Improving the permanent deformation resistance of asphalt pavements is a vital challenge. Nanomaterials have emerged as promising additives due to their ability to enhance the binder stiffness and elasticity. This study evaluated the influence of five nanomaterials, namely Nano-Silica (NS), Nano-Alumina (NA), Nano-Zinc (NZ), Nano-Titanium (NT), and Carbon Nanotubes (CNTs) incorporated into a base asphalt binder at varying dosages, with up to 10% for NS, NA, and NT, and up to 5% for NZ and CNT. Fifteen modified binders were assessed using the Multiple Stress Creep Recovery (MSCR) test to obtain non-recoverable creep compliance (Jnr), while the corresponding hot mix asphalt samples underwent repeated load testing and rut depth prediction using the VESYS 5 W model. The results showed that most nanomaterials improved the high-temperature binder properties with a reduced rutting potential. Strong correlations were observed between Jnr and the mixture performance for NS and NZ, whereas NA and CNTs enhanced the mixture stiffness and deformation resistance beyond what was indicated by Jnr alone. NT showed minimal correlation between the binder and mixture performance. While Jnr is a valuable parameter for rutting prediction, it may not always accurately reflect the nano-modified mixture performance, particularly when using higher modification dosages. Therefore, combining the binder with mixture tests provides a reliable performance prediction and optimal nanomaterial selection.
In the present study, the growth and total lipid contents of two oleaginous fungal isolates Aspergillus terreus, Aspergillus fumigatus were compared in different nitrogen and organic carbon sources. Artificially the fungi were cultured on media consisting of various mono- or di- or polysaccharides and peptone or yeast extract as elementary sources for carbon and nitrogen, respectively. Media containing sucrose /yeast extract or glucose/ yeast extract were the most effective for lipid production from fungal, during two weeks incubation period, the highest biomass of dry weight was (19.6 , 18.8) g / L , (25.8 , 30.5) g /L and lipid yield (1, 0.97 )g/L, (0.65, 0.65) g/ L for two isolates Aspergillus terreus
... Show MoreRecently the use of nanofluids represents very important materials. They are used in different branches like medicine, engineering, power, heat transfer, etc. The stability of nanofluids is an important factor to improve the performance of nanofluids with good results. In this research two types of nanoparticles, TiO2 (titanium oxide) and γ-Al2O3 (gamma aluminum oxide) were used with base fluid water. Two-step method were used to prepare the nanofluids. One concentration 0.003 vol. %, the nanoparticles were examined. Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM) and X-ray diffraction (XRD) were used to accomplish these tests. The stability of the two types of nanofluids is measured by
... Show MoreIn the 1980s, the French Administration Roads LCPC developed high modulus mixtures (EME) by using hard binder. This type of mixture presented good resistance to moisture damage and improved . mechanical properties for asphalt mixtures including high modulus, good fatigue behaviour and excellent resistance to rutting. In Iraq, this type of mixture has not been used yet. The main objective of this research is to evaluate the performance of high modulus mixtures and comparing them with the conventional mixture, to achieve this objective, asphalt concrete mixes were prepared and then tested to evaluate their engineering properties which include moisture damage, resilient modulus, permanent deformation and fatigue characteristics. These prope
... Show MoreAssessment of the in service behavior of asphalt stabilized subgrade soil under environmental impact has got little attention by the research workers. However, the sustainability of the roadway depends mainly on the welfare of its subgrade soil condition. In this work, Gypseous soil was stabilized with asphalt emulsion for subgrade usage, the durability of the mixture has been assessed in term of its ability to maintain the compressive strength when practicing the environmental impacts. Specimens of 38 mm in diameter , and 76 mm in height have been prepared with various water-asphalt percentages, and subjected to 30 cycles of (freezing-thawing), (heating-cooling) and (wetting-drying) processes. Specimens have been tested for unconfined comp
... Show MoreMany researchers tried to prevent or reduce moisture damage and its sensitivity to temperature to improving the performance of hot mix asphalt because it is decreasing the functional and structural life of fixable pavement due to the moisture damage had exposed to it.
The main objective of this study is to inspect the effect of (fly ash “3%, 6%, 12%”, hydrated lime”5%, 10%, 20%” and silica fumes”1%, 2%, 4%) referring to previous research by the net weight asphalt cement as a modified material on the moisture and temperature sensitivity of hot mix asphalt. This was done using asphalt from AL-Nasiria refinery with penetration grade 40-50, nominal maximum size (12.5) mm (surface course) of aggregate and on
... Show MoreThe objective of the study to develop an amorphous solid dispersion for poorly soluble raltegravir by hot melt extrusion (HME) technique. A novel solubility improving agent plasdone s630 was utilized. The HME raltegravir was formulated into tablet by direct compression method. The prepared tablets were assessed for all pre and post-compression parameters. The drug- excipients interaction was examined by FTIR and DSC. All formulas displayed complying with pharmacopoeial measures. The study reveals that formula prepared by utilizing drug and plasdone S630 at 1:1.5 proportion and span 20 at concentration about 30mg (trail-6) has given highest dissolution rate than contrasted with various formulas of raltegravir.
Keywor
... Show MoreUndoubtedly, rutting in asphalt concrete pavement is considered a major dilemma in terms of pavement performance and safety faced by road users as well as the road authorities. Rutting is a bowl-shaped depression in the wheel paths that develop gradually with the increasing number of load applications. Heavy axle loadings besides the high pavement summer temperature enhance the problem of rutting. According to the AASHTO design equation for flexible pavements, a 1.1 in rut depth will reduce the present serviceability index of relatively new pavement, having no other distress, from 4.2 to 2.5. With this amount of drop in serviceability, the entire life of the pavement in effect has been lost. Therefore, it is crucial to look at the mechani
... Show MoreReflective cracking is one of the primary forms of deterioration in pavements. It is widespread when Asphalt concrete (AC) overlays are built over a rigid pavement with discontinuities on its surface. Thus, this research work aims to reduce reflection cracks in asphalt concrete overlay on the rigid pavement. Asphalt Concrete (AC) slab specimens were prepared in three thicknesses (4, 5, and 6 cm). All these specimens were by testing machine designed and manufactured at the Engineering Consulting Office of the University of Baghdad to examine for the number of cycles and loads needed to propagate the reflection cracking in the asphalt concert mixture at three temperatures (20, 30, and 30°C). It was noticed that the higher thickness A
... Show MoreThis research investigated the influence of water-absorbent polymer balls (WAPB) on reinforced concrete beams’ structural behavior experimentally. Four self-compacted reinforced concrete beams of identical geometric layouts 150 mm × 200 mm × 1,500 mm, reinforcement details, and compressive strength