Preferred Language
Articles
/
joe-397
Studying of Some Mechanical Properties of Reactive Powder Concrete Using Local Materials
...Show More Authors

This research aims to investigate and evaluate a reactive powder concrete (RPC) cast using economical materials. Its mechanical properties were investigated and evaluated by studying the effects of using different cement and silica fume contents and locally steel fibers aspect ratios as reinforcement for this concrete. A compressive strength of about 155.2MPa, indirect tensile strength of 16.0MPa, modulus of elasticity of 48.7GPa, flexural strength of 43.5MPa, impact energy of 3294.4kN.m and abrasion loss 0.59%  have been achieved for reinforced RPC contains  910 kg/m3 cement content, silica fume content 185 kg/m3 of cement weight and fiber volume fraction 2%. The water absorption values were 1.5 times higher for the normal strength concrete in comparison with the reactive powder concrete.

                                                                    

 

View Publication Preview PDF
Quick Preview PDF
Publication Date
Thu Mar 01 2018
Journal Name
Materials Today Communications
Improved mechanical properties of sol-gel derived ITO thin films via Ag doping
...Show More Authors

View Publication
Scopus (24)
Crossref (28)
Scopus Clarivate Crossref
Publication Date
Wed Dec 30 2020
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Experimental Investigation of Pomegranate Peel and Grape Seed Powder Additives on the Rheological and Filtration Properties of Un-Weighted WBM
...Show More Authors

   The chemical additives used to enhance the properties of drilling mud cause damage to humans and the environment. Therefore, it is necessary to search for alternative additives to add them to the drilling mud. Thus, this study investigates the effects of pomegranate peel and grape seed powders as natural waste when added to un-weighted water-based mud. The test includes measurements of the rheological properties and filtration, as well as the alkanity and density of the drilling mud. The results showed a decrease in PH values ​​with an increase in the concentrations of pomegranate peel or grapeseed, and a decrease in mud density with an increase in powders of pomegranate peel and grape seed concentrations that resulted f

... Show More
View Publication Preview PDF
Crossref (3)
Crossref
Publication Date
Sat Aug 31 2019
Journal Name
Iraqi Journal Of Physics
The Q-switched Nd:YAG laser shock processing effects on mechanical properties of C86400 Cu-Zn alloy: Q-switched Nd:YAG laser shock processing effects on mechanical properties of C86400 Cu-Zn alloy
...Show More Authors

The aim of this paper is to investigate the effects of Nd:YAG laser shock processing (LSP) on micro-hardness and surface roughness of 86400Cu-Zn alloy. X-ray fluorescence technique was used to analyze the chemical composition of this alloy. LSP treatment was performed with a Q-switched Nd: YAG laser with a wavelength of 1064 nm. The results show that laser shock processing can significantly increase. The micro-hardness and surface roughness of the LSP-treated sample. Vickers diamond indenter was used to measure the micro-hardness of all samples with different laser pulse energy and the different number of laser pulses. It is found that the metal hardness can be significantly increased to more than 80% by increasing the laser energy and t

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Sat Apr 01 2023
Journal Name
Journal Of Engineering
Manufacture of Load Bearing Concrete Masonry Units Using Waste Demolishing Material
...Show More Authors

The presence of construction wastes such as clay bricks, glass, wood, plastic, and others in large quantities causes serious environmental problems in the world. Where these wastes can be used to preserve the natural resources used in construction and reduce the impact of this problem on the environment, it also works to reduce the problem of high loads of concrete blocks. Clay bricks aggregate (AB) can be recycled as coarse aggregate and replaced with volumetric proportions of coarse aggregate by ( 5% and 10%), as well as the use of clay brick powder (PB) by replacing its weight of cement (5% and 10%) and reduced in the manufacture of concrete blocks (blocks). Four mixtures will be prepared and tested to learn how to re

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Sat Aug 01 2020
Journal Name
Key Engineering Materials
Quality Control of Production Lightweight Ferrocement Plate Using Sustainable Materials
...Show More Authors

This research is concerned with a new type of ferrocement characterized by its lower density and enhanced thermal insulation. Lightweight ferrocement plates have many advantages, low weight, low cost, thermal insulation, environmental conservation. This work contain two group experimental : first different of layer ferrocement, second different of ratio aggregate to cement. The experiments were made to determined the optimum proportion of cement and lightweight aggregate (recycle thermestone ). A low W/C ratio of 0.4 was used with super plasticizer conforming to ASTM 494 Type G. The compressive strength of the mortar mixes is 20-25 MPa. The work also involved the determination of thermal properties .Thermal conductivity value of thi

