Background: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive resin. Shear bond strength was measured by using Tinius Olsen universal testing machine. After debonding, each bracket and zirconium surface were examined and adhesive remnant index was registered. The difference in shear bond strength among groups was analyzed by using ANOVA test. The adhesive remnant index was assessed using Chi-square test. Results: The 2nd laser group had the highest mean value of shear bond strength then the 1st laser group followed by the sandblasting group, while the control group had the least value, non-significant difference in the shear bond strength was found between the laser groups and highly significant difference was found between all other comparable groups. Non-significant difference in the site of bond failure was found between the laser groups and sandblasting group, and between the two laser groups. Conclusion: The laser conditioning method showed higher value of shear bond strength than the sandblasting conditioning method.
Objective(s): This study aims to evaluate the hardness of two commercially available cold cured acrylic resin material
(Vertex and PAN) when polymerized at different temperature in comparison to those polymerized by conventional
methods in air at 23C ± 5C.
Methodology: Eighty specimens, forty from cold cured acrylic (Vertex Type) and forty from cold cured acrylic (PAN
type) were prepared, flasking and packing procedure were done according to manufacturer direction and divided
according to processing as follow: 20 specimens (10 from Vertex type and 10 from PAN type) were processed in air for
two hours at 23C ± 5C under press (bench curing) as a control, and 60 specimens (30 from Vertex type and 30 from
PAN type) wer
Background: The microhardness of a composite resin is a vital parameter that is used to determine its clinical behavior. Measuring the microhardness of a composite resin has been used as an indirect method to assess its degree of conversion and extent of polymerization. The purpose of this in vitro study was to evaluate the effect of three curing distances (0, 2, and 4 mm) on the microhardness of the top and bottom surfaces of three types of flowable bulk-fill composite resins (smart dentin replacement, Opus bulk fill flow, and Tetric N). Material and method: Sixty-three specimens from the three types of composite resins (n=21) were fabricated using Teflon mold with a 4mm depth and a 5 mm internal diameter and cured for 20 seconds. For e
... Show MoreAn experimental study was conducted on pressure drop of water flow through vertical cylindrical packed beds in turbulent region and the influence of the operating parameters on its behavior. The bed packing was made of spherical and non-spherical particles (spheres, Rasching rings and intalox saddle) with aspect ratio range 3.46 D/dp 8.486 obtaining bed porosities 0.396 0.84 and Reynolds number 1217 21758. The system is consisted of 5 cm inside diameter Perspex column, 50 cm long; distilled water was pumped through the bed with flow rate 875, 1000, 1125, 1250,1375 and 1500 l/h and inlet water temperature 20, 30, 40 and 50 ˚C. The packed bed system was monitored by using LabVIEW program, were the result
... Show MoreBackground: Radiotherapy, is therapy using ionizing radiation in order to deliver an optimal dose of either particulate or electromagnetic radiation to a particular area of the body with minimal damage to normal tissues. The source of radiation may be outside the body of the patient (external beam irradiation) or it may be an isotope that has been implanted or instilled into abnormal tissue or a body cavity. Called also radiotherapy. The aim of work studies the relationship between the depth dose and the high photon xray energies (6MeV and 10MeV). Patients and methods: in our work, we studied the dose distribution in water phantom given at different depths (zero-18) cm deep at1cm intervals treated with different field size (5×5-,10×1
... Show MoreIn humans, Pseudomonas aeruginosa is the second most frequent gram negative nosocomial pathogen in hospitals and has the highest case-fatality rate of all hospital-acquired bacteremia because of the hardy resistance of these bacteria to mechanical cleansing as well as to disinfectant, and many antibiotics. The susceptibility of bacteria against the antibiotics is modulated by several local factors such as temperature which modified drug efficacy, so this study was carried out to evaluate the effect of different temperature (20,42,45)Ċon the susceptibility of Pseudomonas aeruginosa to the minimum inhibitory concentrations (MIC) of the antimicrobial agents before and after irradiation. The samples collected from 150 persons suffering from
... Show MoreBackground: Nicotine is the foremost chemical constituent responsible for addiction in tobacco products, in the non-ionized condition can be easily absorbed via epithelial tissue of the lung, the mouth, the nose and across the skin
Objective:The study examines the harmful effect of the nicotine which is an important component of cigarette in vitro.
Type of the study: Cross-sectional study.
Methods: Examines the harmful effect of the nicotine which is an important component of cigarette in vitro by using two types of lung cancer cell lines (H460 TP53+/+, H441 TP53-/-).