Highly Modified Asphalt (HiMA) binders have garnered significant attention due to their superior resistance to rutting, fatigue cracking, and thermal distress under heavy traffic loads and extreme environmental conditions. While elastomeric polymers such as Styrene- Butadiene-Styrene (SBS) have been extensively used in HiMA applications, the potential of plastomeric polymers, including Polyethylene (PE) and Ethylene Vinyl Acetate (EVA), remains largely unexplored. This study aims to evaluate the performance of reference binder (RB) modified with plastomeric HiMA asphalt in comparison to SBS-modified binders and determine the optimal polymer dosage for achieving an optimal balance between rutting resistance and fatigue durability. The experimental program involved modifying a base asphalt binder with SBS, PE, and EVA at dosages of 6%, 7%, and 8% by weight of binder. A comprehensive evaluation was conducted, including conventional tests (penetration, softening point, viscosity, mass loss, storage stability, and specific gravity) and rheological characterization using the Dynamic Shear Rheometer (DSR). The Multiple Stress Creep Recovery (MSCR) test was employed to assess high-temperature performance, while the Linear Amplitude Sweep (LAS) test evaluated fatigue behavior. Additionally, an Overall Desirability (OD) analysis was performed to integrate multiple performance criteria and establish a ranking for each modification. The results demonstrated that SBS-modified binders exhibited the most balanced performance, with SBS8 achieving the highest elastic recovery (52.87%) and superior fatigue life, exceeding 1,017,904 cycles at 2.5% strain. PE8 exhibited exceptional rutting resistance, reaching the lowest Jnr 3.2 value (0.0078 kPa−1); however, its limited elasticity (15.7% recovery) indicated reduced flexibility. EVA modifications demonstrated marginal improvements in fatigue resistance but failed to meet the AASHTO M332 criteria for high-traffic applications. The OD analysis ranked SBS8 as the most effective HiMA binder (OD score = 0.715), followed by SBS7 (0.588) and SBS6 (0.509). PE7 (0.354) and PE6 (0.337) demonstrated moderate performance, whereas EVA had the lowest desirability score (0.000). Based on these findings, SBS-modified binders are recommended for applications requiring a balance between fatigue and rutting resistance, whereas PE-based HiMA is more suitable for high-temperature regions where rutting is the primary concern. Further field studies are necessary to validate the long-term durability of plastomeric HiMA binders and optimize their use for specific pavement conditions.
Moisture induced damage in asphaltic pavement might be considered as a serious defect that contributed to growth other distresses such as permanent deformation and fatigue cracking. This paper work aimed through an experimental effort to assess the behaviour of asphaltic mixtures that fabricated by incorporating several dosages of carbon fiber in regard to the resistance potential of harmful effect of moisture in pavement. Laboratory tests were performed on specimens containing fiber with different lengths and contents. These tests are: Marshall Test, the indirect tensile test and the index of retained strength. The optimum asphalt contents were determined based on the Marshall method. The preparation of asphaltic mixtures involved
... Show MoreThis study explores the role of nanomaterials in the performance of asphalt binders and mixtures. Two commonly available nanomaterials, i.e., nanosilica (NS) and nanoalumina (NA), were used at contents of 0%, 2%, 4%, 6%, and 8% by weight of asphalt binder. A set of experiments was carried out at the binder level to investigate properties such as penetration, softening point, aging-related mass loss, nanomaterial dispersion (storage stability), and workability (rotational viscosity). In addition, the suitability of NS and NS was also assessed through the testing of nanomodified asphalt mixtures, which focused on Marshall properties, the resilient modulus, moisture susceptibility, permanent deformation, and fatigue resistance. The findings in
... Show MoreRecently, interest in the use of projectiles in research on recycling waste materials for construction applications has grown. Using recycled materials for the construction of asphalt concrete pavement, in the meantime, has become a topic of research due to its significant benefits, such as cost savings and reduced environmental impacts. This study reports on comprehensive experimental research conducted using a typical mechanical milling waste, iron filing waste (IFW), as an alternative fine aggregate for warm mix asphalt (WMA) for pavement wearing surface applications. A type of IFW from a local machine workshop was used to replace the conventional fine aggregate, fine natural sand (FNS), at percentages of 25%, 50% 75%, and 100% b
