Direct Shear Behavior of Fiber Reinforced Concrete Elements
...Show More Authors

Improving the accuracy of load-deformation behavior, failure mode, and ultimate load capacity for reinforced concrete members subjected to in-plane loadings such as corbels, wall to foundation connections and panels need shear strength behavior to be included. Shear design in reinforced concrete structures depends on crack width, crack slippage and roughness of the surface of cracks.

This paper illustrates results of an experimental investigation conducted to investigate the direct shear strength of fiber normal strength concrete (NSC) and reactive powder concrete (RPC). The tests were performed along a pre-selected shear plane in concrete members named push-off specimens. The effectiveness of concrete compressive strength, volume fraction of steel fiber, and shear reinforcement ratio on shear transfer capacity were considered in this study. Furthermore, failure modes, shear stress-slip behavior, and shear stress-crack width behavior were also presented in this study.

Tests’ results showed that volume fraction of steel fiber and compressive strength of concrete in NSC and RPC play a major role in improving the shear strength of concrete. As expectedly, due to dowel action, the shear reinforcement is the predominant factor in resisting the shear stress. The shear failure of NSC and RPC has the sudden mode of failure (brittle failure) with the approximately linear behavior of shear stress-slip relationship till failure. Using RPC instead of NSC with the same amount of steel fibers in constructing the push-off specimen result in high shear strength. In NSC, shear strength influenced by the three major factors; crack surface friction, aggregate interlock and steel fiber content if present. Whereas, RPC has only steel fiber and cracks surface friction influencing the shear strength. Due to cementitious nature of RPC in comparisons with NSC, the RPC specimen shows greater cracks width.

It is observed that the Mattock model gives very satisfactory predictions when applied to the present test results with a range of parametric variations; ranging from 0 % to 0.5 % in steel fibers content; from 0 % to 0.53 % in transverse reinforcement ratio; from 15 to 105 MPa in compressive strength of concrete. While it gives a poor prediction for a specimen with 1% steel fiber.

 

View Publication Preview PDF
Quick Preview PDF
Publication Date
Sat Mar 01 2008
Journal Name
Iraqi Journal Of Physics
Mathematical Model of Amplified Stimulated Raman Scattering and Fiber Raman Amplifier
...Show More Authors

The result of a developed mathematical model for predicting the design
parameters of the fiber Raman amplifier (FRA) are demonstrated. The amplification
parameters are tested at different pump power with different fiber length. Recently,
the FRA employed in optical communication system to increase the repeater distance
as will as the capacity of the communication systems. The output results show, that
high Raman gain can be achieved by high pumping power, long effective area that
need to be small for high Raman gain. High-stimulated Raman gain coefficient is
recommended for high Raman amplifier gain, the low attenuation of the pump and the
transmitted signal in the fiber lead to high Raman gain.

View Publication Preview PDF
Publication Date
Fri Mar 28 2003
Journal Name
Journal Of Engineering
STABILITY OF UNREINFORCED AND REINFORCED EMBANKMENTS ON SOFT SOILS
...Show More Authors

Publication Date
Sun Jun 03 2012
Journal Name
Baghdad Science Journal
Mechanical properties of carbon nanotube reinforced Epoxy Resin composites
...Show More Authors

Overlapped have been prepared from epoxy resin material added to carbon Nanotube and percentages weight (0.1, 0.05, 0.01) % Studied the mechanical properties of the composite (bending, tensile an d hardness) has been found that the Flexural and tensile modulus of the composites were higher than the pure epoxy resin this may be due to the high mechanical strength of carbon nano tube (CNT). The hardness of the epoxy carbon Nanotube composites increased and the reason is due to increased overlap and stacking between the additives and material basis, which reduces the movement of polymer molecules leading to increased resistance to scratching material and cutting, will become more resistance to plastic deformation.

View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Mon Jun 01 2020
Journal Name
Iraqi Journal Of Physics
A Calculation real abundance of gaseous elements of the comet PanSTARRS C/2011 S4
...Show More Authors

    X-ray emission contains some of the gaseous properties is produced when the particles of the solar wind strike the atmosphere of comet ISON and PanSTARRS Comets. The data collected with NASA Chandra X-ray Observatory of the two comets, C/2012 S1 (also known as Comet ISON) and C/2011 S4 (Comet PanSTARRS) are used in this study.

