Structural and optical properties of CdO and CdO0.99Cu0.01 thin
films were prepared in this work. Cadmium Oxide (CdO) and
CdO0.99Cu0.01semiconducting films are deposited on glass substrates
by using pulsed laser deposition method (PLD) using SHG with Qswitched
Nd:YAG pulsed laser operation at 1064nm in 6x10-2 mbar
vacuum condition and frequency 6 Hz. CdO and CdO0.99Cu0.01 thin
films annealed at 550 C̊ for 12 min. The crystalline structure was
studied by X-ray diffraction (XRD) method and atomic force
microscope (AFM). It shows that the films are polycrystalline.
Optical properties of thin films were analyzed. The direct band gap
energy of CdO and CdO0.99Cu0.01 thin films were determined from
(αhυ)1/2 v
Cadmium sulfide (CdS) thin films with n-type semiconductor characteristics were prepared by flash evaporating method on glass substrates. Some films were annealed at 250 oC for 1hr in air. The thicknesses of the films was estimated to be 0.5µ by the spectrometer measurement. Structural, morphological, electrical, optical and photoconductivity properties of CdS films have been investigated by X-ray diffraction, AFM, the Hall effect, optical transmittance spectra and photoconductivity analysis, respectively. X-ray diffraction (XRD) pattern shows that CdS films are in the stable hexagonal crystalline structure. Using Debye Scherrerś formula, the average grain size for the samples was found to be 26 nm. The transmittance of the
... Show MoreThe creation and characterisation of biodegradable blend films based on chitosan and polyvinyl alcohol for application in a range of packaging is described. The compatibility between the chitosan and PVA polymers was good. Composite films had a compact and homogeneous structure, according to the morphology analysis. The mechanical test result of PVA/CH at concentrations 5% showed, that The higher values of TS recorded in sample (p1, with 40 MPa) while the lower values appeared in sample (p9, with 22.09 MPa), the TS decreased gradually as the amount of PVA increased in blend film. While the blend film of pure Chitosan exhibits a poor mechanical strength which makes it a poor candidate for packaging but Blending CH with PVA together improved
... Show MoreBacopa monnieri L. (Scrophulariaceae), synoname is Herpestis monniera that provides bioactive compounds, especially triterpenoid saponins (Bacosides) which exhibits an important biological activities, like hypothyroidism, anticonvulsant, memory enhancing and antistress. Because there are no researches about B. monnieri L. plant that grow in Iraq, and there active compounds especially triterpenoid saponin (TS), and there effects. This study was detected the presence of (TS) in, and examined the cytotoxic and the antioxidant activity of these compounds in vitro. The study was included the extraction and identification of TS from the whole parts of B. monnieri L. by using three methods, and the best yield was analyzed by High Performance Liqui
... Show MoreThe current study deals with host-guest complex formation between cucurbit [7] urils as host and lansoprazole as guesti using PM3 (semi empirical molecules orbital calculations) also DFT calculations. In this complex, the formation of hydrogen bonding may be occurred through portal oxygen atoms(O2) of cucurbit [7] urils and amine groups (NH 2 )of the drug. The energies of HOMO and LUMO orbital’s have been computed for the host guest complex and its components. The result of the stabilization energy explained a complex formation.
The study was conducted in the Tigris River in Baghdad during May 2021 until March 2022 to follow the impact of climate change, rising temperatures, and the presence of pollutants on the dynamics of phytoplankton and some physicochemical variables from four sites. The results showed that the climatic conditions during different seasons, in addition to the nature of the sampling sites, have a clear and significant impact on the studied traits and, in turn, affect the phytoplankton community. The highest average temperature (30.67 ˚C) was recorded; the pH values ranged between 8.70 & 6.75; the electrical conductivity (1208.18-770.11 µS/cm ) and the total dissolved solids (TDS) (778.95- 439.49 mg/L) were evaluated. Upon measuring
... Show More