Background: one of the complications of power bleaching is surface roughness of enamel which increases the possibility of post bleaching teeth discoloration. The aim of the present study is to evaluate the effect of toothpaste containing nano hydroxyapatite, NovaMin and kin sense fluoride on surface roughness of human tooth enamel after laser bleaching with 35% hydrogen peroxide bleaching gel. Materials and Methods: Twenty human enamel incisors were cleaned and their labial surface polished up to #1200, then categorized into four equal groups; first group kept without bleaching as a control group, while the remaining three experimental groups were bleached with 35% hydrogen peroxide, and each group treated with a restore paste containing one of the following: nano hydroxyapatite, NovaMin, and Kin fluoride. Bleaching was done with laser hybrid system (DMC Whitening Lase II, Sao Paulo, Brazil). Enamel roughness values assessed by an atomic force microscopy (AA3000, Bosten, USA) before and after treatment with restore tooth paste. Results: Paired t-test used to compare the mean roughness values before and after treatment with each restore paste. One-way analysis of variance and Duncan post hoc tests used to determine the differences between mean roughness values of the groups. A p-value of 0.05 or less considered a significant. The results showed a highly significant statistical differences of remineralization of all types of restore tooth pastes. Conclusions: Nano hydroxyapatite past exhibiting a higher ability to reduce the surface roughness after laser bleaching than other tested pastes.
Due to the rapid advancement of technology and the technology of things, modern industries start to need a highprecision equipment and surface finishing, so many finishing processes began to develop. One of the modern processes is Magnetic Abrasive Finishing (MAF), which is a high-precision process for internal and external finishing under the influence of a magnetic field of abrasive particles. Boron Carbide (B4C) ceramics was tested by mixing it with iron (Fe) and produced abrasive particles to reduce the intensity of scraping on the surface, reduce the economic cost and achieve a high finishing addition to remove the edges at the same time. The material selected for the samples was mild steel (ASTM E415) under (Quantity of Abrasives, Mac
... Show MoreABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreBackground: To evaluate the effect of antierosive agents (10% Nano-Hydroxyapatite (NHA), 10% Casein Phophopeptide-Amorphous Calcium Phosphate (CPP-ACP), and combination of 10% NHA and 10% CPP-ACP) on loss of minerals from enamel surface of permanent teeth treated with antierosive agents when exposed to an acidic beverage and investigate the morphological changes of treated enamel surface after demineralization with cola based beverage under Scanning Electron Microscope (SEM). Materials and Methods: Sixty maxillary first premolars were randomly divided into four groups, 15 teeth for each group. Group I treated with 10% NHA, Group II treated with 10% CPP-ACP, Group III treated with 10% NHA and 10% CPP-ACP, and Group IV did not treat with any
... Show MoreBackground: Reduction in bond strength when bonding was done immediately after intracoronal bleaching procedure has been recognized. The purpose of this study is to assess the effect of antioxidants (10% sodium ascorbate (SA), 0.1M thiourea and7% sodium bicarbonate (SB)) on reversing bonding strength of composite resin to bleached dentin. Materials and method: Sixty upper 1st premolar teeth, were selected, the crowns of the teeth were embedded in acrylic resin blocks exposing a flat dentin from the buccal surface, then divided into 6 groups (10 samples each). Bleaching for the experimental groups was performed using 35% hydrogen peroxide bleaching gel (pola–office).Group A (Negative
... Show MoreAbstract
Magnetic abrasive finishing (MAF) is one of the advanced finishing processes, which produces a high level of surface quality and is primarily controlled by a magnetic field. This paper study the effect of the magnetic abrasive finishing system on the material removal rate (MRR) and surface roughness (Ra) in terms of magnetic abrasive finishing system for eight of input parameters, and three levels according to Taguchi array (L27) and using the regression model to analysis the output (results). These parameters are the (Poles geometry angle, Gap between the two magnetic poles, Grain size powder, Doze of the ferromagnetic abrasive powder, DC current, Workpiece velocity, Magnetic poles velocity, and Finishi
... Show MoreObjectives: This study aimed to evaluate and compare the effect of plasma treatment versus conventional treatment on the micro shear bond strength (μSBS), surface roughness, and wettability of three different CAD/CAM materials. Materials and methods: Sixty cylindrical specimens (5 mm diameter ×3 mm height) were prepared from three different CAD/CAM materials: Group A: Zirconia, Group B: Lithium disilicate, and Group C: Resin nano-ceramic. Each group was subdivided into two subgroups according to surface treatment used: Subgroup I: Conventional treatment, zirconia was sandblasted with Al2O3, while lithium disilicate and resin nano-ceramic were etched with hydrofluoric acid. Subgroup II: Plasma treatment, the surface of each material was tr
... Show MoreABSTRACT Background:Hydrogen absorption and related degradation in the mechanical properties of Ni-Ti based orthodontic wires has been demonstrated following exposure to fluoride prophylactic agents. This study was designed to investigate the effects of three fluoride containing agents on the load deflection characteristics of heat activated nickel titanium arch wires during unloading phase. Material and method: Eighty specimens of heat activated nickel titanium arch wires were obtained from Ortho Technology Company, half of which had a 0.016 inch round and 0.019x0.025 rectangular. Ten specimens from both wire size were immersed in one of the tested fluoride prophylactic agents (neutral sodium fluoride gel, stannous fluoride gel or phos-flu
... Show MoreLaser skin wound soldering offers many distinct advantages over conventional closure and laser welding techniques. Objective : to compare the histological effects of human skin wound soldering using 50 % human albumin solder and compound charcoal photosensitiser with 980 nm diode laser acting in various modes of action and parameters. Study Design/Materials and Methods: In this in vitro experimental study , Multiple 3-4 cm long full thickness incisions in a specimen of human skin were soldered using a 4 mm spot diameter beam of 980 nm diode laser(at different laser parameters and modes of action) with 50 % human albumin solder mixed with the compound charcoal at 5 % W/V concentration .After obtaining a successful wound soldering , the wo
... Show MoreObjective. This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. Materials and Methods. Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water stora