Background: Masseter muscle is a jaw closing muscle of the mandible involved in Para functional habits; which include lip and cheek chewing, fingernail biting, and teeth clenching or bruxism which can be classified as awake or sleep bruxism. Patients with sleep bruxism are three to four times more likely to experience jaw pain and limitation of movement than people who do not experience sleep bruxism. The aim of this study is to measure the thickness of the masseter muscle in bruxist subjects and compare it with non-bruxist subjects by using sonography. Materials and Method: Forty Iraqi subjects with age ranged (20-40) divided into two groups according to the presence of bruxism. Clinical examination was made and masseter muscle thickness measured for both groups using sonography. Results: For bruxist subjects the mean thickness of masseter muscle in relaxation and clenching were (11.7 ± 1.4 mm) and (16.4 ± 1.3 mm). For non bruxist subjects were (11.2 ± 0.4 mm) and (13 ±0.3 mm) respectively. There was an extremely high statistical significant difference in masseter muscle thickness under clenching between bruxist and non bruxist subjects ( it was higher in bruxist group). Masseter muscle thickness under relaxation was significantly lower than that under clenching for both groups. Also there was a positive correlation between masseter muscle thickness and muscle function in bruxism situation. Conclusion: Masseter muscle in bruxist subject was thicker when compared to non-bruxist subject. Masseter muscle thickness was found to be positively correlated with increasing muscle function. The findings of this study indicate that the functional capacity of the masseter muscle affected by bruxism and may be considered as one of the factors influencing muscle thickness.
Aims: This study was conducted to assess the effect of the addition of yttrium oxide (Y2O3) nanoparticles on the tensile bond strength, tear strength, shore A hardness, and surface roughness of soft-denture lining material. Materials and Methods: Y2O3 NPs with 1.5 and 2 wt.% were added into acrylic-based heat-cured soft-denture liner. A total of 120 specimens were prepared and divided into four groups according to the test to be performed (tensile bond strength, tear strength, surface hardness, and surface roughness). Results: There was a highly significant increase in tensile bond strength between the soft liner and the acrylic denture base, tear strength, and hardness at both concentrations as compared to the control group, whereas ther
... Show MoreA chemometric method, partial least squares regression (PLS) was applied for the simultaneous determination of piroxicam (PIR), naproxen (NAP), diclofenac sodium (DIC), and mefenamic acid (MEF) in synthetic mixtures and commercial formulations. The proposed method is based on the use of spectrophotometric data coupled with PLS multivariate calibration. The Spectra of drugs were recorded at concentrations in the linear range of 1.0 - 10 μg mL-1 for NAP and from 1.0 - 20 μg mL-1 for PIR, DIC, and MEF. 34 sets of mixtures were used for calibration and 10 sets of mixtures were used for validation in the wavelength range of 200 to 400 nm with the wavelength interval λ = 1 nm in methanol. This method has been used successfully to quant
... Show MoreThis work includes preparation of Az, Qz, and Tz derivatives from the reaction of Schiff base (Sb) derivative with anthranilic acid, chloroacetyl chloride, and sodium azide, as well as, the characterization via FT-IR, 1H-NMR, and 13CNMR. The anticorrosion inhibition of these compounds was studied and the measurements of carbon steel (CS) corrosion in sodium chloride solution 3.5% (blank) and inhibitor in solutions were calculated at a temperature range of 293-323 K by the technique of electrochemical polarization. In addition, some thermodynamic and kinetic activation parameters for inhibitor and blank solutions (Ea⋇, ΔH⋇, ΔS⋇, and ΔG⋇) were determined. The results showed high inhibition efficacy for all the prepared compounds,
... Show MoreThe electrochemical polymerization of the monomer sulfanilamide (SAM) in an aqueous solution at room temperature produces polysulfanilamide (PSAM). The Fourier Transform Infrared spectroscopy (FTIR) was used to investigate the properties of the prepared polymer layer that generated on the stainless steel (St.S) surface (working electrode) and Atomic Force Microscope (AFM) was used to characterize the morphology, topology, and detailed surface structure of polymer layer that generated on the surface. The corrosion behavior of uncoated and coated St.S were evaluated by using the electrochemical polarization method in a 0.2 M HCl solution and a temperature range of 293–323 K, the anticorrosion action of the polymer coating on stainless steel
... Show More