Optical losses represent one of the primary obstacles to increasing the efficiency of silicon solar cells. The recommended solution to minimize optical losses is the use of plasmonic metal nanoparticles; however, they act as recombination centers within the solar cell construction, leading to a decrease in performance. The goal of this article is to introduce cobalt/graphene nanoparticles into the solar cell to minimize the optical losses. An ultra-thin film silicon PIN solar cell of dimensions (400 ×400 ×900) nm3 with ring metal contact shape was designed and numerically investigated using COMSOL Multiphysics software version 6.2 by the finite element method (FEM). Core/shell cobalt-graphene (Co/Gr) nanoparticles are periodically introduced into the cell between two layers (electron transport and active) in a ratio of 50:50 with an inter-spacing of a similar diameter. The Co/Gr parameters, number of nanoparticles (2, 4, 6), radius (10, 20, 30) nm, and shell thickness (1, 2, 4) nm were extensively studied. In addition, the arrangement of the core/shell nanoparticle material was considered. The results manifest the best performance of the proposed cell at 4 nanoparticles of 30 nm radius with 2 nm shell thickness for Co/Gr nanoparticles to get a maximum photocurrent of 26.28 mA/cm2. It is concluded that the optical losses of the Co/Gr core/shell nanoparticles embedded in an ultra-thin film silicon solar cell are significantly reduced owing to the increment in the absorption and hence the photocurrent. This enhancement opens a new avenue for further improvements.
Copper oxide (CuO) nanoparticles were synthesized through the thermal decomposition of a copper(II) Schiff-base complex. The complex was formed by reacting cupric acetate with a Schiff base in a 2:1 metal-to-ligand ratio. The Schiff base itself was synthesized via the condensation of benzidine and 2-hydroxybenzaldehyde in the presence of glacial acetic acid. This newly synthesized symmetric Schiff base served as the ligand for the Cu(II) metal ion complex. The ligand and its complex were characterized using several spectroscopic methods, including FTIR, UV-vis, 1H-NMR, 13C-NMR, CHNS, and AAS, along with TGA, molar conductivity and magnetic susceptibility measurements. The CuO nanoparticles were produced by thermally decomposing the
... Show MoreCopper oxide (CuO) nanoparticles were synthesized through the thermal decomposition of a copper(II) Schiff-base complex. The complex was formed by reacting cupric acetate with a Schiff base in a 2:1 metal-to-ligand ratio. The Schiff base itself was synthesized via the condensation of benzidine and 2-hydroxybenzaldehyde in the presence of glacial acetic acid. This newly synthesized symmetric Schiff base served as the ligand for the Cu(II) metal ion complex. The ligand and its complex were characterized using several spectroscopic methods, including FTIR, UV-vis, 1H-NMR, 13C-NMR, CHNS, and AAS, along with TGA, molar conductivity and magnetic susceptibility measurements. The CuO nanoparticles were produced by thermally decomposing the
... Show MoreIn this work, a simulated study was carried out for designing a novel spiral rectangular patch of microstrip antenna that is used in ultra-wideband applications by using a high frequency structure simulator software (HFSS). A substrate with dielectric constant of 4.4 and height 2.10 mm (commercial substrate height available is about 0.8-1.575 mm) has been used for the design of the proposed antenna. The design basis for enhancing bandwidth in the frequency range 6.63 - 10.93 GHz is based on increasing the edge areas that positively affect the antenna's efficiency. This design makes the designed antenna cost less by reducing the area of the patch. It has been noticed that the bandwidth of the antenna under this study is increasing to 4.30
... Show MoreThin filis have been prepared from the tin disulphide (SnS2 ), the pure and the doped with copper (SnS2:Cu) with a percentages (1,2,3,4)% by using ahemical spray pyrolysis techniqee on substrate of glass heated up to(603K)and sith thicknesses (0.7±0.02)?m ,after that the films were treated thermally with a low pressure (10-3mb) and at a temperature of (473K) for one hour. The influence of both doping with copper and the thermal treatment on some of the physical characteristics of the prepared films(structural and optical) was studied. The X-ray analysis showed that the prepared films were polycrystalline Hexagonal type. The optical study that included the absorptance and transmitance spectra in the weavelength range (300-900)nm
... Show MoreThe effect of heat treatment using different annealing temperatures on optical properties of bulk heterojunction blend (BHJ) Alq3: C60 thin films which are fabricated by the spin coating technique were investigated in this study. The films have been coated on a glass substrate with speed of 2000 rpm for one min and treated with different annealing temperature (373, 423 and 473) K under vacuum. The optical properties and the chemical bonds structure of blends as-deposited and heat treated have been studied by UV-Vis spectroscopic and Fourier Transform-Infra Red (FTIR) measurements respectively. The results of UV visible show that the optical energy gap decreasing with increasing the annealing temperature for the ratio (100:1) while decrea
... Show MoreIn this paper the effect of thermal annealing on the structural and optical properties of Antimony Selenide (Sb2Se3) is investigated. Sb2Se3 powder is evaporated on clean amorphous glass substrates at room temperature under high vacuum pressure (4.5×10-6 mbar) to form thin films. The structural investigation was done with the aid of X-ray diffraction (XRD) and atomic force microscopy (AFM). The amorphous to polycrystalline transformation of these thin films was shown by X-ray diffraction analysis after thermal annealing. These films' morphology is explained. (UV-Vis ) spectra in ranges from 300 to 1100 nm was used to examine the optical properties of the films .The absorption coefficient and optical energy gap of the investigated films are
... Show MoreTi6Al4V thin film was prepared on glass substrate by RF
sputtering method. The effect of RF power on the optical properties
of the thin films has been investigated using UV-visible
Spectrophotometer. It's found that the absorbance and the extinction
coefficient (k) for deposited thin films increase with increasing
applied power, while another parameters such as dielectric constant
and refractive index decrease with increasing RF power.
Undoped and Iodine (I)–doped chrome oxide (Cr2O3)thin films have been prepared by chemical spray pyrolysis technique at substrate temperatures(773K) on glass substrate. Absorbance and transmittance spectra have been recorded as a function of wavelength in the range (340-800 nm) in order to study the optical properties such as reflectance, Energy gap of allowed direct transition, extinction coefficient refractive index, and dielectric constant in real and imagery parts all as a function of wavelength. It was found that all the investigated parameters affect by the doping ratios.
CdS and CdS:Sn thin films were successfully deposited on glass
substrates by spray pyrolysis method. The films were grown at
substrate temperatures 300 C°. The effects of Sn concentration on the
structural and optical properties were studied.
The XRD profiles showed that the films are polycrystalline with
hexagonal structure grown preferentially along the (002) axis. The
optical studies exhibit direct allowed transition. Energy band gap
vary from 3.2 to 2.7 eV.