Preferred Language
Articles
/
joe-623
Heat Transfer and Thermal Expansion of Coefficient EP -(MWCNT/x-TiO2)Nanocomposites
...Show More Authors

The thermal properties (thermal transfer and thermal expansion coefficient) of the enhanced epoxy resin (MWCNT / x-TiO2) were studied by weight ratios with the values (0%, 3%, 5%, 7% and 10%) and a constant ratio of 3% of MWCNT. The ultrasonic technology was used to prepare the neat and composites which were then poured into Teflon molds according to standard conditions. Thermo-analyzer sensor technology was used to measure thermal transfer (thermal conductivity, thermal flow, thermal diffusion, thermal energy and heat resistance). The thermal conductivity, flow, and thermal conductivity values were increased sequentially by increasing the weight ratio of the filler while the results of stored energy values and thermal resistance decreased by increasing the percentage of salts. The thermal mechanical analysis was used to measure thermal expansion and elasticity coefficient. The scanning electron microscopy was used to interpret the results of thermal analysis and distribution of the nanoparticle within the polymer matrix.

 

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Mon Aug 08 2022
Journal Name
Egyptian Journal Of Chemistry
Synthesis, Characterization, Spectroscopic, Thermal and Biological Studies for New Complexes with N1, N2-bis(3-hydroxyphenyl) Oxalamide
...Show More Authors

View Publication Preview PDF
Scopus (8)
Scopus Clarivate Crossref
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of addition ZrO2-Al2O3 nanoparticles mixture on some properties and denture base adaptation of heat cured acrylic resin denture base material
...Show More Authors

Background: The PMMA polymer denture base materials are low mechanical properties, adaptation of the denture base to underlying tissue is important for retention and stability of denture. The aim of the study was toevaluate the effect of mixtureZrO2-Al2O3 nanoparticles on impact strength, transverse strength, hardness, roughness, denture base adaptation of heat cured acrylic resin denture base material. Materials and methods: One hundred (100) specimens were prepared, the specimens were divided into five groups (20 specimens to each) according to the test type, each group was subdivided in to two subgroups (control and experimental) each subgroup consist of 10 specimens, the experimental group included mixture of 2% (ZrO2-Al2O3ratio2:1) b

... Show More
View Publication Preview PDF
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of glass flakes reinforcement on the surface hardness and surface roughness of heat-cured poly (methyl methacrylate) denture base material
...Show More Authors

Background: Heat-cured poly (methyl methacrylate) the principal material for the fabrication of denture base have a relatively poor mechanical properties. The aim of this study was to investigate the effect of glass flakes used as reinforcement on the surface hardness and surface roughness of the heat-processed acrylic resin material. Material and method: Glass flakes (product code: GF002) pretreated with silane coupling agent were added to Triplex® denture base powder using different concentrations. A total of 100 specimens of similar dimensions (65 x 10 x 2.5) mm were prepared, subdivided into 2 main groups of 50 specimens for each of the study tests. Ten specimens for the control group and 40 specimens for each of the experimental gro

... Show More
View Publication Preview PDF
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Zirconium Silicate Nanopowder Reinforcement on Some Mechanical and Physical Properties of Heat Cured Poly (Methyl Methacrylate) Denture Base Materials
...Show More Authors

Background: Polymethylmethacrylate (PMMA) has relatively unsatisfactory mechanical properties such as low flexural strength and impact strength also dimensional instability. Material and method: Zirconium silicate nanoparticles were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 1% and 1.5% by weight then mixed with powder using conventional procedure, (150) samples were prepared and divided into three groups, each group consisted of (50) samples, the first group prepared from PMMA without addition (control), another group with the addition of 1% wt Zrsio4 nanoparticles (experimental) and the third one with 1.5% wt Zrsio4 nanoparticles (experimental). Each group

... Show More
View Publication Preview PDF
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of silanized alumina nano -fillers addition on some physical and mechanical properties of heat cured polymethyl methacrylate denture base material
...Show More Authors

Background: Polymethyl methacrylate (PMMA) is the most commonly used material in denture fabrication. The material is far from ideal in fulfilling the mechanical requirements. Midline fracture; poor thermal conductivity and water sorption, are common problem in this material. The purpose of this study was to evaluate the effect of addition of surface treated Aluminum oxide nano fillers on some properties of heat cured (PMMA). Materials and methods: In addition to controlled group of heat cured PMMA the silanized (Al2O3) nanoparticles was added to PMMA powder by weight in three different percentages 1wt%, 2wt% and 3wt%, mixed by probe ultra-sonication machine. 200 specimens were constructed and divided into 5 groups according to the test (e

