Background: Studying and investigating the transverse strength(Ts), impact strength(Is), hardness (Hr) and surface roughness(Ra) of conventional and modified autopolymerizing acrylic resin with different weight percentages of biopolymer kraftlignin, after curing in different water temperatures; 40°C and 80°C. Material and Methods: Standard acrylic specimens were fabricated according to ADA specification No.12 for transverse strength, ISO 179 was used for impact testing, Shore D for hardness and profilometerfor surface roughness. The material lignin first dispersed in the monomer, then the powder PMMA is immediately added. Ligninadded in different weight percentages. Then cured using pressure pot (Ivomet) in two temperatures;40°C and 80°C under 2 bar pressure, for 30 minutes.Atotal of 144samples were prepared for this study. Ts, Is, Ra, and Hr were tested, by using Instron universal testing machine, charpy impact tester, shore D tester, and profilometer respectively. Results: The transverse strength increased in both the conventional and modified onewhen compared with that cured in air. The addition of 0.5wt% lignin gave the higher effect (78.0017MPa) with highly significant difference found between groups at 40°C polymerizing temperature. While the impact strength in both temperatures in the modified resin revealed increased results than conventional one, 1.25wt% of kraft lignin gave the highest value (12.7355KJ/m2) with highly significant differences found between groups at 80°C polymerizing temperature. Hardness and surface roughness showed also highly significant differences found between groups at 40°C polymerizing temperature, all the groups had increased Hr. than the control one (78.95), while the Ra. decreased for 1.0% ,1.25,1.50 and 1.75 wt% lignin content to (0.26,0.10,0.063, 0.12µm) respectively in 40°C polymerizing temperature, the lowest value present in 1.75 wt% lignin (0.05 µm) at 80°Cpolymerizing temperature. Conclusions: It seems that increasing the polymerizing temperature to 40°C had a positive effect on the mechanical properties of autopolymerizing acrylic resin and the one enforced by kraft lignin biopolymer in low percentages. Increasing the polymerizing temperature to 80°C will doesn’t have much positive effect but it doesn’t deteriorate the mechanical properties. However, when submitted to increasing the temperature to 80°C, specimens showed a significant increase in impact strength.
Background: The aim of this in vitro study was to evaluate and compare the microleakage between Vertise Flow T M composite material and other conventional (Filtek Z250, riva light cure and SDR) composite materials when restoring CII mesial box only cavity at gingival margin through die penetration test Materials and methods: Forty maxillary first premolars were prepared with class II box design only cavities. Samples were divided into four groups of ten teeth according to material used: group I (FiltekZ250 only). Group II (SDR+FiltekZ250). Group III (Vertise Flow +FiltekZ250). Group IV (Riva light cure+ FiltekZ250). After 24 hrs. immersion in 2% in methylene blue, samples were sectioned and micro leakage was estimated. Results: None of the
... Show MoreChange the morphological characteristics with the change of the factors affecting it has been shown that the Tigris River has the characteristics of the morphology of the low values in terms of depth, width and perimeter wet and gradient which in turn affected the morphological and other characteristics in terms of the direction and pattern of runoff came through the study of 48 cross-section is taken of the Tigris River Year 2008 by section for each 1 km, it has been shown that the average width of the Tigris River does not exceed 221.1 meters and the average depth of 3.9 meters either wet ocean amounted to 268.9 meters and changed the cross-section area of the last section at a rate of 4594.3 square meters, and through the study turned
... Show MoreBackground: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. St
... Show MoreThe current research aims to reveal the level of satisfaction of the mentors with the evaluation of their performance according to gender (male - female) and to formulate the predictive equation for the level of performance (dependent variable) from knowing the level of satisfaction with the evaluation (independent variable). (16 paragraphs) contains alternatives to the answer that measures the level of satisfaction (weak, medium, and high) (1,2,3), that is, with a hypothetical average of (32). It consisted of 100 educational counselors consisting of 45 males and 55 females, the results of the research concluded that the level of satisfaction with performance is below the mean when compared with the hypothetical average of the scale of s
... Show MoreSeveral schottky diodes were fabricated from polyaniline/ Carbon nanotube (single and multiwalled) composites. These composites were synthesized with different concentration and two carbon nanotubes types, Single and Multi-Walled Carbon Nanotubes (SWCNT & MWCNT). Aluminum and silver paste were chosen as schottky and ohmic contact respectively. physical and electrical were used to studied these composite by using Atomic Force Microscopy (AFM) and electrical measurements. The Root Mean Square RMS surface roughness of the composite samples was found to be around 4nm. The currentvoltage characteristic were measurements for all samples in the bias range ±15V at room temperature. The results shows the increasing in carbon nanotubes concentration
... Show MoreIn this work, functionally graded materials were synthesized by centrifugal technique at different
volume fractions 0.5, 1, 1.5, and 2% Vf with a rotation speed of 1200 rpm and a constant rotation time, T
= 6 min . The mechanical properties were characterized to study the graded and non-graded nanocomposites
and the pure epoxy material. The mechanical tests showed that graded and non-graded added alumina
(Al2O3) nanoparticles enhanced the effect more than pure epoxy. The maximum difference in impact strength
occurred at (FGM), which was loaded from the rich side of the nano-alumina where the maximum value was
at 1% Vf by 133.33% of the sample epoxy side. The flexural strength and Young modulus of the fu
Roller-Compacted Concrete is a no-slump concrete, with no reinforcing steel, no forms, no finishing and wet enough to support compaction by vibratory rollers. Due to the effect of curing on properties and durability of concrete, the main purpose of this research is to study the effect of various curing methods (air curing, 7 days water curing, and permanent water curing) and porcelanite (local material used as an Internal Curing agent) with different replacement percentages of fine aggregate (volumetric replacement) on some properties of Roller-Compacted Concrete and to explore the possibility of introducing practical Roller-Compacted Concrete for road pavement with minimum requirement of curing. Specimens were sawed fro
... Show MoreSome of the characters of the Staphylolysin A and D enzymes purified from Pseudomonas aeruginosa P16 and P5 respectively were studied, the molecular weights of Staphylolysin A and D were 20.417 kilo dalton and 23.988 kilo Dalton respectively by SDS- polyacryl amide gel electrophoresis. The optimum pH for staphylolysin A activity was found to be 8 which gives higher activity reaches 150 unit/ml, and for enzyme stability was 7.5-8.5 in which the enzyme nearly retained its full activity, while it was 9.5 for staphylolysin D that gives higher activity of 16 unit/ml,and 8.5-9.5 for enzyme stability in which the enzyme nearly retained its full activity, Maximum activity of two enzymes was obtained at 40C in which the specific activity for st