This study involves the synthesis of a new class of silicon polymers, designated as P1-P7, derived from dichlorodimethylsilane (DCDMS) in combination with various organic compounds (Schiff bases prepared from different amines and appropriate aldehydes or ketones) [I-V] through condensation polymerization. The structures of all monomers and polymers were characterization by FTIR and 1HNMR spectroscopy (for some polymers). The results of thermogravimetric analysis (TGA) and differential scanning calorimetry DSC test show stable thermal behaviour. Polymers with a higher concentration of aromatic rings in their repeating structural units exhibited a higher temperature for weight loss, indicating increased thermal stability. Thermal measurements reflect the fact that all the polymers prepared in this study possess thermal stability, and the most thermally stable are the polymers that contain more phenyl rings. The inhibitory feature of the prepared polymers is studied through many tests, which include measuring the erosion rate through methods known as weight loss and scanning electron microscopy tests. In the weight loss method, the inhibiter gives good efficiency in protecting aluminium metal, to reach the inhibition efficiency to 83% using polymer P5 inhibitor with concentration of 0.15 in 0.1 M solution of NaOH. On the other hand, P4 it showed the lowest inhibition efficiency of 16.74% at a concentration of 0.05. Scanning electron microscopy (SEM) images showed that a high corrosion inhibition efficiency of the polymers in NaOH solution (0.1 M), while the metal surface under the corrosion containing the inhibitors showed lower corrosion than that which could be found on the same metal surface, that is located in a completely empty media of the barrier and also clearly showed the protective layer on the surface. Viscosity testing in dimethylsulfoxide solvent showed that the true viscosity increases three fold when the concentration increases from 0.1 to 0.7. The results also showed that copolymer P7 has a higher viscosity.
A new series of ?-D-glucose as Schiff bases derivatives is synthesized and characterized with studying their bioactivity. Hydroxyl groups at C (1,2&5,6) sugar moiety are converted into acetal form through a reaction with dry acetone using phosphoric acid and anhydrous zinc chloride as catalysts producing 1,2:5,6-di-O-isopropyledine ?-D-glucofuranose(I). The five memberd ring acetal of C(5,6) is hydrolyzed with acetic acid (65%)and a reaction of the new product with sodium periodate is carried on to get an aldehyde moiety which is used to produce a new series of Schiff bases through reacting with different amino compounds such as 4-amino antipyrene . The suggested chemical structures of the prepared compounds are confirmed by using UV., FT
... Show MoreAcetophenone sulfamethoxazole and 3-Nitrobenzophenone sulfamethoxazole were prepared from the reaction of sulfamethoxazole with two ketones. The prepared ligands were identified by (C.H.N) analysis and UV-VIS, FT-IR spectroscopic techniques. Metal complexes of the two ligands were prepared in an aqueous alcohol with Zn (II), Mn (II) and Cu (II) ions with a molar ratio1:1. The proposed general formula for the resulting complexes was [ML.CL2.H2O]H2O .The complexes were characterized by (C.H.N) technique , spectroscopic methods ,conductivity, atomic absorption ,magnetic susceptibility measurements and melting point. According to the results obtained, the suggested geometry is to be octahedral for all the complexes.
ABSTRACT
Naproxen(NPX) imprinted liquid electrodes of polymers are built using polymerization precipitation. The molecularly imprinted (MIP) and non imprinted (NIP) polymers were synthesized using NPX as a template. In the polymerization precipitation involved, styrene(STY) was used as monomer, N,N-methylenediacrylamide (N,N-MDAM) as a cross-linker and benzoyl peroxide (BPO) as an initiator. The molecularly imprinted membranes and the non-imprinted membranes were prepared using acetophenone(AOPH) and di octylphathalate(DOP)as plasticizers in PVC matrix. The slopes and detection limits of the liquid electrodes ranged from)-18.1,-17.72 (mV/decade and )4.0 x 10-
... Show MoreFour electrodes were synthesized based on molecularly imprinted polymers (MIPs). Two MIPs were prepared by using the diclofenac sodium (DFS) as the template, 2-hydroxy ethyl metha acrylate(2-HEMA) and 2-vinyl pyridine(2-VP) as monomers as well as divinyl benzene and benzoyl peroxide as cross linker and initiator respectively. The same composition used for prepared non-imprinted polymers (NIPs) but without the template (diclofenac sodium). To prepared the membranes electrodes used different plasticizers in PVC matrix such as: tris(2-ethyl hexyl) phosphate (TEHP), tri butyl phosphate (TBP), bis(2-ethyl hexyl) adipate (BEHA) and tritolyl phosphate (TTP). The characteristics studied the slop, detection limit, life time and linearity range of DF
... Show MoreWe discussed the proper preparation, directing, and implementation of physical education lessons, and clarification of the duties that fall upon the physical education teacher in addition to his physical and skill duties, which is the duty of the physical education lesson. The problem of the research lies in the fact that interactive harmonic exercises are not implemented accurately by physical education teachers because they require great experience, exceptional efforts, and accuracy in performance. The research aims to identify the level of some physical and motor abilities and intelligence among students aged (9-10) years, and to know the effect of some harmonic exercises. Interactivity at the level of some physical and motor abi
... Show MoreThe primary purpose of this paper is to introduce the, 2- coprobabilistic normed space, coprobabilistic dual space of 2- coprobabilistic normed space and give some facts that are related of them
The photooxidative degradation process of plastics caused by ultraviolet irradiation leads to bond breaking, crosslinking, the elimination of volatiles, formation of free radicals, and decreases in weight and molecular weight. Photodegradation deteriorates both the mechanical and physical properties of plastics and affects their predicted life use, in particular for applications in harsh environments. Plastics have many benefits, while on the other hand, they have numerous disadvantages, such as photodegradation and photooxidation in harsh environments and the release of toxic substances due to the leaching of some components, which have a negative effect on living organisms. Therefore, attention is paid to the design and use of saf
... Show MoreIn this work was prepared three different types of modified screen printed carbon electrode (SPCEs) with drops casted method, the used carbone nanomaterials were the MWCNT, functionalized –MWCNT (f-MWCNT) and After several experiments were made to find an appropriate ratio to make good GOT/f-MWCNT nanocomposite, and found the suspension mixture (1:1) from GOT/f-MWCNT (f-MWCNT-GOT). The electrical and physical properties were performed with cyclic voltammeter technique, and studied the maximum current response, the effective surface area, effect of the pH value and the determination of active surface area for MWCNT-SPCE , f-MWCNT-SPCE and f-MWCNT-GOT/SPCE as (0.04 cm2), (0.119 cm2) and (0.115 cm2) respectively, the surface coverage concent
... Show MoreIron oxide(Fe3O4) nanoparticles of different sizes and shapes were synthesized by solve-hydrothermal reaction assisted by microwave irradiation using ferrous ammonium sulfate as a metal precursor, oleic acid as dispersing agent, ethanol as reducing agent and NaOH as precipitating agent at pH=12. The synthesized Fe3O4 nano particles were characterized by X-ray diffraction (XRD), FTIR and thermal analysis TG-DTG. Sizes and shapes of Fe3O4 nanoparticles were characterized by Scanning Electron Microscopy (SEM), and atomic force microscopy (AFM).