Industrial development has recently increased, including that of plastic industries. Since plastic has a very long analytical life, it will cause environmental pollution, so studies have resorted to reusing recycled waste plastic (sustainable plastic) to produce environmentally friendly concrete (green concrete). In this research, producing environmentally friendly load-bearing concrete masonry units (blocks) was considered where five concrete mixtures were compressed at the blocks producing machine. The cement content reduced from 400 kg/m3 (B-400) to 300 kg/m3 (B-300) then to 200 kg/m3 (B-200). While (B-380) was produced using 380 kg/m3 cement and 20 kg/m3 nano-silica sand powder, and 10% plastic waste instead of coarse aggregate. Finally (B-285) included 285 kg/m3 cement and 15 kg/m3 nano silica sand powder and 10% plastic waste replacement for coarse aggregate. All production of concrete masonry unit types. According to IQS 1077 /1987, except (B-200) and (B-285) type B. When increasing the curing age from 14 to 28 days, blocks (B-285and B-380) change from type B to A. The compressive strength of the types (B-400, B-300, B-200, B-380, and B-285) was (9.65, 7.11, 5.35, 6.57, and 5.86) MPa, respectively, at 14 days and (11.98, 9.33, 6.84, 8.62 and 7.64) MPa respectively at 28 days.
Tests were performed on Marshall samples and were implemented for permanent deformation and resilient modulus (Mr) under indirect tensile repeated loading (ITRL), with constant stress level. Two types of liquid asphalt (cutback and emulsion) were tried as recycling agents, aged materials that were reclaimed from field (100% RAP), samples were prepared from the aged mixture, and two types of liquid asphalt (cutback and emulsion) with a weight content of 0.5% were utilized to prepare a recycled mixture. A group of twelve samples was prepared for each mixture; six samples were tested directly for ITRL test (three samples at 25˚C and three samples at 40˚C), an average value for ITRL for every three samples was calculated (
... Show MoreProtease enzyme production was studied and optimized as a first step to collect information about solid state fermenter) to produce protease enzyme. A local isolated Aspergillus niger was used for this study with constant spores feeding in every experiment at (105/g). Experiments carried out in conical flasks with (250 ml) containing (10 g) of wheat straw as a substrate with different conditions included temperature, pH, hydration ratio, and fermentation time, the results comprised by measuring protease activity (u). The results showed that the best activity can be obtained at (T = 32°C, t= 100 hrs, pH= 2.5 and hydration ratio is 1:3). On the other hand the results is courage to p
... Show MoreThe action of high repeated trucks load associated with dramatically elevated ambient temperatures leads to the most harmful distress in asphalt pavements occurred in Iraq known as rutting. Essentially, it is produced from the accumulation of irrecoverable strains, which mainly occurred in the asphalt layers. That visually demonstrated as a longitudinal depression in the wheel paths as well as small upheavals to the sides. Poly Phosphoric Acid (PPA) has been used as a means of producing modified asphalt binders and the interest to use it has increased in recent years. The PPA provides modified asphalt binder, which is relatively cheaply produced compared to polymer-modified asphalt. In this paper, PPA was used by three-percentages 1
... Show More