Experimental research was carried out on eight reinforced concrete beams to study the embedded length of the longitudinal reinforcement. Six beams were casted using self compacted concrete, and the two other beams were casted using normal concrete. The test was carried out on beams subjected to two point loads. The strain and the slip of the main reinforcement have been measured by using grooves placed during casting the beams at certain places. The measured strain used to calculate the longitudinal stresses (bond stress) surrounding the bar reinforcement, The study was investigated the using of self compacted concrete SCC on the embedded length of reinforcing bars, and comparing the results with normal concrete. The test results show that using SCC improve the concrete properties like the compressive strength and the tensile strength which mainly affected the bond strength and the splitting of the concrete cover failure. The testes show that with increasing concrete strength the bond strength increased.
In the period after the collapse of the Soviet Union in 1991, the Federal Republic of Russia witnessed a setback in the overall strategic performance of the country, as it went through a stage of performance flop between the orientation towards Europe in the era of President Boris Yelsen (1991-1999), or the change of direction towards Eurasia, as the Russian Federation managed After President Vladimir Putin assumed power in 2000, from rebuilding the same state and preserving national unity and social cohesion, as well as building a phased military doctrine that made clear moves in Russian strategic thought and future directions towards regions of eternal importance in Russian strategic perception Lack of a set of motivations based on it:
... Show MoreThe ability to inhibit corrosion of low carbon steel in a salt solution (3.5%NaCl) has been checked with three real expired drugs (Cloxacillin, Amoxicillin, Ceflaxin) with variable concentrations (0, 250, 500, 750) mg/L were examined in the weight loss. The inhibition efficiency of the Cloxacillin 750 mg/L showed the highest value (82.8125 %) and the best inhibitor of the rest of the antibiotics. The different concentrations of Cloxacillin drug (0, 250, 500, 750) mg/L and temperature (25, 35, 45, 55) oC were studied as variables with potentiodynamic polarization, Scanning Electron Microscopy (SEM) for surface morphology and electrochemical impedance spectroscopy (EIS) depending on current values and the resistance of charge to
... Show MoreTwo nanocomposite corrosion inhibitors were synthesized from Aloe vera extract: one incorporating sodium thiosulfate and the other silver nitrate. Both nanocomposites were subjected to structural characterization using atomic force microscopy (AFM), which revealed distinct morphological features. The sodium thiosulfate-based nanocomposite exhibited uniform and well-dispersed nanoparticles with an average size of 47.51 nm, suggesting a stable and homogeneous distribution. In contrast, the silver nitrate-based nanocomposite displayed slightly larger particles with an average diameter of 58.34 nm, indicating a tendency toward moderate aggregation. The corrosion inhibition performance of these nanocomposites for carbon steel (CS1137) was invest
... Show MoreTwo nanocomposite corrosion inhibitors were synthesized from Aloe vera extract: one incorporating sodium thiosulfate and the other silver nitrate. Both nanocomposites were subjected to structural characterization using atomic force microscopy (AFM), which revealed distinct morphological features. The sodium thiosulfate-based nanocomposite exhibited uniform and well-dispersed nanoparticles with an average size of 47.51 nm, suggesting a stable and homogeneous distribution. In contrast, the silver nitrate-based nanocomposite displayed slightly larger particles with an average diameter of 58.34 nm, indicating a tendency toward moderate aggregation. The corrosion inhibition performance of these nanocomposites for carbon steel (CS1137) was invest
... Show MoreIn the 1980s, the French Administration Roads LCPC developed high modulus mixtures (EME) by using hard binder. This type of mixture presented good resistance to moisture damage and improved mechanical properties for asphalt mixtures including high modulus, good fatigue behaviour and excellent resistance to rutting. In Iraq, this type of mixture has not been used yet. The main objective of this research is to evaluate the performance of high modulus mixtures and comparing them with the conventional mixture, to achieve this objective, asphalt concrete mixes were prepared and then tested to evaluate their engineering properties which include moisture damage, resilient modulus, permanent deformation and fatigue characteristics. These pro
... Show MoreCurrent design codes and specifications allow for part of the bonded flexure tension reinforcement to be distributed over an effective flange width when the T-beams' flanges are in tension. This study presents an experimental and numerical investigation on the reinforced concrete flanged section's flexural behavior when reinforcement in the tension flange is laterally distributed. To achieve the goals of the study, numerical analysis using the finite element method was conducted on discretized flanged beam models validated via experimentally tested T-beam specimen. Parametric study was performed to investigate the effect of different parameters on the T-beams flexural behavior. The study revealed that a significant reduction in the
... Show MoreStraight tendons in pretensioned members can cause high-tensile stresses in the concrete extreme fibers at end sections because of the absence of the bending stresses due to self-weight and superimposed loads and the dominance of the moment due to prestressing force alone. Accordingly, the concrete tensile stresses at the ends of a member prestressed with straight tendons may limit the service load capacity of the member. It is therefore important to establish limiting zone in the concrete section within which the prestressing force can be applied without causing tension in the extreme concrete fibers. Two practical methods are available to reduce the stresses at the end sections due to the prestressing force. The first method based
... Show MoreIn the 1980s, the French Administration Roads LCPC developed high modulus mixtures (EME) by using hard binder. This type of mixture presented good resistance to moisture damage and improved . mechanical properties for asphalt mixtures including high modulus, good fatigue behaviour and excellent resistance to rutting. In Iraq, this type of mixture has not been used yet. The main objective of this research is to evaluate the performance of high modulus mixtures and comparing them with the conventional mixture, to achieve this objective, asphalt concrete mixes were prepared and then tested to evaluate their engineering properties which include moisture damage, resilient modulus, permanent deformation and fatigue characteristics. These prope
... Show More