Background: This clinical trial aims to evaluate the color changes of direct resin composite veneer (DCV) restorations based on spectrophotometric analysis of 4 different types of resin composites between the baseline immediately after polishing and after one year of follow-up. Materials and methods: 28 patients were assessed for eligibility for participation, aged between 18 and 38 years old, who indicated for DCV restorations in anterior maxillary teeth were considered for participation in this study. In total, 25 patients who met the inclusion criteria were selected (6 males and 19 females, mean age: 20.9 at the time of restoration placement), and 3 patients were excluded. Participants were divided into four groups based on the type of composite resin used for restorations. Group 1 nanohybrid Ips Empress direct (Ivoclar Vivadent)](IPS) (13 restorations/6 patients), group 2 microfilled [Essentia (GC cooperation Japan)](ES) (14 restorations / 7 patients), group 3 supra-nano filled [ Estelite ∑ Quick (Tokuyama, Tokyo, Japan)](EQ) (17 restorations / 7 patients) and group 4 nanofill [Filtek Ultimate (3M ESPE)](FU) (13 restorations / 5 patients). Baseline Color measurements were performed with a spectrophotometer immediately after finishing and polishing (baseline), and after one year of recall, color change (ΔE) from baseline values and after one year of follow-up of DCVs were calculated according to CIELab color coordinates. For this, a silicone mold was fabricated for each patient and used as a guide for each measurement to standardize the site of the readings. Statistical analysis of the data was applied using the Kruskal-Wallis test with Dunn-Bonferroni posthoc test after controlling the distribution of data in terms of normality with the Shapiro Wilk test. Results: At the end of one year,25 participants(57restorations) were followed up. The mean ΔE of IPS, EQ, and FU composites were higher than the ES composite resin, but there was no statically significant difference between all types of composites (P> 0.05). There was no statistically significant difference in the mean ΔL* between any types of composite resin (p> 0.05). There was a significant change in Δa* and Δb* after a one-year recall for all the types of DCV restorations (p < 0.05). Conclusion: After one year of follow-up, the spectrophotometer measurements of direct resin composite veneer restorations, it was concluded no difference between the mean ΔE of ES, IPS, FU, and EQ resin composite. ES (Microfilled hybrid) showed a lower mean ΔE value compared to the other groups. All groups of resin composite showed color changes within clinically acceptable levels after a one-year follow-up.
Background: Restoration of the gingival margin of Class II cavities with composite resin continues to be problematic, especially where no enamel exists for bonding to the gingival margin. The aim of study is to evaluate the marginal leakage at enamel and cementum margin of class II MOD cavities using amalgam restoration and modern composite restorations Filtek™ P90, Filtek™ Z250 XT (Nano Hybrid Universal Restorative) and SDR bulk fill with different restoratives techniques. Materials and method: Eighty sound maxillary first premolar teeth were collected and divided into two main groups, enamel group and cementum group (40 teeth) for each group. The enamel group was prepared with standardized Class II MOD cavity with gingival margin (1 m
... Show MoreBackground: The incorporation of rubber has not been entirely successful because it can have detrimental effects on the transverse Strength and hence the rigidity of the denture base. Materials and methods: Zirconium oxide nanoparticales were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 3% by weight then mixed with powder using conventional procedure.(100) samples were prepared and divided into five groups according to the test performed ,Each group consisted of 20 specimens and these were subdivided into 2 groupsGroup (A): control group (10 specimens of high impact acrylic resin without zirconium oxide) and Group (B):zirconium oxide group(10 specimens of high impac
... Show MoreBackground: Vibration decreases the viscosity of composite, making it flow and readily fit the walls of the cavity. This study is initiated to see how this improved adaptation of the composite resin to the cavity walls will affect microleakage using different curing modes
Materials and methods: Standard Class V cavities were prepared on the buccal surface of sixty extracted premolars. Teeth were randomly assigned into two groups (n=30) according to the composite condensation (vibration and conventional) technique, then subdivided into three subgroups (n=10) according to light curing modes (LED-Ramp, LED-Fast and Halogen Continuous modes). Cavities were etched and bonded with Single Bond Universal
... Show MoreWe know that the experiments which conducted by latin square in one location or in one period (season), but there are many cases that need to conduct the same experiments in many locations or in many periods (seasons) to study the interaction between the treatments and locations or between the treatments and periods (seasons) .In this research we present an idea for conduct the experiment in several locations and in many period (seasons) by using LSD , it represent acontribution in the area of design and analysis of experiments ,we had written. we had written (theoretically) the general plans, the mathematical models for these experiments, and finding the derivations of EMS for each component (
... Show MoreThis work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.
In the present study, composites were prepared by Hand lay-up molding and investigated. The composites constituents were epoxy resin as the matrix, 6% volume fractions of Glass Fibers (G.F) as reinforcement and 3%, 6% of industrial powder (Calcium Carbonate CaCO3, Potassium Carbonate K2CO3 and Sodium Carbonate Na2CO3) as filler. Density, water absorption, hardness test, flexural strength, shear stress measurements and tests were conducted to reveal their values for each type of composite material. The results showed that the non – reinforced epoxy have lower properties than composites material. Measured density results had show an incremental increase with volume fraction increase
... Show More