... Show More
View Publication
Crossref (2)
Crossref
Publication Date
Sun Mar 01 2020
Journal Name
Journal Of Engineering
The effect of titanium oxide microparticles on mechanical properties, absorption and solubility processes of a glass ionomer cement
...Show More Authors

Glass Ionomer Cement (GIC) is one of the important dental temporary filing materials. The aim of this study is to evaluate the effect of adding 3, 5 and 7 wt. % of TiO2 microparticles to conventional GIC powder (Riva Self Cure) on mechanical properties and its effect on absorption and solubility processes. TiO2 particles additives improved compressive strength and biaxial flexural strength, where the compressive strength increased with increasing in the added ratio, while the highest value of the biaxial flexural strength was at 3 wt.%. The addition of TiO2 particles improved the surface Vickers microhardness values, with highest value at 5 wt. %. On other hand TiO2 addition im

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Sun Sep 04 2016
Journal Name
Baghdad Science Journal
Study the Shielding Properties against Gamma-rays for Epoxy Resin Reinforced by Different materials
...Show More Authors

In the present work the Buildup factor for gamma rays were studied in shields from epoxy reinforced by lead powder and by aluminum powder, for NaI(Tl) scintillation detector size ( ×? ), using two radioactive sources (Co-60 and Cs-137). The shields which are used (epoxy reinforced by lead powder with concentration (10-60)% and epoxy reinforced by aluminum powder with concentration (10-50)% by thick (6mm) and epoxy reinforced by lead powder with concentration (50%) with thick (2,4,6,8,10)mm. The experimental results show that: The linear absorption factor and Buildup factor increase with increase the concentration for the powders which used in reinforcement and high for aluminum powder than the lead powder and decrease with inc

... Show More
View Publication Preview PDF
Crossref
Publication Date
Mon May 31 2021
Journal Name
Iraqi Geological Journal
Mechanical Rock Properties Estimation for Carbonate Reservoir Using Laboratory Measurement: A Case Study from Jeribe, Khasib and Mishrif Formations in Fauqi Oil Field
...Show More Authors

Estimation of mechanical and physical rock properties is an essential issue in applications related to reservoir geomechanics. Carbonate rocks have complex depositional environments and digenetic processes which alter the rock mechanical properties to varying degrees even at a small distance. This study has been conducted on seventeen core plug samples that have been taken from different formations of carbonate reservoirs in the Fauqi oil field (Jeribe, Khasib, and Mishrif formations). While the rock mechanical and petrophysical properties have been measured in the laboratory including the unconfined compressive strength, Young's modulus, bulk density, porosity, compressional and shear -waves, well logs have been used to do a compar

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Sun Dec 01 2019
Journal Name
Journal Of Engineering
Analysis of Prosthetic Running Blade of Limb Using Different Composite Materials
...Show More Authors

Prostheses are used as an alternative to organs lost from the body. Flex-Foot Cheetah is considered one of the lower limb prostheses used in high-intensity activities such as running. This research focused on testing two samples of Flex-Foot Cheetah manufactured of two various materials (carbon, glass) with polyester and compare between them to find the foot with the best performance in running on the level of professional athlete. In the numerical analysis, the maximum principal stress, maximum principal elastic strain, strain energy; finally, the blade total deformation were calculated for both feet. In experimental work, the load-deflection test was done for foot to calculate the bending the results were very close to

... Show More
View Publication Preview PDF
Crossref (16)
Crossref
Publication Date
Wed Sep 01 2021
Journal Name
Iop Conference Series: Earth And Environmental Science
Post Fire Residual Concrete and Steel Reinforcement Properties
...Show More Authors

he paper presents the results of exposure of normal concrete to high temperatures (400 and 700°C). In addition to the exposure of steel reinforcement bar Ø 12 mm, where two types of steel reinforcement burning situations were performed. Directly exposed to high temperatures (400 and 700°C) and others were covered by concrete layer (15 mm). From the experimental results of fire exposure for 1 hour of 400 and 700°C and gradually cooled, it was found that the residual average percentage of compressive strength of concrete was 85.3 and 41.4%, while the residual average percentage of modulus of elasticity of concrete was 75 and 48%, respectively. The residual average percentage of yielding tensile stress (Ø 12 mm) after burning and cooling

... Show More
View Publication Preview PDF
Scopus (5)
Crossref (4)
Scopus Crossref