... Show More
View Publication Preview PDF
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of poly propylene fibers incorporation and their oxygen plasma treatment on tensile strength, wettability and wear resistance of heat cure denture base acrylic resin
...Show More Authors

Background: Recently, Poly propylene fibers with and without plasma treatment have been used to reinforce heat cure denture base acrylic but, so far some of properties like tensile strength , wettability and wear resistance not evaluated yet, the aim of the study is to clarify the influence of incorporation of treated and untreated fibers on these properties. Materials and methods: Twenty one specimens were fabricated for every tested property(tensile strength, wear resistance and wettability) that classified into three groups(control, untreated poly propylene fibers reinforced specimens and Oxygen plasma treated group)and for each test sevens amples were used(n=7). Tensile strength was tested using Instron universal testing machine, wear

... Show More
View Publication Preview PDF
Publication Date
Sun Jan 01 2017
Journal Name
Optics & Laser Technology
Finite element thermal analysis for PMMA/st.st.304 laser direct joining
...Show More Authors

This work is concerned with building a three-dimensional (3D) ab-initio models that is capable of predicting the thermal distribution of laser direct joining processes between Polymethylmethacrylate (PMMA) and stainless steel 304(st.st.304). ANSYS® simulation based on finite element analysis (FEA) was implemented for materials joining in two modes; laser transmission joining (LTJ) and conduction joining (CJ). ANSYS® simulator was used to explore the thermal environment of the joints during joining (heating time) and after joining (cooling time). For both modes, the investigation is carried out when the laser spot is at the middle of the joint width, at 15 mm from the commencement point (joint edge) at traveling time of 3.75 s. Process par

... Show More
View Publication
Scopus (47)
Crossref (43)
Scopus Clarivate Crossref
Publication Date
Thu Oct 01 2020
Journal Name
Ieee Transactions On Very Large Scale Integration (vlsi) Systems
Low-Power, Highly Reliable Dynamic Thermal Management by Exploiting Approximate Computing
...Show More Authors

With the continuous downscaling of semiconductor processes, the growing power density and thermal issues in multicore processors become more and more challenging, thus reliable dynamic thermal management (DTM) is required to prevent severe challenges in system performance. The accuracy of the thermal profile, delivered to the DTM manager, plays a critical role in the efficiency and reliability of DTM, different sources of noise and variations in deep submicron (DSM) technologies severely affecting the thermal data that can lead to significant degradation of DTM performance. In this article, we propose a novel fault-tolerance scheme exploiting approximate computing to mitigate the DSM effects on DTM efficiency. Approximate computing in hardw

... Show More
View Publication
Scopus (5)
Crossref (5)
Scopus Clarivate Crossref
Publication Date
Sun Jan 15 2023
Journal Name
Dental Hypotheses
Effect of addition of polymerized polymethyl methacrylate (PMMA) and zirconia particles on impact strength, surface hardness, and roughness of heat cure PMMA: An in vitro study
...Show More Authors

Introduction: This study was designed to examine the effects of addition of the combination of polymerized polymethyl methacrylate (PMMA) and zirconia (ZrO2) particles to heat cure PMMA resin on impact strength, surface hardness, and roughness. Methods: The 70% (w/w) of polymerized PMMA powder (particle size: 0.70mm) was mixed with 30% (w/w) of zirconia powder (ZrO2) (1mm) to produce PMMA-ZrO2 filler. Ninety acrylic specimens created were divided into three groups containing 0% wt (Control group), 2% wt, and 4% wt, PMMA-ZrO2 filler. Ten specimens were used for impact strength, surface hardness and roughness test, blindly. Data were analyzed via oneway ANOVA and the Tukey post hoc test using R 3.6.3. Results: There was statistically signific

... Show More
Publication Date
Mon Oct 06 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of thermocycling and different pH of artificial saliva on the impact and transverse strength of heat cure resin reinforced with silanated ZrO2 nano-fillers.
...Show More Authors

Background: The aim of this study was to evaluate the effect of thermo cycling and different pH of artificial saliva (neutral, acidic, basic) on impact and transverse strength of heat cure acrylic resin reinforced of with 5% silanated ZrO2 nano fillers. Materials and methods: 120 samples were prepared, 60 samples for impact strength test and another 60 samples for transverse strength test, for each test, samples were divided into two major groups (before and after thermo cycling), then each of these major groups were further subdivided into 3 subgroups according to the pH of prepared artificial saliva (neutral, acidic, basic). Charpy impact device was used for impact strength test and Flexural device was used for transverse strength test. R

... Show More