Background: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CAD/CAM blocks (IPS e. max CAD) and Group D: Restored with resin nano ceramic CAD/CAM blocks (Lava Ultimate Restorative). Standard preparations were done using Ceramic Veneer Set (Komet). Indirect laminate veneers were cemented with the Relyx Veneer Cement (3M ESPE) and all specimens were stored in distilled water at 37°C for 2 weeks. The load was applied on the occlusal part of the veneer at 45˚ to long axis of the tooth using universal testing machine. Results were analyzed with one-way ANOVA and LSD tests. Specimens were examined by stereomicroscope at a magnification of 20x to evaluate the mode of failure. Results: Control group showed higher mean of fracture strength with highly significant difference in comparison to the experimental groups (P<0.01). (Group A) showed higher mean of fracture strength with statistically significant difference in comparison to (Group B and Group D). On the other hand the difference between (Group A and Group C) was statistically highly significant. Statistically non-significant difference was found among the three indirectly restored groups. Conclusions: All veneers used in this study can be considered as acceptable treatment in the premolars region for patients with normal biting force. Direct composite veneer is the most favorable technique in term of fracture strength, while IPS e. max CAD laminate veneers were least likely to fracture and most likely to completely debond.
The problem of the damage caused by terrorist acts has raised many difficulties in many countries, including Iraq, which requires the existence of a law that sets out sufficient rules for compensating the victims of terrorist acts, in order to compensate them for the harm they have not suffered. It may be difficult or impossible for them to identify causing damage, and therefore unable to obtain compensation by applying the traditional rules of liability that require proof of fault and identify the culprit. The security funds come as an appropriate alternative that pays compensation in such cases for victims to reparation for the damage they suffered. Therefore, this problem remains one of the most problems that Iraq suffers from it, which
... Show MoreThrust blocks and restraint joints are the two most popular methods of counteracting the thrust force that generated at pipe fittings (bends, Tee, wye, reducers, dead ends, etc…). Both systems perform the same function, which is to prevent the joints from separating from the pipes. The aim of the study is to review previous studies and scientific theories related to the study and design of thrust blocks and restraint joints to study the behavior of both systems under thrust force and to study the factors and variables that affect the behavior of these systems. The behavior of both systems must be studied because they cannot be abandoned, as each system has conditions whose use is more feasible, scientific, and economic
... Show MoreDBN Rashid, JOURNAL OF XI'AN UNIVERSITY OF ARCHITECTURE & TECHNOLOGY, 2020
The objective of the present investigation was to enhance the solubility of practically insoluble mirtazapine by preparing nanosuspension, prepared by using solvent anti solvent technology. Mirtazapine is practically insoluble in water which act as antidepressant .It was prepared as nano particles in order to improve its solubility and dissolution rate. Twenty formulas were prepared and different stabilizing agents were used with different concentrations such as poly vinyl pyrrolidone (PVPK-90), poly vinyl alcohol (PVA), poloxamer 188 and poloxamer 407. The ratios of drug to stabilizers used to prepare the nanoparticles were 1: 1 and 1:2. The prepared nanoparticles were evaluated for
... Show MoreBackground: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreBackground: Tooth wear is one of the most common problems in the older dentate population which results from the interaction of three processes (attrition, abrasion and erosion) and it affects all societies, different age groups, and all cultures. This study was achieved to evaluate the prevalence and distribution of tooth wear among institutionalized residents in Baghdad city\ Iraq. Subjects and Methods: This survey was accomplished on four private and one governmental institution in Baghdad city. One-hundred twenty three (61 males, 62 females) aged 50-89 years were participated in this study. The diagnosis and recording of tooth wear were according to criteria of Smith and Knight. Results: The prevalence of tooth wear was 100% with a mean
... Show More