Background: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CAD/CAM blocks (IPS e. max CAD) and Group D: Restored with resin nano ceramic CAD/CAM blocks (Lava Ultimate Restorative). Standard preparations were done using Ceramic Veneer Set (Komet). Indirect laminate veneers were cemented with the Relyx Veneer Cement (3M ESPE) and all specimens were stored in distilled water at 37°C for 2 weeks. The load was applied on the occlusal part of the veneer at 45˚ to long axis of the tooth using universal testing machine. Results were analyzed with one-way ANOVA and LSD tests. Specimens were examined by stereomicroscope at a magnification of 20x to evaluate the mode of failure. Results: Control group showed higher mean of fracture strength with highly significant difference in comparison to the experimental groups (P<0.01). (Group A) showed higher mean of fracture strength with statistically significant difference in comparison to (Group B and Group D). On the other hand the difference between (Group A and Group C) was statistically highly significant. Statistically non-significant difference was found among the three indirectly restored groups. Conclusions: All veneers used in this study can be considered as acceptable treatment in the premolars region for patients with normal biting force. Direct composite veneer is the most favorable technique in term of fracture strength, while IPS e. max CAD laminate veneers were least likely to fracture and most likely to completely debond.
The current study included the isolation, purification and cultivation of blue-green alga Oscillatoria pseudogeminata G.Schmidle from soil using the BG-11liquid culture medium for 60 days of cultivation. The growth constant (k) and generation time (G) were measured which (K=0.144) and (G=2.09 days).
Microcystins were purified and determined qualitatively and quantitatively from this alga by using the technique of enzyme linked immunosorbent assay (Elisa Kits). The alga showed the ability to produce microcystins in concentration reached 1.47 µg/L for each 50 mg DW. Tomato plants (Lycopersicon esculentum) aged two months were irrigated with three concentrations of purified microcystins 0.5 , 3.0 and 6.0
... Show MoreThis article presents the simultaneous adsorption of bimetal Cu2+ and Zn2+ from an aqueous solution using activated carbon synthesized from a plum seed precursor by sulfuric acid and microwave activation: plum seeds chemically activated by 45% (w/w) sulfuric acid with 2:1 ratio for 4 h, then carbonized for 2 h at 700 °C and the product obtained activated in a microwave oven for 20 min at 700 W for final of activation. Plum seeds and activated carbon produced were characterized in terms of their physical and chemical composition using Brunauer–Emmett–Teller measurements, field emission scanning electr
The modified Hummers method was applied to prepare graphene oxide (GO) from the graphite powder. Tin oxide nanoparticles with different loading (10-20 wt.%) supported on reduced graphene oxide were synthesized to evaluate the oxidative desulfurization efficiency. The catalyst was synthesized by the incipient wetness impregnation (IWI) technique. Different analysis methods like FT-IR, XRD, FESEM, AFM, and Brunauer-Emmett-Teller (BET) were utilized to characterize graphene oxide and catalysts. The XRD analysis showed that the average crystal size of graphene oxide was 6.05 nm. In addition, the FESEM results showed high metal oxide dispersions on the rGO. The EDX analysis shows the weight ratio of Sn is close to its theoretical weight.
... Show MoreThe study included selection six species of the fungi related to Pleurotus genus were evaluated for their ability to production of Pleurotin, one of them, Pleurotus ostreatus (P.11) was isolated and identified in the present study. Pleurotin was extracted with screening by Thin Layer Chromatography (TLC) and quantification High Performance Liquid Chromatography (HPLC). Cytotoxicity of Pleurotin extracted from P. ostreatus (P.11) grown in different sugar sources (galactose, mannitol, sucrose, dextrose and lactose) liquid media was test against three selected cancer cell lines, CaSki, MCF-7 and A549 addition to Human Non Cancer Fibroblast Cell Line (MRC-5). Pleurotin of P. ostreatus (P.11) grown in galactose induced the significant highest
... Show MoreIn this work pyrazolin derivatives were prepared from the diazonium chloride salt of 4-aminobenzoic acid. Azo compounds were prepared from the reaction of an ethanolic solution of sodium acetate and calculated amount of active methylene compound namely, acetyl acetone to obtain the corresponding hydrazono derivative (1). Cyclocondensation reaction of compounds (1) with hydrazine hydrate and phenyl hydrazine in boiling ethanol affording the corresponding pyrazoline-5-one derivatives of 4-aminobenzoic acid (2,3). Then compound (3) was reacted with thionyl chloride to give the corresponding acid chloride derivative(4), followed by conversion into the corresponding acid hydrazide derivative (5) carboxylic acid thiosemicarbazide (11), esters
... Show More