Background: The aim of this study was to measure the radiopacity (RO) of modified microhybrid composite resins by adding 2 types of nanofillers (Zinc Oxide and Calcium Carbonate) in two concentrations 3% and 5% and comparing them to unmodified microhybrid composite resins and to nanofilled composite resin. Materials and Methods: Two types of composite resin were used (Microhybrid composite MH Quadrent anterior shine and Nanofilled composite resin Filtek Z350 XT), for each tested group five disk-shaped specimens (1-mm-thick and 15 mm diameter) were fabricated. The material samples were radiographed together with the aluminum step wedge. The density of the specimens was determined with a transmission densitometer and was expressed in term of equivalent thickness of aluminum. Data analyzed by one-way ANOVA. Results: The radiopacity (RO) values of the tested group ranged between (0.9293- 2.6242 Eq. Al thickness) and there were significant differences among them. Nanofilled composite resin Filtek Z350 XT showed the highest value of RO while unmodified Microhybrid composite MH Quadrent anterior shine showed the lowest value of RO. Conclusion: The addition of 3% of both the ZnO and CaCO3 nanofillers fillers to microhybrid composite significantly increased the RO, while the addition of 5% of CaCO3 and ZnO nanofillers to microhybrid composite showed non-significant increase in the RO of the composite.
Effects of Ozonated Water on Micro Leakage between Enamel and Fissure Sealants Prepared by Different Etching Technique (An in vitro Study), Baraa M Jabar*, Muna S Khalaf
Objective. This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. Materials and Methods. Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water stora
... Show MoreMefenamic acid was esterified with starchwith[1:1] Molar ratio, as drug substituted with natural polymer, to prolongthe period of hydrolysis of drug polymer with other advantages. The new prodrug starch was characterized by FT-IR and UV-Visible and 1H-NMR spectroscopies. The physical properties were studied and controlled drug release was studied in different pH values at 37oC. The stability of drug was carried out by measuring the absorbance of mefenamic starch which hydrolyzed in HCl solution of pH 1.1 (artificial gastric fluid) and phosphate buffer of pH 7.4 (simulating intestinal fluid SIF) at 37oC for several days. The thermal analysis such as DSC was studied.
Objectives: This study aims to assess and compare the micro-shear bond strength (μSBS) of a novel resin-modified glass-ionomer luting cement functionalized with a methacrylate co-monomer containing a phosphoric acid group, 30 wt% 2-(methacryloxy) ethyl phosphate (2-MEP), with different substrates (dentin, enamel, zirconia, and base metal alloy). This assessment is conducted in comparison with conventional resin-modified glass ionomer cement and self-adhesive resin cement. Materials and methods: In this in vitro study, ninety-six specimens were prepared and categorized into four groups: enamel (A), dentin (B), zirconia (C), and base metal alloys (D). Enamel (E) and dentin (D) specimens were obtained from 30 human maxillary first premolars e
... Show MoreABSTRACT Background: This study measured the effects of three parameters pH value, length of immersion and type of archwire on metal ions released from orthodontic appliances. Materials and Methods: Ninety maxillary halves simulated fixed orthodontic appliances that were immersed in artificial saliva of different pH values (6.75, 5 and 3.5) during 28 day period. Three types of archwires were used: stainless steel, nickel titanium and thermal activated nickel titanium. The quantity of nickel and chromium ions was determined with the use of atomic force spectrophotometer while iron ions by spectrophotometer. Each orthodontic set was weighted two times, before the ligation and immersion in the artificial saliva and after 28 days at the end of
... Show MoreMetoprolol is a β1 adrenergic blocker used in treatment of heart diseases. Metoprolol (100mg) tablets was formulated as a modified release oral system utilizing the concept of bilayer system, first layer contained (30mg) as immediate release and the other (70mg) in the sustained release matrix. The immediate release layer consisted of lactose or microcrystalline cellulose as diluents with sodium starch glycolate or sodium croscarmellose as disintegrants. The result showed that the layer contains microcrystalline cellulose and 2% sodium starch glycolate gave disintegration time similar to that of conventional metoprolol tartrate tablet. This result was subjected in the subsequent preparation of the bilayer tablet. The
... Show MoreIntroduction: We aimed to assess the impact of adhesive and wires types on the tensile bond strength of fixed lingual retainers. Methods: A total of 160 intact bovine teeth were collected, cleaned, stored in 25% sodium hypochlorite, and randomly assigned to two groups based on the adhesive type: a two-step adhesive and a one-step adhesive. Each group was further divided into four subgroups based on the type of lingual retainer wire, which included (A) 8-strand braided stainless steel wire, (B) three-strand titanium retainer wire, (C) stainless steel chain, and (D) fiber-reinforced retainer. A tensile bond strength test was conducted using a universal testing machine at a controlled speed of 10 mm/min. Result: The 8-strand braided stainles
... Show More