Background: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown restoration with deep chamfer finishing line all around the tooth with (1mm) depth, axial length (4mm) and convergence angle (6 degree). The specimens separated into two groups; Group A; eight specimens were scanned digitally by using Omnicam scanner; Group B; conventional impressions were taken for the remaining thirty two specimens and further subdivided to four groups according to the time of impression pouring; Group B1: PVS were poured after 30 minutes; Group B2: PVS were poured after 24 hours; Group B3: PVS were poured after 7 days; Group B4:PVS were poured after 14 days. Marginal discrepancy was measured at four points at each tooth surface. Sixteen points per tooth were measured using digital microscope at (180X) magnification. One-way ANOVA test and LSD test were carried out to see if there was any significant difference among the means of the conventional impression groups. Independent samples t-test was carried out to examine if there is any significant difference between digital and conventional impression technique. Results: group B2 had the least mean of marginal gap with statistically significant difference when compared to group B1 and statistically highly significant difference when compared to group B3 and B4. There was a statistically highly significant difference in the vertical marginal gap between digital impression technique and conventional impression. Conclusions: the pouring of conventional impression after 24 hours provides better marginal fit than other pouring time. The digital impression provides better marginal fit than conventional impression.
The influence of different thickness (500,750, and 1000) nm on the structure properties electrical conductivity and hall effect measurements have been investigated on the films of copper indium selenide CuInSe2 (CIS) the films were prepared by thermal evaporation technique on glass substrates at RT from compound alloy. The XRD pattern show that the film have poly crystalline structure a, the grain size increasing with as a function the thickness. Electrical conductivity (σ), the activation energies (Ea1,Ea2), hall mobility and the carrier concentration are investigated as function of thickness. All films contain two types of transport mechanisms of free carriers increase films thickness. The electrical conductivity increase with thickness
... Show MoreThe civil engineering field currently focus on sustainable development. It is important to develop new sustainable and economic generations of concrete, using eco-friendly materials in the construction industry with a fair amount of costs and minimizing the impact upon the environment by reducing CO2 emissions from the cement industry as a whole while still obtaining high cement quality and strength. The main objective of this research is to clarify the mechanical behavior and ability to use Portland limestone cement in producing self compacted concrete, due to the beneficious effec of the limestone cement economically and enviromently. The research investigates the effect of using steel and polymer meshs as reinforcement, where the results
... Show MoreLow- and medium-carbon structural steel components face random vibration and dynamic loads (like earthquakes) in many applications. Thus a modification to improve their mechanical properties, essentially damping properties, is required. The present study focuses on improving and developing these properties, significantly dampening properties, without losing the other mechanical properties. The specimens used in the present study are structural steel ribbed bar ISO 6935 subjected to heating temperatures of (850, 950, and 1050) ˚C, and cooling schemes of annealing, normalizing, sand, and quenching was selected. The damping properties of the specimens were measured experimentally with the area under the curve for the loadi
... Show MoreIn this paper the effect of thermal annealing on the structural and optical properties of Antimony Selenide (Sb2Se3) is investigated. Sb2Se3 powder is evaporated on clean amorphous glass substrates at room temperature under high vacuum pressure (4.5×10-6 mbar) to form thin films. The structural investigation was done with the aid of X-ray diffraction (XRD) and atomic force microscopy (AFM). The amorphous to polycrystalline transformation of these thin films was shown by X-ray diffraction analysis after thermal annealing. These films' morphology is explained. (UV-Vis ) spectra in ranges from 300 to 1100 nm was used to examine the optical properties of the films .The absorption coefficient and optical energy gap of the investigated films are
... Show MoreThe current work studies the effect of adding chopped carbon fiber (CCF) on gypsum plaster properties (precisely the compressive strength and the modulus of rupture). The research plan consists of using six mixes of gypsum plaster; these mixes are divided into two groups according to the (Water/Gypsum) ratios (0.5 & 0.6). Each group was divided into three subgroups according to CCF volume fraction (Vf): 0.0%, 0.2% and 0.4%. Three cubic (50×50×50) mm and three prismatic (40×40×160) mm samples were performed for each mix. It was found that, the addition of CCF to the gypsum plaster mixes increases both the compressive strength and the modulus of rupture for both (W/G) ratios, an
Using photo electrochemical etching technique (PEC), porous silicon (PS) layers were produced on n-type silicon (Si) wafers to generate porous silicon for n-type with an orientation of (111) The results of etching time were investigated at: (5,10,15 min). X-ray diffraction experiments revealed differences between the surface of the sample sheet and the synthesized porous silicon. The largest crystal size is (30 nm) and the lowest crystal size is (28.6 nm) The analysis of Atomic Force Microscopy (AFM) and Field Emission Scanning Electron Microscope (FESEM) were used to research the morphology of porous silicon layer. As etching time increased, AFM findings showed that root mean square (RMS) of roughness and po
... Show MoreAbstract: This study aims to investigate the effects of solvents of various polarities on the electronic absorption and fluorescence spectra of RhB and Rh6G. The singlet‐state excited dipole moments (me) and ground state dipole moments (mg) were estimated from the equations of Bakshiev -Kawski and Chamma‐ Viallet using the variation of Stokes shift along with the solvent’s dielectric constant (e) and refractive indexes (n). The observed singlet‐state excited dipole moments were found to be larger than the ground‐state ones. Moreover, the obtained fluorescence quantum yield values were influenced by the environment of the fluorescing molecule. Consequently, the concentration of the dye solution, excited singlet state absorption and
... Show MoreObjective: To evaluate the effect of mouth rinses (Biofresh and ZAK) on the surface micro hardness
of two light cure restorative material (Tetric ceram ivoclar-vivadent) and (3M Z 250) dental
composite.
Methodology: The microhardness values of (sixty) composite specimens were measured at the top
surfaces after 24 hours of immersion in different solutions (Biofresh, Zak mouth wash and distilled
water as control). Comparison done using descriptive statistics (mean, SD, SEM, minimum and
maximum values) and inferential statistics (ANOVA and LSD) test.
Results: The biofresh mouth rinse which has high alcohol containing has less effect on
microhardness of tetric ceram than the zak &distiled water , while the effect
Poly vinyl alcohol has been studied for its ability to form crystallites by using annealing method. Semicrystalline films of poly vinyl alcohol (PVA) were prepared by casting 11.5 wt. % and 13 wt. % PVA aqueous solution onto glass slides at annealing temperature range 90 -120°C and duration time 15- 60 minute. This allowed the macromolecules to form crystallites, small regions of folded and compacted chains separated by amorphous regions where single PVA chain may pass through several of these crystallites. Degree of crystallinity of PVA films (hydrogels) was determined by method of density; on the other hand the swelling behavior was conducted by the determination of water uptake, wet degree of crystallinity, gel fraction and solubilit
... Show MoreCdS and CdTe thin films were thermally deposited onto glass substrate. The CdCl2 layer was deposited onto CdS surface. These followed by annealing for different duration times to modify the surface and interface of the junction. The diffraction patterns showed that the intensity of the peaks increased with the CdCl2/annealed treatment, and the grain sizes are increased after CdCl2/annealed treatment