the failure. T
The subject of the listen to the voice of the customer of topics relatively new in management thought, as it won the attention of many organizations of different types, because it is important to achieve success and to continue and superiority to them, so there is a need to study this term in the Iraqi organizations and try to diagnose the implementation of the study sample to listen voice of the Customer and its
... Show More