The permanent deformation of flexible pavement represent serious problem in hot climate region. Numerous efforts are devoted to mitigate this distress such as modifying asphalt binder by polymers. The present study demonstrate the effect of utilizing four types of polymers to reduce the permanent deformation, these polymers are Polyethylene Wax (PEW), Styrene Butadiene Rubber (SBR), Ethylene Propylene Dien Monomer (EPDM) and Ethylene Vinyl Acetate (EVA). The prepared mixtures composed of 4.9 % of 40/50 asphalt binder, 12.5 mm nominal aggregate maximum size and limestone dust as filler. The permanent and resilient strains have been recorded when the cylindrical specimens, 101.6 mm in diameter and 203.2 mm in height, tested by repeated loading system. The main conclusions exhibit that SBR and EPDM with the same concentration (15 % by weight of asphalt binder) reduced the permanent deformation by 30.20 % and 30.46 % respectively. Although, the PEW and EVA reduced permanent deformation by lower values, 13.24 % and 17.35 % respectively, but the incremental percentage of their action are higher. The influences of testing temperature and stress level on permanent deformation were investigated. Linear regression model was established to correlate the values of permanent deformation and the resilient modulus of asphalt mixtures.
This research was to determine the effect of rare earth metal (REM) on the as-cast microstructure of Mg-4Al alloy. The rare earth metal used here is Lanthanum to produce Mg-4Al-1.5La alloy. The microstructure was characterized by optical microscopy. The phases of this alloy were identified by X-ray diffraction. The microstructure of Mg-4Al consists of α-Mg and grain boundaries with precipitated phase particles. With the addition of Lanthanum, three distinct phases were identified in the X-ray diffraction patterns of the as cast Mg-4Al-1.5La: Mg, Al11La3, Al4La. The Mg17Al12 phase was not detected. The addition of Lanthanium increases the hardness and dec
... Show MoreStudy the effect of additives polymer polyvinyl alcohol (PVA) after solving in water by concentration 10% since represent a standard of PVA solution with added to cement – silica composite of ratio (1:2) with 5%, 10%, 15%, 20%, and 25% respectively to the standard quantity of water which using as a mortar of building. The results are demonstrate increasing on compression resistance with increase of PVA solution until 20%, and decreasing of thermal conductivity which represent a composite are increasing in thermal insulating. The results were recommended decreasing of water absorption with increase of PVA solution ratio as illustrated in this study.
In this study, the effect of construction joints on the performance of reinforced concrete beams was experimentally investigated. Seven beam specimens, with dimensions of 200×100×1000 mm, were fabricated. The variables were considered including; the location and configuration of the joints. One beam was cast without a joint (Reference specimen), two specimens were fabricated with a one horizontal joint located either at tension, or compression zone. The fourth
beam had two horizontal joints placed at tension, and compression area. The remaining specimens were with one or two inclined joints positioned at the shear span or beam’s mid-span. The specimens were subjected to a monotonic central concentrated loading until the failure. T
MR Younus, Nasaq Journal, 2022
Background: Methotrexate (MTX) was one of the first drugs synthesized for a specific chemotherapeutic purpose used to inhibit folic acid (FA) for the treatment of acute lymphoblastic leukemia in children. Its history is closely related to the discovery and characterization of folic acid. It is used clinically in medicine to treat a range of cancerous and noncancerous conditions. MTX is currently used in gynecology to treat disorders arising from trophoblastic tissue, namely, ectopic pregnancy. MTX, the most frequently used diseasemodifying anti-rheumatic drug (DMARD), suppresses disease activity and reduces joint damage. The aim of study: It is designed to demonstrate the effect of MTX (7.5 mg/wk.) on the histogenesis of gonad (testis) of n
... Show MoreThe present work aimed to study the SiO2μPs, and NPs effect on the biodegradability of St/PVA blends. The samples were prepared by casting method as PVA, St/PVA blends with different concentrations (30, 40, 50, and 60 %). FTIR test was carried out for the samples preparation. The results proved some changes which might be related to changing in crystallinity of St/PVA matrix as well as physical incorporation of SiO2 μPs, and NPs addition. The enzymatic test and water uptake results proved that increase in weight loss with increases of starch ratio. The lowest weight loss was PVA; the highest weight loss is 60% St/PVA whereas the lowest weight loss is 30%St/PVA for blends involved. SiO2μPs (753.7 nm), and NPs (263.1 nm) were added at d
... Show MoreTunnel construction below or adjacent to piles will affect the performance and eventually the stability of piles due to ground deformation resulting in the movement of piles and changes in the axial force distribution along the piles. A three dimensional finite element analysis using PLAXIS 3D (2013) was performed to study the behaviour of a single pile and 3 x 3 piles group during the advancement of shield tunnelling in ground. The 10-node tetrahedral elements were used to model both the soil and the tunnel lining. The Hardening Soil (HS) model was used to simulate the soil structure interaction at the tunnel-soil interface. An isotropic elastic model was used for the pile, piles
High temperature superconductors with a nominal composition HgBa2Ca2Cu3O8+δ
for different values of pressure (0.2,0.3, 0.5, 0.6, 0.9, 1.0 & 1.1)GPa were prepared by
a solid state reaction method. It has been found that the samples were semiconductor
P=0.2GPa.while the behavior of the other samples are superconductor in the rang
(80-300) K. Also the transition temperature Tc=143K is the maximum at P is equal to
0.5GPa. X-ray diffraction showed a tetragonal structure with the decreasing of the
lattice constant c with the increasing of the pressure. Also we found an increasing of
the density with the pressure.
In the present research, the chemical washing method has been selected using three chelating agents: citric acid, acetic acid and Ethylene Diamine Tetraacetic Acid (EDTA) to remove 137Cs from two different contaminated soil samples were classified as fine and coarse grained. The factors that affecting removal efficiency such as type of soil, mixing ratio and molarity have been investigated. The results revealed that no correlation relation was found between removal efficiency and the studied factors. The results also showed that conventional chemical washing method was not effective in removing 137Cs and that there are further studies still need to achieve this objective.