The green method was chosen for the preparation of nano iron oxide due to its simplicity, ease of preparation, and purity, compared to other methods. Nano iron oxide was made using a substance that causes precipitation and a coating from the alcoholic extract of orange leaves from Iraq. It was examined structurally and spectrally using several techniques, including X-ray diffraction, Fourier transform infrared spectroscopy, field-emission scanning microscopy (FESEM), energy-dispersive X-ray spectroscopy, and UV-Vis spectroscopy. The diagnosis proved that the nano iron oxide was successfully prepared in a spherical form and with an average size of 71.1 nm. The nano iron oxide particles were tested for their ability to remove crystal violet (CV) dye from an aqueous solution using the adsorption technique, achieving a removal percentage of 51% at 298K, with an adsorbent dose of 0.01 g, a contact time of 90 minutes, and an initial dye concentration of 11 mg/L. The adsorption process data were analyzed kinetically using kinetic models. It was found that the process follows the pseudo-second-order kinetic model, suggesting that the type of adsorption is chemical. The results indicate the potential use of nano iron oxide to protect the aquatic environment.
The removal of boron from aqueous solution was carried out by electrocoagulation (EC) using magnesium electrodes as anode and stainless steel electrodes as cathode. Several operating parameters on the removal efficiency of boron were investigated, such as initial pH, current density, initial boron ion concentration, NaCl concentration, spacing between electrodes, electrode material, and presence of carbonate concentration. The optimum removal efficiency of 91. 5 % was achieved at a current density of 3 mA/cm² and pH = 7 using (Mg/St. St. ) electrodes, within 45 min of operating time. The concentration of NaCl was o. 1 g/l with a 0.5cm spacing between the electrodes. First and second order rate equation were applied to study adsorp
... Show Moreيصف هذا البحث الإنتاج الصديق للبيئة لجسيمات النحاس النانوية باستخدام مستخلص نبات الجرجير والحرق عند درجة حرارة 400 درجة مئوية لمدة 3 ساعات. تم استخدام SEM و TEM لتحليل حجم الجسيمات النانوية المحضرة. تم استخدام حيود الأشعة السينية لتحديد الهيكل البلوري. كشف التحليل الطيفي للأشعة السينية المشتتة للطاقة لهيكل المنتج الذي تم إنشاؤه عن مكونات النحاس والأكسجين فقط ، مما يدل على نقاء المادة المحضرة. استخدمت الماد
... Show MoreThis work is focused on studying the effect of liquid layer level (height above a target material) on zinc oxide nanoparticles (ZnO and ZnO2) production using liquid-phase pulsed laser ablation (LP-PLA) technique. A plate of Zn metal inside different heights of an aqueous environment of cetyl trimethyl ammonium bromide (CTAB) with molarity (10-3 M) was irradiated with femtosecond pulses. The effect of liquid layer height on the optical properties and structure of ZnO was studied and characterized through UV-visible absorption test at three peaks at 213 nm, 216 nm and 218 nm for three liquid heights 4, 6 and 8 mm respectively. The obtained results of UV–visible spectra test show a blue shift accomp
... Show MoreCurrent studies interested on the biosynthesis of zinc oxide nanoparticles (ZnO-NPs) using hot plants extracts of Allium sativum and characterization of them using: Atomic Force Microscopy (AFM), X-ray diffractions (XRD), Fourier Transform Infrared Spectroscopy (FT- IR), UV–visible spectral and Hot stage. The results found that all NPs are had nano-size. ZnO NPs was produced by four procedures using hot extract of Allium sativum. The average diameters were: 101.59 nm, 110.33 nm, 75.69 nm, 88.67 nm for first, second, third and fourth procedures respectively compared with 47.57 nm for standard NPs. The Roughness averages (Ra) were: 10.8 nm, 6.83 nm, 13.8 nm, 0.541 nm for first, second, third and fourth respectively. The Root mean square (Sq
... Show MoreIn this work, metal oxides nanostructures, mainly, copper oxide (CuO), nickel oxide (NiO), titanium dioxide (TiO2), and multilayer structure were synthesized by dc reactive magnetron sputtering technique. The structural purity and nanoparticle size of the prepared nanostructures were determined. The individual metal oxide samples (CuO, NiO and TiO2) showed high structural purity and minimum particle sizes of 34, 44, 61 nm, respectively. As well, the multilayer structure showed high structural purity as no elements or compounds other than the three oxides were founds in the final sample while the minimum particle size was 18 nm. This reduction in nanoparticle size can be considered as an advantage for the dc reactive magnetron sputtering tec
... Show Moreفي الدراسة الحالية، تم تصنيع جسيمات ZrO2 النانوية باستخدام مستخلص نباتي مشتق من نبات Vitex agnus castus، ووسط قلوي مثل هيدروكسيد الصوديوم. تم استخدام أسلوب التخليق الحيوي لتحضير جزيئات أوكسيد الزركونيوم النانوية لهذا المشروع البحثي. تتميز هذه الطريقة عن غيرها بسبب فعاليتها من حيث التكلفة وبساطتها وقلة المخاطر المحتملة. وتم تشخيص العينات المحضرة باستخدام المجهر الإلكتروني النافذ TEM، المجهر الإلكتروني الماسح SEM،
... Show MoreThis paper presents the effect of Cr doping on the optical and structural properties of TiO2 films synthesized by sol-gel and deposited by the dip- coating technique. The characteristics of pure and Cr-doped TiO2 were studied by absorption and X-ray diffraction measurement. The spectrum of UV absorption of TiO2 chromium concentrations indicates a red shift; therefore, the energy gap decreases with increased doping. The minimum value of energy gap (2.5 eV) is found at concentration of 4 %. XRD measurements show that the anatase phase is shown for all thin films. Surface morphology measurement by atomic force microscope (AFM) showed that the roughness of thin films decrease with doping and has a minimum value with 4 wt % doping ratio.
In this work, multilayer nanostructures were prepared from two metal oxide thin films by dc reactive magnetron sputtering technique. These metal oxide were nickel oxide (NiO) and titanium dioxide (TiO2). The prepared nanostructures showed high structural purity as confirmed by the spectroscopic and structural characterization tests, mainly FTIR, XRD and EDX. This feature may be attributed to the fine control of operation parameters of dc reactive magnetron sputtering system as well as the preparation conditions using the same system. The nanostructures prepared in this work can be successfully used for the fabrication of nanodevices for photonics and optoelectronics requiring highly-pure nanomaterials.