Background: Limited data are available on the dimensional stability and surface roughness of ThermoSens, which is a material used in denture processing. This study aimed to measure the vertical teeth changes and surface roughness of ThermoSens dentures prepared using three different investment materials. Materials and methods: For the dimensional changes test, 30 complete maxillary dentures were prepared using different investment methods: group I, dental stone; group II, silicone putty; and group III, a mixture of dental stone and plaster (ratio, 1:1; n = 10 for each group). Four screws were attached to the dentures: two were attached to the buccal surface of the canine and first molar, and the other two were attached in the flange areas of the canine and first molar in line with the previously mentioned screws. Measurements were made using a micrometer microscope in the wax stage before flasking and in the deflasking stage. The above investment techniques were also used to prepare samples for a surface roughness test (n = 10 per group). These samples were prepared according to the specifications of the American Dental Association. Data were examined using analysis of variance (ANOVA) and the least significant difference (LSD) test. Results: One-way ANOVA and LSD revealed that dimensional changes significantly differed among all groups, except that the vertical teeth changes on the left side did not differ between groups I and II for both the canine and molar regions. Surface roughness was significantly higher in group I than in group II, and in group III than in group II. Conclusion: The use of putty silicone for investing ThermoSens complete dentures reduced dimensional changes and resulted in dentures with a better fit. Surface roughness could be reduced by the addition of a putty silicone layer over the denture before the addition of the second investment layer during denture processing.
Background: The most widely used material for fabrication of denture base is poly methyl methacrylate, despite its popularity, the main problems associated with it as a denture base material are poor strength particularly under fatigue failure inside the patient mouth, impact failure outside the patient mouth, which are the main causes for fracture of denture, several studies was done to increase mechanical properties of denture base. The present study was conducted to evaluate and compare the effect of addition single walled carbon nanotubes in different concentrations to polymethyl methacrylate on some mechanical properties (surface hardness, surface roughness, impact strength and transverse strength). Materials and methods: Forty eight
... Show MoreABSTRACT Background:Hydrogen absorption and related degradation in the mechanical properties of Ni-Ti based orthodontic wires has been demonstrated following exposure to fluoride prophylactic agents. This study was designed to investigate the effects of three fluoride containing agents on the load deflection characteristics of heat activated nickel titanium arch wires during unloading phase. Material and method: Eighty specimens of heat activated nickel titanium arch wires were obtained from Ortho Technology Company, half of which had a 0.016 inch round and 0.019x0.025 rectangular. Ten specimens from both wire size were immersed in one of the tested fluoride prophylactic agents (neutral sodium fluoride gel, stannous fluoride gel or phos-flu
... Show MoreTo investigate the effects of losartan and enalapril on serum uric acid in hypertensive patients with metabolic syndrome, one hundred and twenty six newly diagnosed mild hypertensive patients, having markers of metabolic syndrome included in the study. The patients were divided into two groups. Group 1 (60 patients) was given losartan (50 mg/ day) and group 2 (66 patients) enalapril (20 mg/ day) for a duration of 2 months. A control group of seventy apparently healthy individuals were included. Metabolic syndrome was diagnosed according to diagnostic criteria of metabolic syndrome related to the American National Cholesterol Education Program-Adult Treatment Panel III. Serum uric acid levels were measured bef
... Show MoreTen isolates of Klebsiella pneumoniae, seven isolates of Pseudomonas aeruginosa and nine isolates of Staphylococcus aureus, were obtained from 100 urine samples collected from Baghdad hospitals. All isolates were identified biochemically and confirmed by using VITEK 2 and were then tested for their susceptibility towards 6 antibiotics and for phenolic extracts of Thymus vulgaris and Cinnamomum cassia. All bacteria were greatly affected by T. vulgaris, especially K. pneumoniae. Viable count was performed, it was noted that the number of bacterial cells reduced from 1×108 CFU to 1.2× 103, 2×105 and 1.8×106CFU of K. pneumoniae, P. aeruginosa and S. aureus respectively. While C. cassiahad a slight effect on them. K. pneumoniae isola
... Show MoreEnd Stage Renal Disease is a well-known global public health problem. Maintenance hemodialysis is considered a life-saving treatment for patients with such disease. This treatment method that requires patients to be adherent to hemodialysis attendance, dietary and fluid recommendations as well as adherence to prescribed medications to ensure success. The aim of the current study was to assess adherence, perception, and counseling among hemodialysis patients to different modalities of treatment (fluid restriction, dietary recommendations, medications, and hemodialysis schedules). A cross-sectional study carried out on hemodialysis patients who attended to the dialysis centers at al- Karama teachi
... Show MoreZirconia ceramic restoration (ZCR) has a higher fracture incidence rate than metal ceramic restoration. Different surface treatments were used to improve fracture performance of ZCR such as grit blasting (GB) by aluminium oxide powder. This type of surface treatment generate residual stresses on veneering ceramic causing crack initiation and ending with a fracture. In order to overcome the stress generated by GB, zirconia surface coating is used as a surface treatment to improve fracture resistance and to accommodate stresses along the ZCR layers. Fifty zirconia ceramic crowns were fabricated and divided according to the type of surface treatment into three groups; the first group is (ZG), involving 20 cores were coated with a mixture of pa
... Show More