Background: Change in palatal vault shape and Reinforcement of high impact acrylic denture base resin may in turn affect the dimensional accuracy of acrylic resin and affecting the fitness of the denture.This study evaluated tostudy the effect of fiber reinforcement for high-impact acrylic resin denture base with different palatal vault shapes on adaptation or gap space between the denture base and the stone cast and compare with non-fiber reinforcement and effect of palatal vault shapes on adaptation of non-reinforced and fiber reinforced high impact denture base acrylic resin Material and method: Three different palatal vault shapes were prepared on standard casts using CNC (computer numerical control) machine. 60 samples of heat polymerized high impact acrylic resin maxillary denture base were fabricated onto each definitive cast according to manufacturer instruction. Samples divided into three main experimental groups represented the three different palatal vault shapes (20 samples for each main group); 1st rounded 2nd U-shaped and the 3rd groups V-shaped. Each main group divided into two subgroups (10 samples for each subgroup) representing non fiber reinforced high impact acrylic group as a control and the fiber reinforced high impact acrylic. The measurements of gap-space changes of denture bases done at two stages, 1st 24 hour after polymerization and 2nd measurement done after one month storage in distilled water at room temperature. Results and conclusion: Dimensional changes of high impact acrylic denture base not affected by glass fiber reinforcement p-value for all reference pointes ≥ 0.05, while topographical change in maxillary vault shapes effects on the gap-space in non-fiber reinforced high impact acrylic denture base p-value < 0.05 in point one, four, and seven.
An experiment was conducted using pots (capacity of 4 kg soil/pot) in the glasshouse of Biology Dept. College of Education (Ibn Al-Haitham) University of Baghdad during 2008-2009 growing season, in order to determine the effect of different levels of urea fertilizer (Zero, 0.1, 0.2, 0.4 gm/4 kg soil in pot) these equal to (Zero, 100,200,400 kg/ha) and different levels of superphosphate fertilizer (Zero, 0.1, 0.2 gm/4kg soil in pot), these equal to (Zero, 100,200 kg/ha) on some morphological and physiological characteristics of fenugreek plant. This experiment was conducted using Completely Randomized Design (CRD) with three replications and the experiment included (36) pots. Results indicated clear increase in all studied characteristics wi
... Show MoreAbstract: An unfavorable complication of root canal is vertical root fracture. The aim of present study is to evaluate the vertical root fracture of treated teeth filled with gutta percha and Resilon obturating material using different sealers. Forty mandibular premolars used in the study. Canals randomly divided into four groups (n=10). Group-A eugenol-based (Endofill) sealer with gutta percha; GroupB epoxy-amine (AH Plus) sealer with gutta percha; Group-C resin-based (Real Seal) sealer with Resilon; or Group-D epoxide-based (Perma Evolution) sealer with gutta percha. Roots mounted vertically in cold cure acrylic blocks and subjected to vertical loading with a crosshead speed of 1mm ̸min. The point at which fracture of the roots occurred
... Show MoreThis study was conducted in the poultry field of the Department of Animal Production - Faculty of Agriculture - University of Baghdad (Abu Ghraib) for the period from 28/9/2017 to 9/11/2017 for a period of six weeks (42 days), was used in the experiment 300 chick of broiler (Ross 308) one day old. The aim of this study was to effect of adding supplementing different levels of bee pollen (0, 250, 500, 750 and 1000) gm/100kg on Productive Performance. The chicks were randomly distributed in to five treatments, T1 control (without any addition), (T2, T3, T4 and T5) adding bee pollen in the diet 250, 500, 750 and 1000 gm/100kg respectively. The results showed that bee pollen in the diet level 1000 gm/100 kg led to significant increase in the we
... Show MoreThis research foxed on the effect of fire flame of different burning temperatures (300, 400 and 500)oC on the compressive strength of reactive powder concrete (RPC).The steady state duration of the burning test was (60)min. Local consuming material were used to mixed a RPC of compressive strength around (100) MPa. The tested specimens were reinforced by (3.0) cm hooked end steel fiber of (1100) MPa yield strength. Three steel fiber volume fraction were adopted in this study (0, 1.0and 1.5)% and two cooling process were included, gradual and sudden. It was concluding that increasing burning temperature decreases the residual compressive strength for RPC specimens of(0%) steel fiber volume fraction by (12.16, 19.46&24.49) and (18.20, 27.77 &3
... Show MoreIn this study, geopolymer mortar was designed in various experimental combinations employing 1% micro steel fibers and was subjected to different temperatures, according to the prior works of other researchers. The geopolymer mortar was developed using a variety of sustainable material proportions (fly ash and slag) to examine the influence of fibers on its strength. The fly ash weight percentage was 50%, 60%, and 70% by slag weight to study its effect on the geopolymer mortar's properties. The optimal ratio produced the most significant results when mixed at a 50:50 ratio of fly ash and slag with 1% micro steel fibers at curing temperature 240oC for 4 hours through two days. The compressive strength of the geopolymer mortar increas
... Show More
The nanocompsite of alumina (Al2O3) produced a number of beneficial effects in alloys. There is increasing in resistance of materials to surface related failures , such as the mechanical properties , fatigue and stress corrosion cracking .The experimental results observed that the adding of reinforced nanomaterials type Al2O3 enhanced the HB hardness, UTS, 0.2 YS and ductility of 2014 Al/Al2O3 nano composites . the analysis of experiments, indicated that The maximum enhancement was observed at 0.4 wt.% Al2O3. The ultimate improvement percentage were 15.78% HB hardness, 18.1% (UTS), 12.86% (
... Show MoreBackground: to evaluate the effect of different dentifrices on the surface roughness of two composite resins (nanofilled-based and nanoceramic – based composite resins). Materials and methods: Forty specimens (diameter 12 mm and height of 2mm) prepared from different composite resin materials: Z350 (nanofilled composite, and Ceram-X (nanoceramic) .they were subjected to brushing simulation equivalent to the period of 1 year. The groups assessed were a control group brushed with distilled water (G1), Opalescence whitening toothpasteR (G2), Colgate sensitive pro-relief (G3) and Biomed Charcoal Toothpaste (G4). The initial and final roughness of each group was tested by surface roughness tester. The results were statistically analyzed using
... Show MoreCorrosion resistance of metals is one of the most important topics for researchers. In this work, epoxy-TiO2 nanocomposite has been developed for protection of 6061AL alloy. The dip-coating technique used to deposit the coating on 6061 Al alloy substrate. Different concentrations of TiO2 NPs (1,3,5 )Wt% have been used to study the corrosion behavior in 3.5% NaCl medium. Also, 200,150 and 100 mm/min dipping speeds have been employed for 1%wt TiO2 to show their effects on coating layer and corrosion rate. Characterization of coated surfaces were investigated by AFM, FESEM andEDS,while theelectrochemical measurementswas using to evaluate protective nature of the coating. The results have shown that the corrosion rate has decreased with
... Show More