Background: The present in-vitro study was undertaken to evaluate and compare fracture resistance of weakened endodontically treated premolars with class II MOD cavities restored with different bulk fill composite restorations (EverX posterior, Alert, Tetric EvoCeram Bulk Fill, and SDR). The type and mode of fracture were also assessed for all the experimental groups. Materials and Method: Forty-eight human adult maxillary premolar teeth were selected for this study. Standardized extensive class II MOD cavities with endodontic treatment were prepared for all teeth, except those that were saved as intact control. The teeth were divided into six groups of eight teeth each (n=8): (Group 1) intact control group, (Group 2) unrestored teeth with endodontic treatment, (Group 3) restored with (TetricEvoCeram Bulk Fill), (Group 4) restored with SDR bulk-fill flowable composite, (Group 5) restored with EverX Posterior composite and (Group 6) restored with Alert composite. . All specimens were subjected to compressive axial loading until fracture in a universal testing machine. The data were statistically analyzed using one-way ANOVA test and LSD test. Macroscopic fracture type were observed and classified into favorable and unfavorable. Specimens in groups 3, 4, 5 and 6 were examined by stereomicroscope at a magnification of 20× to evaluate the mode of failure into adhesive, cohesive or mixed. Results: The mean fracture load was (1.2505Kn) for group 1, (0.371Kn) for group 2, (0.512 Kn) for group 3, (0.6435 Kn) for group 4, (0.608 Kn) for group 5, and (0.8315) for group 6. Using one way ANOVA test a highly significant difference (P < 0.01) were found among all groups. The use of Alert composite (which contain micro glass fiber) improved the fracture resistance significantly in comparison to other groups. SDR bulk-fill flowable composite showed better improvement in fracture resistance but with no significant differences in comparison to EverX composite restoration (which contain Short E-glass fiber filler). The type of failure was unfavorable for all the restored groups. Conclusion: All experimental composite restorations showed significant improvement in the resistance to cuspal fracture in comparison to unrestored one (group 2). However, under the conditions of this study, direct composite restorations should be considered as a valid interim restoration for weakened endodontically treated teeth before cuspal coverage can be provided.
الخلاصة: الحكة اليوريمية لدى مرضى غسيل الكلى يؤثر على أكثر من 40٪ من المرضى. وربما ترتبط الحكة المستمرة بمستويات عالية من الإنترلوكين 31. الاهداف: النظر إلى مستويات مصل إنترلوكين 31 لدى مرضى غسيل الكلى المصابين بمرض الكلى في المرحلة النهائية، سواء مع أو بدون حكة يوريمية. النتائج: لم يكن مستوى المصل [الوسيط (] لـ IL-31 في المرضى الذين يعانون من الحكة اليوريميةأو بدون حكة في عينة مصل ما قبل غسيل الكلى مختلفًا بشكل م
... Show MoreAn essential issue in obstetrics is the prevalence of maternal and fetal complications in pregnant women with polycystic ovary syndrome (PCOS). The purpose of the present study was to investigate the prevalence of pregnancy complications among various phenotypes of pregnant women with PCOS.
This paper deals with finite element modeling of the ultimate load behavior of double skin composite (DSC) slabs. In a DSC slab, shear connectors in the form of nut bolt technique studs are used to transfer shear between the outer skin made of steel plates and the concrete core. The current study is based on finite element analysis using ANSYS Version 11 APDL release computer program. Experimental programmes were carried out by the others, two simply supported DSC beams were tested until failure under a concentrated load applied at the center. These test specimens were analyzed by the finite element method and the analyses have shown that these slabs displayed a high degree of flexural characteristics, ultimate strength,
... Show MoreBackground: The objective of this in vitro study was to evaluate the vertical marginal fit of crowns fabricated with ZrO2 CAD/CAM, before and after porcelain firing cycles and after glaze cycles. Materials and Methods: An acrylic resin model of a left maxillary first molar was prepared and duplicated to have Nickel-Chromium master die. Ten die stone dies were sent to the CAD/CAM (Amann Girrbach) for crowns fabrication. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) before (Time 0) and after porcelain firing cycles (Time 1) and after glaze cycles (Time 2) using a light microscope at a magnification of ×100. One way ANOVA LSD tests were performed to determine wh
... Show MoreThe primary objective of this study was to identify the mechanisms for the development and propagation of longitudinal cracks that initiate at the surface of composite pavement. In this study the finite element program ANSYS version (5.4) was used and the model worked out using this program has the ability to analyze a composite pavement structure of different layer properties. Also, the aim of this study was modeling and analyzing of the composite pavement structure with the physical presence of crack induced in concrete underlying layer. The results obtained indicates that increasing the thickness of the asphalt layer tends to decrease the stress intensity factor, which may be attributed to the rapidly decrease of horizontal tensile st
... Show MoreBackground: In this study we evaluate the effect of plasma treatment (oxygen and argon) gas in two different exposure times on the surface of heat cure and light cure acrylic resin. Materials and method: 100 specimens of heat cure and light cure acrylic resin were fabricated. The measurements of the samples were (75mm, 25mm and 4.5mm) length, width and depth respectively with stopper of 3mm depth. Two types of gas used oxygen and argon in (5,10) min by using (DC-glow discharge plasma device) then we apply cold cure soft lining material, with the help of Instron machine we test the shear stress value. Results: A highly significant effect after argon and oxygen gases treatment in both 5 and 10 min exposure times on shear bond strength to soft
... Show MoreBackground: The aim of this study was to evaluate the effect of thermo cycling and different pH of artificial saliva (neutral, acidic, basic) on impact and transverse strength of heat cure acrylic resin reinforced of with 5% silanated ZrO2 nano fillers. Materials and methods: 120 samples were prepared, 60 samples for impact strength test and another 60 samples for transverse strength test, for each test, samples were divided into two major groups (before and after thermo cycling), then each of these major groups were further subdivided into 3 subgroups according to the pH of prepared artificial saliva (neutral, acidic, basic). Charpy impact device was used for impact strength test and Flexural device was used for transverse strength test. R
... Show More