Background: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive resin. Shear bond strength was measured by using Tinius Olsen universal testing machine. After debonding, each bracket and zirconium surface were examined and adhesive remnant index was registered. The difference in shear bond strength among groups was analyzed by using ANOVA test. The adhesive remnant index was assessed using Chi-square test. Results: The 2nd laser group had the highest mean value of shear bond strength then the 1st laser group followed by the sandblasting group, while the control group had the least value, non-significant difference in the shear bond strength was found between the laser groups and highly significant difference was found between all other comparable groups. Non-significant difference in the site of bond failure was found between the laser groups and sandblasting group, and between the two laser groups. Conclusion: The laser conditioning method showed higher value of shear bond strength than the sandblasting conditioning method.
a laser ablation Q-switched Nd: YAG laser with a wave-length of 355 nm at a variety of laser pulse energies (E) and deposited on porous silicon (PS). Optical emission spectrometer was used to diagnosed medium air to study gold plasma characteristics and prepared Au nanoparticles. The laser pulse energy influence has been studied on the plasma characteristics in air. The data showed the emergence of the ionic (Au II) spectral emission lines in the gold plasma emission spectrum. XRD has been utilized to examine structural characteristics. Moreover, AFM results 37.2 nm as the mean value of the diameter that is coordinated in a shape similar to the rod that appears for Au NPs, in addition to that, TEM has been an indication of the fact that syn
... Show MoreBackground: The gene encoding a disintegrin and metalloproteinase domain 33 (ADAM33) is known to be associated with asthma in different ethnic groups. In Iraq, among the Arab ethnic background, this association has not yet been highlighted. Methods: One hundred and ninety-two asthmatics were examined; 118 males and 74 females (mean age 38.23 ± 9.13 years). The control group was 183; 110 males and the rest were females. The SNP of rs2280091 A/G (T1) was studied here to determine adam33 genotyping status using polymerase chain reaction–restriction fragment length polymorphism (PCR–RFLP). The level of total IgE was measured using enzyme-linked immunosorbent assay (ELISA). Results: Significant differences (p = 0.004) in the frequencies of
... Show MoreIn this work, the synergistic effect of chlorinated rubber (additive I),with zeolite 3A (additive II), zeolite 4A (additive III), and zeolite 5A (additive IV) in (1:1) weight percentage, on the flammability for unsaturated polyester resin was studied in the weight ratios for (3,7,10,13&15%) by preparing films of (130×130×3) mm in diameters. Three standard test methods used to measure were the flame retardation which are; ASTM: D-2863, ASTM: D- 635& ASTM: D-3014. Results obtained from these tests indicated that all of the additives were effective additive IV has the highest efficiency as a flame retardant.
The study involved preparing a new compound by combining between 2-hydroxybenzaldehyde and (Z)-3-hydrazineylideneindolin-2-one resulting in Schiff bases and metal ions: Mn(II), Co(II), Ni(II), Cu(II), and Zn(II) forming stable minerals-based-Schiff complexes. The formation of resulting Schiff bases is detected spectrally using LC-Mss which gave corresponding results with theoretical results, 1H-NMR proves the founding of N=CH signal, FT-IR indicates the occurrence of imine band and UV-VIs mean is proved the ligand formation. On the other hand, minerals-based-Schiff was characterized using the same spectral means that relied with ligand (Schiff bases). Those means gave satisfactory results and proved the suggested distinguishable geometries.
... Show MoreBiodiesel can be prepared from various types of vegetable oils or animal fats with the aid of a catalyst.
Calcium oxide (CaO) is one of the prospective heterogeneous catalysts for biodiesel synthesis. Modification
of CaO by impregnation on silica (SiO2) can improve the performance of CaO as catalyst. Egg shells and rice
husks as biomass waste can be used as raw materials for the preparation of the silica modified CaO catalyst.
The present study was directed to synthesize and characterize CaO impregnated SiO2 catalyst from biomass
waste and apply it as catalyst in biodiesel synthesis. The catalyst was synthesized by wet impregnation
method and characterized by x-ray diffraction, x-ray fluorescence, nitr
The preparation and characterization of innovative nanocomposites based on zinc oxide nanorods (ZNR) encapsulated by graphene (Gr) nanosheets and decorated with silver (Ag), and cupper (Cu) nanoparticles (NP) were studied. The prepared nanocomposites (ZNR@Gr/Cu-Ag) were examined by different techniques including Field Emission Scanning Electron Microscope (FESEM), Transmission electron microscopy (TEM), Atomic force microscopy (AFM), UV-Vis spectrophotometer and fluorescence spectroscopy. The results showed that the ZNR has been good cover by five layers of graphene and decorated with Ag and Cu NPs with particles size of about 10-15 nm. The ZNR@Gr/Cu-Ag nanocomposites exhibit high absorption behavior in ultraviolet (UV) region of sp
... Show MoreThe removal of heavy metal ions from wastewater by ion exchange resins ( zeolite and purolite C105), was investigated. The adsorption process, which is pH dependent, shows maximum removal of metal ions at pH 6 and 7 for zeolite and purolite C105 for initial metal ion
concentrations of 50-250 mg/l, with resin dose of 0.25-3 g. The maximum ion exchange capacity was found to be 9.74, 9.23 and 9.71 mg/g for Cu2+, Pb2+, and Ni2+ on zeolite respectively, while on purolite C105 the maximum ion exchange capacity was found to be 9.64 ,8.73 and 9.39 for Cu2+, Pb2+, and Ni2+ respectively. The maximum removal was 97-98% for Cu2+ and Ni2+ and 92- 93% for Pb2+ on zeolite, while it was 93-94% for Cu2+, 96-97% for Ni2+, and 87-88% for Pb2+ on puroli