Effect of Polyamide (Nylon 6) Micro-Particles Incorporation into RTV Maxillofacial Silicone Elastomer on Tear and Tensile Strength
...Show More Authors

Background: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were prepared with different percentage of PA-6 micro particles (1%, 3%, and 5%) by weight. Each group was further subdivided into 2 groups according to the conducted tests, i.e. tear and tensile strength tests (n=10). The data were analyzed with a descriptive statistical analysis, one-way ANOVA, post-hoc LSD test. Results: The mean value of tear and tensile strength of 1% PA-6 reinforcement group increased significantly when compared to control group on the contrast to the same values of 3% and 5% PA-6 reinforcement groups which were decreased significantly. Conclusion: the 1% PA-6 reinforcement improved tear as well as tensile strength among all other percentages (0%, 3% and 5%).

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sun Mar 01 2020
Journal Name
Iraqi Journal Of Physics
Effect of Laser Energy and Repetition Rate on Holmium Plasma Emission
...Show More Authors

The holmium plasma induced by a 1064-nmQ-switched Nd:YAG laser in air was investigated. This work was done theoretically and experimentally.  Cowan code was used to get the emission spectra for different transition of the holmium target. In the experimental work, the evolution of the plasma was studied by acquiring spectral images at different laser pulse energies (600,650,700, 750, and 800 mJ). The repetition rates of (1Hz and 10Hz) in the UV region (200-400 nm). The results indicate that, the emission line intensities increase with increasing of the laser pulse energy and repetition rate. The strongest emission spectra appeared when the laser pulse energy is 800mJ and 10 Hz repetition rate at λ= 345.64nm, with the maximum intensi

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sat Jan 01 2022
Journal Name
Journal Of The Mechanical Behavior Of Materials
Concrete strength development by using magnetized water in normal and self-compacted concrete
...Show More Authors
Abstract<p>The main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and </p> ... Show More
Crossref (7)
Crossref
Publication Date
Sat Jan 01 2022
Journal Name
Journal Of The Mechanical Behavior Of Materials
Concrete strength development by using magnetized water in normal and self-compacted concrete
...Show More Authors
Abstract<p>The main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and </p> ... Show More
View Publication
Scopus (5)
Crossref (7)
Scopus Clarivate Crossref
Publication Date
Thu Oct 26 2023
Journal Name
Malaysian Journal Of Science
HEMICAL ELUCIDATION AND BIOLOGICAL SCREENING STUDY OF NEW LIGAND DERIVED FROM 5, 6-O-ISO PROPYLIDENE-L-ASCORBIC ACID AND ITS METAL (II) COMPLEXES
...Show More Authors

الوصف A simple chemistry method approach was used to synthesise new ligand derivate from L-ascorbic acid and its complexes. All of them were water-soluble and are used quite extensively in the medical and pharmaceutical fields. This study synthesised the new ligand derivative from L-ascorbic acid-base using the following steps: A 5, 6-O-isopropylidene-L-ascorbic acid was prepared by reacting dry acetone with L-ascorbic acid followed by reacting it with trichloroacetic acid to yield [chloro (carboxylic) methylidene]-5, 6-O-isopropylidene-L-ascorbic acid in the second stage. In the third stage, the derivative was reacted with (methyl (6-methyl-2-pyridylmethyl) amine to create a new ligand (ONMILA). This novel ligand was identified using

... Show More
Publication Date
Thu Oct 12 2017
Journal Name
Iraqi Journal Of Laser
A Comparative Evaluation of Post-Operative Pain and Function after Gingival Depigmentation Using 940 Nm Diode Laser And Conventional Bur Method: 6 Months Study
...Show More Authors

The aim of the study was to evaluate the efficacy of diode laser (λ=940 nm) in the management of gingival hyperpigmentation compared to the conventional bur method. Materials and methods: Eighteen patients with gingival hyperpigmentation were selected for the study with an age between 12-37 years old. The site of treatment was the upper gingiva using diode laser for the right half and the conventional method for the left half. All patients were re-evaluated after the following intervals: 3 days, 7 days, 1 month and 6 months post-operation. Pain and functions were re-evaluated in each visit for a period of 1 day, 3 days and 1 week post-operation. Laser parameters included 1.5 W in continuous mode with an initiated tip (400 μm) placed in

... Show More
View Publication Preview PDF
Publication Date
Wed Apr 01 2020
Journal Name
Plant Archives
Effect of applying selenium element and ascorbic acid on reducing the harmful effect of environmental stress on wheat plants irrigated by water contaminated with lead and cadmium
...Show More Authors

Scopus (4)
Scopus
Publication Date
Tue Feb 17 2026
Journal Name
Journal Of Baghdad College Of Dentistry
Push-out bond strength of different root canal obturation materials
...Show More Authors

Background: The aim of this study was to evaluate the push-out bond strength of four different obturation materials to intraradicular dentin and to determine the failure mode. Materials and method: forty straight palatal roots of the maxillary first molars teeth were used in this study, the roots were instrumented using crown down technique and rotary EndoSequence system, the roots were randomly divided into four groups according to the materials used for obturation (n=10).Group (1): AH Plus sealer and gutta-percha. Group (2): Activ GP glass ionomer sealer and Activ GP gutta-percha (Activ GP system). Group (3): Bioceramic sealer and Bioceramic gutta-percha. Group (4): GuttaFlow2 sealer and gutta-percha. For all groups single cone obturatio

... Show More
View Publication Preview PDF
Publication Date
Fri Jun 02 2017
Journal Name
Kufa Journal Of Engineering
COMPRESSIVE STRENGTH OF CONCRETE CONTAINING WATER ABSORPTION POLYMER BALLS (WAPB)
...Show More Authors

Water absorbent polymers (WAP) are new component in producing building materials. They provide internal curing which reduces autogenous cracking, eliminates autogenous shrinkage, mortar strength increased, enhance early age strength to withstand strain, improve the durability, introduce higher early age compressive strength, have higher performance and reduce the effect of insufficient external curing. This research used different percent of polymer balls to choose the percent that provides good development in compressive strength with time for both water and air curing. The water absorption polymer balls in this research have the ability to absorb water and after usage in concrete they spill out the water (internal curing) and shri

... Show More
Publication Date
Sat Jan 01 2022
Journal Name
Materials Today: Proceedings
Shear strength of steel fibre RC beams under repeated loads
...Show More Authors

Scopus (1)
Scopus Clarivate Crossref
Publication Date
Wed Jan 01 2014
Journal Name
Journal Of Engineering
Punching Shear Strength of Reinforced Concrete Flat Plates with Openings
...Show More Authors