... Show MoreDue to increasing cost of asphalt binder, significant economic savings can be realized by using the amount from reclaimed asphalt pavement (RAP) in the production of new hot mix asphalt (HMA). Moreover, this is an environmentally friendly option as it reduces the demand for virgin materials. It has to be remarked that in Iraq RAP is not used in the production of HMA and this valuable material is mostly degraded for use in lower value applications. Four mixtures were designed, which contains three different percent RAP, it is (0%, 5%, 15%) with asphalt grade (40-50) and (25%) with asphalt grade (60-70), it has been changed the grade of asphalt when adding RAP (25%) to compensate for the aged binder in the RAP when adding to mixture. All type
... Show MoreBackground: Elastomeric chains are used to generate force in many orthodontic procedures, but this force decays over time, which could affect tooth movement. This study aimed to study the force degradation of elastomeric chains. Data and Sources: An electronic search on Cochrane Central Register of Controlled Trials (CENTRAL), MEDLINE, LILACS, and PubMed was made, only articles written in English were included, up to January 2022.Study selection: Fifty original articles, systematic reviews, and RCTs were selected. Conclusion: Tooth movement, salivary enzymes, alcohol-containing mouthwash, whitening mouthwash, and alkaline and strong acidic (pH <5.4) solutions all have a significant impact on elastomeric chain force degradation. The fo
... Show MoreIn the 1980s, the French Administration Roads LCPC developed high modulus mixtures (EME) by using hard binder. This type of mixture presented good resistance to moisture damage and improved . mechanical properties for asphalt mixtures including high modulus, good fatigue behaviour and excellent resistance to rutting. In Iraq, this type of mixture has not been used yet. The main objective of this research is to evaluate the performance of high modulus mixtures and comparing them with the conventional mixture, to achieve this objective, asphalt concrete mixes were prepared and then tested to evaluate their engineering properties which include moisture damage, resilient modulus, permanent deformation and fatigue characteristics. These prope
... Show MorePermanent deformation, fatigue and thermal cracking are the three typical distresses of flexible pavement. Using hydrated lime (HL) into the conventional limestone mineral additive has been widely practiced, including in Europe, to improve the mechanical properties of hot mix asphalt (HMA) concrete and as the result the durability of the constructed pavement. Large number of experimental studies have been reported to find the optimum addition of HL for the improvement on HMA concrete mechanical properties, moisture susceptibility and fatigue resistance. Pavement in service is under complex thermomechanical stress-strain conditions due to coupled atmospheric and surrounding environment temperature variation and the traffic loading. To predic
... Show MoreBackground: The ideal force-delivery system must: provide optimal tooth moving forces that elicit the desired effects, be comfortable and hygienic for the patient, require minimal operator manipulation and patient cooperation and provide rapid tooth movement with minimal mobility during orthodontic therapy, the elastomeric chains have the greatest potential to fulfill these requirements. Materials and Methods: This in vitro study was designed to determine the effect of three different mechanisms for canine retraction : (6-3 , 6-5-3 and chain loop ) on the load relaxation behavior of three types of elastomeric chains : (maximum clear , maximum silver and extreme silver) from the same company (Ortho Technology company) with two different bran
... Show MoreAging of asphalt pavements typically occurs through oxidation of the asphalt and evaporation of the lighter maltenes from the binder. The main objective of this study is to evaluate influence of aging on performance of asphalt paving materials.nAsphalt concrete mixtures, were prepared, and subjected to short term aging (STA) procedure which involved heating the loose mixtures in an oven for two aging period of (4 and 8) hours at a temperature of 135 o C. Then it was subject to Long term aging (LTA) procedure using (2 and 5) days aging periods at 85 o C for Marshall compacted specimens. The effect of aging periods on properties of asphalt concrete at optimum asphalt content such as Marshall Properties, indirect tensile strength at 25 o C,
... Show More