Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtek™ P60 (packable composite), Filtek™ P90 (Silorane-based composite) and Sonic fill™ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtek™ P60 and single bond™ Universal adhesive using horizontal incremental technique, group (B)the teeth were restored with Filtek™ P90 and P90 system adhesive using horizontal incremental technique and group (C) the teeth were restored with Sonic fill™ composite and single bond™ Universal adhesive using bulk technique.After specimens were stored in distilled water at 37°C for 7 days, all specimens were subjected to thermocycling at (5° to 55 °C), then submitted to mechanical load cycling (intermittent axial force of 49N and a total of 50.000 cycles). The specimens were observed under scanning electron microscope at (2000 X) to measure marginal gap width (the distance between the dental wall and the restoration) at occlusal, proximal and gingival regions in micrometer using Tescan software, version 3.5. Data were analyzed statistically by one way ANOVA test and least significant difference tests. Results:The results showed that the silorane-based posterior composite (Filtek™ P90) showed significantly the least marginal gap width at the occlusal, proximal and gingival regions after the application of thermal changes and mechanical load cycling in comparison to the two methacrylate-based posterior composite Filtek™ P60 (packable) and the Sonic fill™ (nano-hybrid). Sonic fill™ bulk fill composite that relied on the vibration concept to lower the viscosity of high filler loaded composite material showed significantly lesser marginal gaps width at occlusal, proximal and gingival composite/enamel interface regions in comparison with Filtek™ P60 (packable composite) using horizontal incremental technique. The silorane-based composite (Filtek™ P90) showed non-significant difference in marginal gaps width at the three different regions. While, both methacrylate based Filtek™ P60 and Sonic fill™ composite showed significantly lesser marginal gap width at the occlusal region in comparison with gingival regions. Conclusion: None of the low-shrinkage composite restorative materials tested in this study totally prevented micro-gap formation at composite/enamel interfaces of Class II MO cavity.
Root-finding is an oldest classical problem, which is still an important research topic, due to its impact on computational algebra and geometry. In communications systems, when the impulse response of the channel is minimum phase the state of equalization algorithm is reduced and the spectral efficiency will improved. To make the channel impulse response minimum phase the prefilter which is called minimum phase filter is used, the adaptation of the minimum phase filter need root finding algorithm. In this paper, the VHDL implementation of the root finding algorithm introduced by Clark and Hau is introduced.
VHDL program is used in the work, to find the roots of two channels and make them minimum phase, the obtained output results are
The study was conducted to identify the toxicity of chromium on scenedesmus quadricauda algae alone and in the presence of nutrient metal (Nitrogen). Different concentrations of chromium (0.5, 1.5 , 2.5, 3.5 , 4.5mg/L) were used and the presence nitrogen is (5 ,10 ,50 ,100mg/L) on cultur media(chu-10) with used for cultivation of the algae in controlled conditions(25oC , light intensity 380 –?E/m2 /s. The results showed increasing in the toxicity of the metal when is alone , excess of concentrations an time of exposure. The growth rate decreased from 0.44 to 0.06 cell/ hour after 12 day of the biging of the experiment and of concentrate 4.5 mg/L of chromium. The intermediate active concentrations of the chromium(EC50) was increase
... Show MoreReactive Powder Concrete (RPC) can be incorporate as a one of the most important and progressive concrete technology. It is a special type of ultra-high strength concrete (UHSC) that’s exclude the coarse aggregate from its constitutive materials. In this research an experimental study had been carried out to investigate the effect of using three types of materials (porcelain aggregate) and others sustainable materials (glass waste and granular activated carbon) as a partial replacement of fine aggregate. Four percentages had considered (0, 10, 15 and 20) % to achieve better understanding for the influence of these materials upon the compressive strength of RPC. Four curing ages had included in this study, these are; 7, 28, 60 and
... Show MoreReactive Powder Concrete (RPC) can be incorporate as a one of the most important and progressive concrete technology. It is a special type of ultra-high strength concrete (UHSC) that’s exclude the coarse aggregate from its constitutive materials. In this research an experimental study had been carried out to investigate the effect of using three types of materials (porcelain aggregate) and others sustainable materials (glass waste and granular activated carbon) as a partial replacement of fine aggregate. Four percentages had considered (0, 10, 15 and 20) % to achieve better understanding for the influence of these materials upon the compressive strength of RPC. Four curing ages had included in this study, these are; 7, 28, 60 and
... Show MoreIn this study, plastic wastes named (PET and PVC) were used to prepare polymer matrix composite (PMC) which can be used in different applications. Composite materials were prepared by mixing unsaturated polyester resin (UP) with plastic wastes, two types of plastic waste were used in this work included polyethylene-terephthalate (PET) and Polyvinyl chloride (PVC) with various weight fractions (0, 5,10,15, 20 and 25%) added as a filler in flakes form. In this work, some of the tests that were carried out included (tensile, bending, and compressive strength) as mechanical tests, in addition to (thermal conductivity and water absorption) as physical tests. The values of tensile, compressive strength and Young's modulus of UP increased after
... Show MoreThis research paper studies the use of an environmentally and not expensive method to degrade Orange G dye (OG) from the aqueous solution, where the extract of ficus leaves has been used to fabricate the green bimetallic iron/copper nanoparticles (G-Fe/Cu-NPs). The fabricated G‑Fe/Cu-NPs were characterized utilizing scanning electron microscopy, BET, atomic force microscopy, energy dispersive spectroscopy, Fourier-transform infrared spectroscopy and zeta potential. The rounded and shaped as like spherical nanoparticles were found for G-Fe/Cu‑NPs with the size ranged 32-59 nm and the surface area was 4.452 m2/g. Then the resultant nanoparticles were utilized as a Fenton-like oxidation catalyst. The degradation efficiency of
... Show MoreThe present study attempts to determine the effect of freezing for different periods on preserved bodies of fish in the laboratory to keep for the research and diagnosis of taxonomic studies and not for consumption. It also endeavors to identify the effect of freezing on some morphometric features of the preserved bodies of fishes. Planiliza abu fish were used to conduct the present study. Fish were frozen by regular freezing in the home refrigerator freezer with temperatures reaching four degrees centigrade below zero. Freezing time is distributed over four months; biometric measurements of frozen fish have been taken in these periods represented by body total length, Standard length, and Head length in centimeters using a ruler ve
... Show MoreThe buildup factor was measured after irradiating Iraq carbon black powder using each of and sources respectively, using mixing ratios 40% & 50% for thickness range . The results showed that the buildup factor depends on energy and has limited dependence on the mixing ratio. The QIFT program succeeded accenting for the experimental results even for expected values more than 4 m.f.p outside the thickness range.
SKF Sami I. Jafar, Mohammad J. Kadhim, Engineering and Technology Journal, 2018 - Cited by 4