In this paper, the behavior of spliced steel girders under static loading is investigated. A group of seven steel I-girders were tested experimentally. Two concentrated loads were applied to each specimen at third points and the load was increased incrementally up to the yield of the specimen. Two types of splices were considered; the bearing type and the friction-grip type splices. For comparison, an analytical study was made for the tested girders in which the finite element analysis program (Abaqus) was used for analysis. It was found that the maximum test load for spliced girders with bearing type splices was in the range of (34%) to (67%) of the maximum test load for the reference girder. For girders spliced by using friction-grip type splices, the maximum test load was in the range of (90%) to (99%) of the maximum test load for the reference girder. The analytical results show a good agreement with the experimental results with a difference in maximum deflection at midspan was not more than (15%) at maximum load for all girders.
In this research, the effects of both current and argon gas pressure on the bending properties of welded joints were studied. Using the possible ranges of welding gas pressures and currents, Tungsten inert gas welding (TIG) of stainless steel (304) sheet was used to obtain their influence on the maximum bending force of the (TIG) welded joints. Design of experiment (DOE) ‘version 10' was used to determine the design matrix of experiments depending on the used levels of the input factors. Response surface methodology (RSM) technique was used to obtain an empirical mathematical model for the maximum bending force as a function of welding parameters (Current and Argon gas pressure). Also, the analysis of variance (ANOVA) was used to verif
... Show MoreThis work investigates the effect of the gas nitriding process on the surface layer microstructure and mechanical properties for steel 37, tool steel X155CrVMo12-1 and stainless steel 316L. Nitriding was conducted at a temperature of 550 °C for 2 hours during the first stage and at 750 °C for 4 hours during the second stage. SEM and X-ray diffraction tests were performed to evaluate the microstructural features and the major phases formed after surface treatment. SEM and X-ray diffraction tests were performed to assess the microstructural features and the primary phases formed after surface treatment. The new secondary precipitates were identified as γ′-Fe4N, ε (Fe2–3N), and α-Fe, exhibiting an uneven chain-like pattern wit
... Show MoreThe main factors that make it possible to get the corrosion of reinforcing steel in concrete are chloride ions and the absorption of carbon dioxide from the environment, and each of them works with a mechanism which destroys the stable immunity of rebar in the concrete. In this work the effect of carbon dioxide content in the artificial concrete solution on the corrosion behavior of carbon steel reinforcing bar (CSRB) was studied, potentiostatically using CO2 stream gas at 6 level of concentrations; 0.03 to 2.0 weight percent, and the effect of rising electrolyte temperature was also followed in the range 20 to 50ᴼ C. Tafel plots and cyclic polarization procedures were obeyed to investigate the c
... Show MoreIn this study, geopolymer mortar was designed in various experimental combinations employing 1% micro steel fibers and was subjected to different temperatures, according to the prior works of other researchers. The geopolymer mortar was developed using a variety of sustainable material proportions (fly ash and slag) to examine the influence of fibers on its strength. The fly ash weight percentage was 50%, 60%, and 70% by slag weight to study its effect on the geopolymer mortar's properties. The optimal ratio produced the most significant results when mixed at a 50:50 ratio of fly ash and slag with 1% micro steel fibers at curing temperature 240oC for 4 hours through two days. The compressive strength of the geopolymer mortar increas
... Show MoreIn this study, the effect of the combination of micro steel fibers and additives (calcium hydroxide and sodium carbonate) on the size of cracks formation and healing them were investigated. This study aims to apply the use of self-healing phenomenon to repair cracks and to enhance the service life of the concrete structures. Micro steel fibers straight type were used in this research with 0.2% and 0.4% by volume of concrete. A weight of 20 and 30 kg/m3 of Ca(OH)2 and 2 and 3 kg/m3 of Na2CO3 were used as a partial cement replacement. The results confirm that the concrete cracks were significantly self-healed up to 30 days re-curing. Cracks width up to 0.2 mm were comp
... Show MoreThis study investigated the structural behavior of a beam–slab member fabricated using a steel C-Purlins beam carrying a profile steel sheet slab covered by a dry board sheet filled with recycled aggregate concrete, called a CBPDS member. This concept was developed to reduce the cost and self-weight of the composite beam–slab system; it replaces the hot-rolled steel I-beam with a steel C-Purlins section, which is easier to fabricate and weighs less. For this purpose, six full-scale CBPDS specimens were tested under four-point static bending. This study investigated the effect of using double C-Purlins beams face-to-face as connected or separated sections and the effect of using concrete material that contains different recycled
... Show MoreIn order to evaluate the performance of introduced varieties of maize and test them under different levels of plant density, and to determine which of the introduced varieties give a high yield and at what plant density, a field experiment was carried out at Station A in the Department of Field Crops- College of Agricultural Engineering Sciences - University of Baghdad- Jadiriyah, for the fall season 2021, the RCBD design was used with four replications, in a split plot arrangement, the three plant densities (50.000, 70.000, and 90.000 Plant s ha-1) were the main plates, while the varieties represented the secondary factor, which is six varieties of maize, class 2 = 5783 DKC, Class 3 = 6315 DKC, Class 4= 6590 DKC, whic
... Show MoreThe study aims to review the literature on the fundamental changes in Managerial Accounting (MA) in light of accelerating Digital Transformations (DT) and increasing Sustainability Requirements (SR) from 2020 to August 2025, with the purpose of informing researchers and professionals about recent developments. The study relied on a qualitative analysis of the content of a group of studies indexed in the Scopus database. The study included a literature review of topics such as artificial intelligence tools and techniques, cloud computing, linear programming, sustainability reporting, and strategic managerial accounting practices. The study results revealed that accelerated DT improves the efficiency of managerial accounting practices
... Show More