Preferred Language
Articles
/
joe-1471
Effect of Distributing Steel Fibers on Some Properties of Slurry Infiltrated Fiber Concrete
...Show More Authors

The slurry infiltrated fiber concrete (SIFCON) is nowadays considered a special type of high fiber content concrete; it is high strength and high performance material. This paper investigates the effect of spread steel fiber into the slurry mortar on some properties of SIFCON. According to fiber distribution, two sets were used in this investigation. The first set consisted of randomly distributing fibers inside the slurry. The second set was by placing the fibers in an orderly manner inside the slurry. Crimped steel fibers with an aspect ratio of (60) were used. Two different volume fractions percentage of (7% and 9%) by volume of mold were used in both sets for this study. Also, a w/c ratio of (0.35) and superplasticizer of (1%) by weight of cement was used to ensure the penetration of the slurry inside the fibers. The compressive and flexural strength were conducted on standard cubes (10*10*10) cm and prisms of (40*7*7) cm respectively to find the effect of how the steel fibers were distributed. The results showed that distributing the fibers randomly gave better results than the ordered distribution. The increment percentage in compressive strength and flexural strength were (1.5%, 6.9%, 23%, and 6.5%), respectively, for both sets and both fiber volume fractions (7% and 9%).

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri Jun 29 2018
Journal Name
Journal Of Engineering
Experimental Investigation of Short Square Normal and Hybrid Fiber Reactive Powder Concrete Columns Subjected to Chloride Solution Attack
...Show More Authors

In this research, the structural behavior of reinforced concrete columns made of normal and hybrid reactive powder concrete (hybrid by steel and polypropylene fibers) subjected to chloride salts with concentration was 8341.6 mg/l. The study consists of two parts, the first one is experimental study and the second one is theoretical analysis.  Three main variables were adopted in the experimental program; concrete type, curing type and loading arrangement. Twenty (120x120x1200) mm columns were cast and tested depending on these variables. The samples were reinforced using two different bars; Ø8 for ties and Ø12 with minimum longitudinal reinforcement (0.01Ag). The specimens were divided into two main groups based o

... Show More
View Publication Preview PDF
Crossref
Publication Date
Tue Mar 30 2010
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
The Inhibition Effect of Peach Juice on Corrosion of Low Carbon Steel in Hydrochloric Acid at Different Temperatures
...Show More Authors

The corrosion inhibition of low carbon steel in1N HCl solution in the presence of peach juice at temperature (30,40,50,and 60)°C at concentration ( 5, 10, 20, 30, 40and 50 cm3/L)were studied using weight loss and polarization techniques. Results show that the inhibition efficiency was increased with the increase of inhibitor concentration and increased with the increase of temperature up to 50ºC ,above 50ºC (i.e. at 60 ºC) the values of efficiency decreases. Activation parameters of the corrosion process such as activation energies, Ea, activation enthalpies, ΔH, and activation entropies, ΔS, were calculated. The adsorption of inhibitor follows Langmuir isotherm. Maximum inhibition efficiency obtained was a bout 91% at 50ºC in the

... Show More
View Publication Preview PDF
Publication Date
Wed Jun 30 2004
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Electrochemical Behavior of Phosphotized Reinforcing Steel in Concrete in Presence of Sugar Can Ash
...Show More Authors

View Publication Preview PDF
Publication Date
Fri Oct 01 2021
Journal Name
Journal Of Engineering
Influence of Using Various Percentages of Slag on Mechanical Properties of Fly Ash-based Geopolymer Concrete
...Show More Authors

In order to implement the concept of sustainability in the field of construction, it is necessary to find an alternative to the materials that cause pollution by manufacturing, the most important of which is cement. Because factory wastes provide siliceous and aluminous materials and contain calcium such as fly ash and slag that are used in the production of high-strength geopolymer concrete with specifications similar to ordinary concrete, it was necessary for developing this type of concrete that is helping to reduce CO2 (dioxide carbon) in the atmosphere. Therefore, the aim of this study was to study the influence of incorporating various percentages of slag as a replacement for fly ash and the effect of sl

