Background: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center of the crown, closer to the lateral incisor. The linear displacement of the teeth, strains of the periodontal ligament, and stresses in PEEK wire and composite were evaluated. The data was numerically produced with color coded display by the software. Selected values were tabulated and compared among models. Results: The amount of linear displacement and strain was very low. Stresses in the wire and composite were affected by the size and position of the composite bonding spot. The safe limits were identified at 235 MPa for PEEK and 100 MPa for composite. The basic model had a von Mises stress in the PEEK wire of 122.09 MPa, and a maximum principal stress in the composite of 99.779 MPa. Both stresses were within the safe limits, which means a lower risk of failure in PEEK and composite. All other models had stresses that exceeded the safe limit of the composite. The 3 mm composite model was the only one that developed stresses in the wire more than the safe limits of PEEK. Conclusions: Within the limitations of this study, bonding PEEK wires with 4 mm bonding spots to the clinical crown center provided the best mechanical performance of the wires and spots; otherwise, the mechanical properties of the wire and composite would be affected and, therefore, might affect the retention process. Keywords: Retention, PEEK, Finite element analysis
Tool wear is a major problem in machining operations because the resulting material loss gradually changes of the machine tool. There many factors may leads to material loss like; friction, corrosion, and also it’s happened by rubbing during machining processes between the work piece and the tool. Dimensional accuracy of the work piece, and also the surface finish will be reducing by tool wear. It can also increase cutting force. In this study, we focused on the effect of the coating process on crater wear problems. Crater wear is caused by the flow between the chip and the rake face of the tool, whereas flank wear is caused by the contact between the tool and the work piece. In reducing crater wear, aluminum titanium nitride (AlTiN) u
... Show MoreThe effects of scattering and secondary radiation generated inside the material on dose equivalent rate where studied using Co60 and Cs137 sources of activity (199.8 , 177.6) MBq , respectively for different thicknesses of Al , Pb and Pb- glass . The results showed that the equivalent rate increases when the effect of scattering was included for Al and Pb shields with cobalt-60 source of energy 1.25 MeV ; and decreases for Pb shield with Cs-137 source of energy 0.662MeV .The results showed also that the atomic number of The material effects the dose equivalent rate . The Pb-glass shield was found to be more efficient in absorption than other shields.
Background: Disinfection and shaping of the canal with a combination of chem¬ical agents and endodontic instruments play an important role in the success of endodontic therapy. Eliminating the microorganisms within the pulp space is a critical and important objective in treating a tooth with apical periodontitis. This study was conducted to evaluate the antibacterial properties of herbal alternatives (Green tea and siwak extracts) as possible irrigants during endodontic treatment compared with the conventional irrigation solutions. Materials and methods: Salvadora Persica (siwak) and Green Tea solutions were prepared.An agar diffusion test was performed on Mueller-Hinton agar using the well diffusion method. The tested solutions (5.25% N
... Show MoreA nanocrystalline CdS thin film with 100 nm thickness has been prepared by thermal evaporation technique on glass substrate with substrate temperature of about 423 K. The films annealed under vacuum at different annealing temperature 473, 523 and 573 K. The X-ray diffraction studies show that CdS thin films have a hexagonal polycrystalline structure with preferred orientation at (002) direction. Our investigation showed the grain size of thin films increased from 9.1 to 18.9 nm with increasing the annealing temperature. The optical measurements showed that CdS thin films have direct energy band gap, which decreases with increasing the annealing temperature within the range 3.2- 2.85 eV. The absorbance edge is blue shifted. The absorption
... Show MoreIn this research, analytical study for simulating a Fabry-Perot bistable etalon (F-P cavity) filled with a dispersive optimized nonlinear optical material (Kerr type) such as semiconductors Indium Antimonide (InSb). An optimization procedure using reflective (~85%) InSb etalon (~50µm) thick is described. For this etalon with a (50 µm) spot diameter beam, the minimum switching power is (~0.078 mW) and switching time is (~150 ns), leading to a switching energy of (~11.77 pJ) for this device. Also, the main role played by the temperature to change the etalon characteristic from nonlinear to linear dynamics.
In the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .
Autorías: Ghassan Adeeb Abdulhasan, Falih Hashim Fenjan, Hussein Jabber Abood. Localización: Revista iberoamericana de psicología del ejercicio y el deporte. Nº. 3, 2022. Artículo de Revista en Dialnet.
Purpose: To evaluate the effect of different surface treatments on shear bond strength between dentin and IPS e.max lithium disilicate glass-ceramic. Materials and Methods: Eighteen extracted third molars were embeded in epoxy resin. The tooth was sectioned vertically in mesiodistal direction using a low speed hard tissue microtome. The buccal and lingual surfaces of each section were ground flat using 600 grit Silicone carbide paper. Eighteen ceramic discs consisted of lithium disilicate glass-ceramic were prepared with a diameter of 4.7mm and height of 2.2mm. The discs were divided in two groups (n=10): (1) IPS e.max treated with hydrofluoric acid and Monobond Plus (MBP) and (2) IPS e.max treated with Monobond Etch &Prime (MBEP). The toot
... Show MoreAn experiment was carried out at Al-Raed Research Station, which is located on the Baghdad-Anbar road during the winter season, in order to study the effect of the type of solar panels and irrigation system on some performance indicators of irrigation systems and germination percentage of bean crop (Vicia Faba L). A randomized complete block design (RCBD) was used with three replications. The experiment consist of two factors. 1st factor was the solar panel type with two levels : monocrystalline and polycrystalline. Second factor was the irrigation system with two levels Drip and sprinkler irrigation system the following indicators were studied : solar panel efficiency (%), Irrigation