   The real abundance of the observed X-ray spectrum elements has been extracted by a new simple mathematic model. The study found some physical properties of these elements in the comet’s gas such as a relationship between the abundance with emitted energy. The elements that have emission energy (2500-6800) eV, have abundance (0.1-0.15) %, while the elements

... Show More
View Publication Preview PDF
Crossref
Publication Date
Wed Dec 01 2010
Journal Name
Al-khwarizmi Engineering Journal
Properties of High Performance Concrete
...Show More Authors

The research deals with a new type of high-performance concrete with improved physical properties, which was prepared by using metal additives minutes (Metakaolin) and by studing their impact on the properties of mortar and concrete high-performance through destructive and non destructive tests. This type of concrete is used broadly in public buildings and in other structures . The research involved a number of experiments such as finding the activity index of burned at a temperature of 750 º C according to the standard ( ASTM C-311/03), as well as casting models for the cubic mortar mixtures and concrete containers at different rates of metakaolin ranging between (5% - 20%) as an added part to the cement mix to get a high- compressive

... Show More
View Publication Preview PDF
Publication Date
Sat Jan 01 2022
Journal Name
International Journal Of Clinical Dentistry
THE EFFECT OF A PROTECTIVE BARRIER ON THE SHEAR BOND STRENGTH OF DIFFERENT ORTHODONTIC BRACKETS
...Show More Authors

Background and objectives: This study aimed at testing the effect of plastic sleeve or barrier, used to cover the guide of the light cure unit to prevent cross-infection, on the shear bond strength and site of bond failure of stainless steel and ceramic orthodontic brackets. Materials and methods: Forty orthodontic brackets; twenty stainless steel and twenty ceramic brackets bonded to forty extracted human maxillary first premolars using light cure adhesive cured with and without the use of a protective plastic barrier on the guide. Comparing the effect of this barrier on the shear bond strength and adhesive remnant index was performed using an independent t-test and Chi-square test. Results: The protective barrier had decreased the shear b

... Show More
Scopus (3)
Scopus
Publication Date
Wed Feb 20 2019
Journal Name
Iraqi Journal Of Physics
The effect of volume fraction on the fatigue strength of unsaturated polyester / glass fiber composite
...Show More Authors

 In this work polymeric composites were done from unsaturated polyester as a matrix reinforced with glass fiber type (E-glass) with two different volume fraction 20% & 40%. Fatigue tests showed that the number of fatigue cycles to failure limit for samples reinforced with uniform (woven Roving 0-90°) E-glass fiber and random (continuous fibers) with volume fraction 40% more than that for the same samples with volume fraction 20%. Also the fatigue results showed that the uniform samples failed with fatigue cycles more than that of random.

View Publication Preview PDF
Crossref
Publication Date
Sat Jan 01 2022
Journal Name
Journal Of The Mechanical Behavior Of Materials
Response of composite steel-concrete cellular beams of different concrete deck types under harmonic loads
...Show More Authors
Abstract<p>This study aims to investigate the adequacy of composite cellular beams with lightweight reinforced concrete deck slab as a structural unit for harmonic loaded buildings. The experimental program involved three fixed-ends supported beams throughout 2140 mm. Three concrete types were included: Normal Weight Concrete (NWC), Lightweight Aggregate Concrete (LWAC), and Lightweight Fiber Reinforced Aggregate Concrete (LWACF). The considered frequencies were (5, 10, 15, 20, 25, and 30) Hz. It was indicated that the harmonic load caused a significant influence on LWAC response (64% greater than NWC) and lattice cracks were observed, especially at 30 Hz. As for LWACF slab, no cracks appeared, </p> ... Show More
Scopus (4)
Crossref (4)
Scopus Clarivate Crossref
Publication Date
Thu Nov 01 2012
Journal Name
Journal Of Cosmetics, Dermatological Sciences And Applications
Direct melanocytes transplant from normal donor area into vitiliginous recipient area by dermabrasion technique
...Show More Authors

KE Sharquie, AA Noaimi, HA Al-Mudaris, Journal of Cosmetics, Dermatological Sciences and Applications, 2012 - Cited by 6

View Publication
Publication Date
Sun Mar 07 2010
Journal Name
Baghdad Science Journal
The Direct Gene Injection Using of Egg Yolk Emulsion as Carrier and its Comparison with Liposomes.
...Show More Authors

The efficiency of egg yolk emulsion in coating DNA and its delivery across cellular membranes was evaluated in comparison with liposomes DOPE . The murine leukemia viral oncogene v-abl , cloned on pBR322 was used as a DNA substrate for direct injection into mice tissue . the DNA complexes were prepared by mixing the DNA with egg yolk emulsion and liposome . Each was directly injected into mice peritoneal cavity with proper control. The gene delivery was examined phenotypically by blood analysis and cytogenetic analysis . Chromosomal changes were detected in the bone marrow as from the fourth day post inoculation through the eleventh day when chromosomal ring s could be seen . this was accompanied by decrease in the WBC count ,

... Show More
View Publication Preview PDF
Crossref