Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
A total of 20 raw milk samples were used as the fouling agent for evaluating the bacteriological effectiveness of cleaning and sanitizing of domestic milking equipment by using ozonated water at 0.5 ppm comparing to the warm water at 55! for 5 minutes respectively. The mean values of total aerobic bacteria, Coliform and E.coli that present on the plastic and stainless-steel containers after using the raw milk as fouling agent were 3.4×10-6 , 6.7x10-5 and 5.8×10-3 cfu/cm2 respectively , after cleaning the stainless steel containers by the ozonated water the mean values of total aerobic bacterial counts, Coliforms and E.coli bacteria were reduced to 1.2×10-6, 4.7×10-5 and 3.3×10-3 CFU/cm2 respectively. while after cleaning by the warm wa
... Show MoreThe aim of the present work, was measuring of uranium concentrations in 25 soil samples from five locations of Al-Kut city. The samples taken from different depths ranged from soil surface to 60cm step 15 cm, for this measurement of uranium concentrations .The most widely used technique SSNTDs was chosen to be the measurement technique. Results showed that the higher concentrations were in Hai Al- Kafaat which recorded 1.49 ± 0.054 ppm . The uranium content in soil samples were less than permissible limit of UNSCEAR(11.7ppm).
The cytotoxicity of different concentrations of purified methionine γ- lyase from Pseudomonas putida on cancer cell lines (RD, AMN3 and AMGM) at 96 hr was studied. The bacterial enzyme with concentration 1000µg/ml was revealed highly cytotoxicity against cancer cell lines in comparison with other concentrations whereas slight cytotoxicity was observed on normal cell (REF).
Zinc oxide (ZnO) nanoparticles were synthesized using a modified hydrothermal approach at different reaction temperatures and growth times. Moreover, a thorough morphological, structural and optical investigation was demonstrated using scanning electron microscopy (SEM), x-ray diffraction (XRD), ultra-violate visible light spectroscopy (UV-Vis.), and photoluminescence (PL) techniques. Notably, SEM analysis revealed the occurrence of nanorods-shaped surface morphology with a wide range of length and diameter. Meanwhile, a hexagonal crystal structure of the ZnO nanoparticles was perceived using XRD analysis and crystallite size ranging from 14.7 to 23.8 nm at 7 and 8 ℎ𝑟𝑠., respectively. The prepared ZnO samples showed good abso
... Show MoreThe use of blended cement in concrete provides economic, energy savings, and ecological benefits, and also provides. Improvement in the properties of materials incorporating blended cements. The major aim of this investigation is to develop blended cement technology using grinded local rocks . The research includes information on constituent materials, manufacturing processes and performance characteristics of blended cements made with replacement (10 and 20) % of grinded local rocks (limestone, quartzite and porcelinite) from cement. The main conclusion of this study was that all types of manufactured blended cement conformed to the specification according to ASTM C595-12 (chemical and physical requirements). The percentage of the compress
... Show MoreThin filis have been prepared from the tin disulphide (SnS2 ), the pure and the doped with copper (SnS2:Cu) with a percentages (1,2,3,4)% by using ahemical spray pyrolysis techniqee on substrate of glass heated up to(603K)and sith thicknesses (0.7±0.02)?m ,after that the films were treated thermally with a low pressure (10-3mb) and at a temperature of (473K) for one hour. The influence of both doping with copper and the thermal treatment on some of the physical characteristics of the prepared films(structural and optical) was studied. The X-ray analysis showed that the prepared films were polycrystalline Hexagonal type. The optical study that included the absorptance and transmitance spectra in the weavelength range (300-900)nm
... Show MoreBackground: Selenium-73 with half- life of 7.15 hour emits β+ in nature and has six stable isotopes which are ( 74Se,76Se,77Se,78Se,80Se and 82Se ). Selenium-73 has many applications in technology and radioselenium compounds of metallic have found various applications in medicine. Objective: To make a comparison between different reactions that produced cross sections of Se-73 radioisotopes. Subjects and methods: The feasibility of the production of Selenium -73 via various nuclear reactions was investigated. Excitation functions of 73Se production by the reactions of 75As (p,3n), 169Tm( d,x), 74Se, natSe, natBr (p,x) , 75As (d,4n), natGe (3He,x), 70Ge (α, n), and 72Ge (α, 3n) and neutron capture were calculated using the avail
... Show MoreBackground: Consideration of mandibular third molar is important from orthodontic perspective due to several factors such as, lower anterior arch crowding, relapse in lower anterior region, interference with uprighting of mandibular first and second molars during anchorage preparation and molar distalization. The aims of this study were to assess of gender differences in the mandibular third molar position and compare and evaluate whether there is any differences in the results provided by CT scan and lateral reconstructed radiograph. Materials and Methods: The sample of present study consisted of 39 patients (18 males and 21 females) with age range 11-15 years. CT images for patients who were attending at Al Suwayra General Hospital/the C
... Show MoreThis work deals with thermal cracking of three samples of extract lubricating oil produced as a by-product from furfural extraction process of lubricating oil base stock in AL-Dura refinery. The thermal cracking processes were carried out at a temperature range of 325-400 ºC and atmospheric pressure by batch laboratory reactor. The distillation of cracking liquid products was achieved by general ASTM distillation (ASTM D -86) for separation of gasoline fraction up to 220 ºC from light cycle oil fraction above 220 ºC. The comparison between the conversions at different operating conditions of thermal cracking processes indicates that a high conversion was obtained at 375°C, according to gasoline production. According to gasoline produ
... Show More