... Show More
View Publication Preview PDF
Crossref (11)
Crossref
Publication Date
Sun Sep 01 2019
Journal Name
Civil Engineering Journal
Effect of PolyPhosphoric Acid on Rutting Resistance of Asphalt Concrete Mixture
...Show More Authors

The action of high repeated trucks load associated with dramatically elevated ambient temperatures leads to the most harmful distress in asphalt pavements occurred in Iraq known as rutting. Essentially, it is produced from the accumulation of irrecoverable strains, which mainly occurred in the asphalt layers. That visually demonstrated as a longitudinal depression in the wheel paths as well as small upheavals to the sides. Poly Phosphoric Acid (PPA) has been used as a means of producing modified asphalt binders and the interest to use it has increased in recent years. The PPA provides modified asphalt binder, which is relatively cheaply produced compared to polymer-modified asphalt. In this paper, PPA was used by three-percentages 1

... Show More
Crossref (4)
Crossref
Publication Date
Thu Jun 30 2022
Journal Name
Iraqi Journal Of Laser
PDF Fiber Laser Effect on Bond Strength of Titanium implant abutment to Resin Cement
...Show More Authors

Aim: surface modification of titanium using fiber laser 1064 nm to enhance the bond strength to resin cement. Material and Methods: thirty titanium discs of 0.6 cm x 0.3 cm (diameter and thickness respectively) were categorized after preparation into three groups (n=10) as follows: control group with no surface treatment and two test groups were treated with fiber laser after estimation the appropriate parameters in the pilot study which are 81 ns pulse duration, 30,000 Hz frequency, 50 µm spot size and 10,000 mm/s scanning speed and different average power values (10 W and 20 W) depending on the tested group. Titanium discs surface characterization was performed by scanning electron microscope (SEM), a

... Show More
View Publication Preview PDF
Publication Date
Fri Sep 01 2006
Journal Name
Journal Of Engineering
Effect of Transverse Base Width Restraint on the Cracking Behavior of Massive Concrete
...Show More Authors

The effect of considering the third dimension in mass concrete members on its cracking behavior is investigated in this study. The investigation includes thermal and structural analyses of mass concrete structures. From thermal analysis, the actual temperature distribution throughout the mass concrete body was obtained due to the generation of heat as a result of cement hydration in addition to the ambient circumstances. This was performed via solving the differential equations of heat conduction and convection using the finite element method. The finite element method was also implemented in the structural analysis adopting the concept of initial strain problem. Drying shrinkage volume changes were calculated using the procedure suggested

... Show More
Publication Date
Sat Jul 22 2023
Journal Name
Journal Of Engineering
Effect of Transverse Base Width Restraint on the Cracking Behavior of Massive Concrete
...Show More Authors

The effect of considering the third dimension in mass concrete members on its cracking behavior is investigated in this study. The investigation includes thermal and structural analyses of mass concrete structures. From thermal analysis, the actual temperature distribution throughout the mass concrete body was obtained due to the generation of heat as a result of cement hydration in
addition to the ambient circumstances. This was performed via solving the differential equations of heat conduction and convection using the finite element method. The finite element method was also implemented in the structural analysis adopting the concept of initial strain problem. Drying shrinkage volume changes were calculated using the procedure sug

... Show More
View Publication Preview PDF
Crossref
Publication Date
Tue Feb 01 2022
Journal Name
Journal Of Engineering Science And Technology
CORROSION of STEEL REINFORCEMENT in INTERNALLY CURED SELF-COMPACTING CONCRETE USING WASTE BRICK and THERMOSTONE
...Show More Authors

Internal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone

... Show More
Scopus (3)
Scopus
Publication Date
Tue Feb 01 2022
Journal Name
Journal Of Engineering Science And Technology
CORROSION of STEEL REINFORCEMENT in INTERNALLY CURED SELF-COMPACTING CONCRETE USING WASTE BRICK and THERMOSTONE
...Show More Authors

Internal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone

... Show More