Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtek™ P60 (packable composite), Filtek™ P90 (Silorane-based composite) and Sonic fill™ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtek™ P60 and single bond™ Universal adhesive using horizontal incremental technique, group (B)the teeth were restored with Filtek™ P90 and P90 system adhesive using horizontal incremental technique and group (C) the teeth were restored with Sonic fill™ composite and single bond™ Universal adhesive using bulk technique.After specimens were stored in distilled water at 37°C for 7 days, all specimens were subjected to thermocycling at (5° to 55 °C), then submitted to mechanical load cycling (intermittent axial force of 49N and a total of 50.000 cycles). The specimens were observed under scanning electron microscope at (2000 X) to measure marginal gap width (the distance between the dental wall and the restoration) at occlusal, proximal and gingival regions in micrometer using Tescan software, version 3.5. Data were analyzed statistically by one way ANOVA test and least significant difference tests. Results:The results showed that the silorane-based posterior composite (Filtek™ P90) showed significantly the least marginal gap width at the occlusal, proximal and gingival regions after the application of thermal changes and mechanical load cycling in comparison to the two methacrylate-based posterior composite Filtek™ P60 (packable) and the Sonic fill™ (nano-hybrid). Sonic fill™ bulk fill composite that relied on the vibration concept to lower the viscosity of high filler loaded composite material showed significantly lesser marginal gaps width at occlusal, proximal and gingival composite/enamel interface regions in comparison with Filtek™ P60 (packable composite) using horizontal incremental technique. The silorane-based composite (Filtek™ P90) showed non-significant difference in marginal gaps width at the three different regions. While, both methacrylate based Filtek™ P60 and Sonic fill™ composite showed significantly lesser marginal gap width at the occlusal region in comparison with gingival regions. Conclusion: None of the low-shrinkage composite restorative materials tested in this study totally prevented micro-gap formation at composite/enamel interfaces of Class II MO cavity.
Background: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown re
... Show MoreBackground: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown re
... Show MoreIn this study, the mechanical properties of an epoxy and unidirectional woven carbon with fiberglass composite were experimentally investigated. When preparing the composite samples, American Society for Testing and Materials (ASTM)standard was used. Tensile, impact and flexural test were conducted to investigate the mechanical properties of the new produced epoxy Unidirectional Woven Carbon and Epoxy Fiberglass composites. The outcome showed that the strength of the produced samples increased with the increase in the number of unidirectional woven carbon layers added. Two methods were utilized: (1) woven carbon composite with glass fiber (2) woven carbon composite). The two methods of composite were compared with each other. The resul
... Show MoreThe present study focused mainly on the buckling behavior of composite laminated plates subjected to mechanical loads. Mechanical loads are analyzed by experimental analysis, analytical analysis (for laminates without cutouts) and numerical analysis by finite element method (for laminates with and without cutouts) for different type of loads which could be uniform or non-uniform, uniaxial or biaxial. In addition to many design parameters of the laminates such as aspect ratio, thickness ratio, and lamination angle or the parameters of the cutout such as shape, size, position, direction, and radii rounding) which are changed to studytheir effects on the buckling characteristics with various boundary conditions. Levy method of classical lam
... Show MoreThis research is presented experimental and numerical investigations of composite concrete-steel plate shear walls under axial loads to predicate the effect of both concrete compressive strength and aspect ratio of the wall on the axial capacity, lateral displacement and axial shortening of the walls. The experimental program includes casting and testing two groups of walls with various aspect ratios. The first group with aspect ratio H/L=1.667 and the second group with aspect ratio H/L=2. Each group consists of three composite concrete -steel plate wall with three targets of cube compressive strength of values 39, 54.75 and 63.3 MPa. The tests result obtained that the increase in concrete compressive strength results in increasing
... Show MoreWe aimed to examine the effect of amoxicillin and azithromycin suspensions on the microhardness of sliver-reinforced glass ionomer and nano-resin modified glass ionomer (GI). Method: Thirty discs (2mm height x 4mm diameter) of each type of GI were prepared, which were randomly assigned to amoxicillin, azithromycin, and artificial saliva groups. Microhardness was evaluated by Vickers hardness test before and after three immersion cycles. Results: The overall model (P < 0.001), before/after intervention (P < 0.001), intervention group (type of antibiotic) (P=0.013), and type of glass ionomer (P < 0.001) showed significant differences among study groups (P < 0.001). Post hoc test showed only non-significant before/after difference for Azithrom
... Show MoreFrictional resistance occurs whenever sliding happens, negatively impacting treatment outcomes and duration. It is a clinical challenge and must be dealt with efficiently to achieve the best orthodontic results. Aims of this study: compare and evaluate the static frictional forces under the wet condition to mimic the oral environment produced by using a polycrystalline ceramic bracket, monocrystalline ceramic bracket, 0.014 of an inch nickel-titanium (Rhodium coated archwires, and ilusio aesthetic archwires), and 0.019 x 0.025 of an inch stainless steel (Rhodium coated archwires, and ilusio aesthetic archwires). Ninety-six aesthetic brackets (48 monocrystalline and 48 polycrystalline brackets) were used and stored in different incub
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreBackground: The irradiation of teeth with a laser results in an interaction between the light and the biological constituents of the dental hard substance, which is converted directly into heat.This thermal effect is the cause of the structural and chemical enamel changes.The combined treatment of topical fluoride agent with laser may increase fluoride uptake, and reduce progression of caries-like lesions. The aim of this study was to measure the uptake of the acidulated phosphate fluoride and sodium fluoride to the buccal and lingual caries-like lesion enamel surfaces before and after irradiated by Nd-YAG laser in comparison with matching control group. Materials and methods: The sample consisted of 30 human healthy upper premolar teeth wh
... Show MoreBackground: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. St
... Show More