Plastic soil exhibits unfavorited geotechnical properties (when saturation), which causes negative defects to engineering structures. Different attempts (included various materials) were conducted to proffer solutions to such defects by experimenting in practical ways. On one hand, these attempts aimed to improve the engineering characteristics of plastic soil, and on the other hand, to use problematic waste materials as a stabilizer, like cement kiln dust, and to reduce environmental hazards. This paper explored the shrinkage, plasticity, and strength behavior of plastic soil enhanced with cement dust. The cement dust contents were 0%, 5%, 10%, 15% and 20% by dry weight of soil. An experimental series of shrinkage and plasticity tests and unconfined compression tests were carried out to explore the effects of cement dust on the quantitative amount of shrinkage, plasticity characteristics, and shear strength experienced by plastic soil. The effects of curing on soil strength were also investigated. The finding of this paper showed that the critical behavior and plasticity of plastic soil could be reduced by mixing the soil with 15% or 20% of cement dust. The undrained shear strength, cu, of plastic soil-cement dust mixtures increased with the increasing dust content up to 20%. In fact, this strength was affected by the curing period. The best enhancement was attained when the content of cement dust was 20%, and the undrained shear strength was increased more than three times at this content.
We wanted to find out how selenium (Se) affects broiler chicken performance, meat physicochemical properties, and selenium deposition in the tissues of broilers. Each of the 96 experimental pens had 30 chickens and included a total of 2,880 one-day-old broilers (Cobb 500 strain). A factorial design of four-by-three (SY + SS) and eight replicates (SY + SS) was used for the 12 experimental treatments, with selenium levels ranging from 0.15 to 0.60 ppm and organic (SY) or inorganic (SS) sources of selenium and their relationship (SY + SS). There were no differences in performance (P > 0.05) across Se levels or sources. 106 g/day of ADFI, 63 g/day of ADG, and 1.6844 kg/kg of FCR were found to be the averaging values for these three parameters:
... Show MoreA comprehensive practical study of typical mechanical properties of welded Aluminum alloy AA7020-T6 (Al-Mg-Zn), adopting friction stir welding (FSW) technique and conventional metal inert gas (MIG) technique, is well achieved in this work for real comparison purposes. The essences of present output findings were concentrated upon the FSW samples in respect to that MIG ones which can be summarized in the increase of the ultimate tensile strength for FSW was 340 MPa while it was 232 MPa for MIG welding, where it was for base metal 400 MPa. The minimum microhardness value for FSW was recorded at HAZ and it was 133 HV0.05 while it was 70 HV0.05 for MIG weld at the welding metal. The FSW produce 2470 N higher than MIG welding in the bending t
... Show MoreIn the present work, poly methyl methacrylate (PMMA) doped with Rhodamine 6G was prepared. The spectral properties (absorption and fluorescence) of the films were studied at different concentrations (1x10-5, 2x10-5, 5x10-5, 7x10-5, and 1x10-4mol/l). The investigated samples were made in the form of thin films. This was achieved by dissolving a certain weight of PMMA in a fixed volume of chloroform, composite films was with thickness (25.8μm) at room temperature. The achieved results were pointed out that absorption and fluorescence spectra have taken a wide spectral rang so when increased the concentratio
... Show MoreBoth normally developed insects and insects developed after cessation of eggs growth were
used in this work. Cessation of eggs growth occurred following abnormal conditions, which
lasted for 3.5 months before developing into adults, due to the war led by the U.S. and her
alliances against Iraq. These insects showed low rates of water contents and an active response
to water loss. Therefore their tolerance of desiccation was weak. In addition, they had an active
ability to restore their water loss quickly, after return them to a culture, this indicates that some
changes occurred in their integumentary properties were not permanent and took their turn
within one population only, but may or may not serve this population
This study was carried out to investigate the possibility of chickpea soaked water as a substitute for yeast in dough fermentation and its effects on sensory properties of the laboratory loaf bread. Chickpea was soaked for 24,48 and 72 hours at room temperature and used in proportion with or without yeast in dough fermentation . The results revealed that , as the percentage of soaked chickpea water substitution increased, the volume of the produced loaf bread decreased as compared with the control treatment (only yeast ).Best results were obtained by using soaked chickpea water for 24 hours in proportion of 1:1 soaked chickpea water : yeast regarding the sensory properties ,volume and leavening of the loaf bread.
Keywords: chickpea so
The Nuclear structure of 110-116Cd isotopes was studied theoretically in the framework of the interacting boson model of IBM-l and IBM-2. The properties of the lowest mixed symmetry states such as the 1+, 2+ and 3+ levels produced by the IBM-2 model in the vibrational-limit U(5) of Cd - isotopes are studied in details. This analysis shows that the character of mixed symmetry of 2+ is shared between and states in 110-114Cd – isotopes, the large shar goes to s, while in isotope, the state is declared as a mixed symmetry state without sharing. This identification is confirmed by the percentage of F-spin contribution. The electromagnetic properties of E2 and Ml operators were investigated and the results were analyzed. Various
... Show More