Background: Sealers should demonstrate adhesive properties to dentin, decreasing the chance of endodontic treatment failure. Increased adhesive properties to dentin may lead to greater strength of the restored tooth, which may provide greater resistance to tooth fracture and clinical longevity of an endodontically treated tooth. The aim of this study was to evaluate the shear bond strength of Bioceramic iRoot SP sealer, AH plus sealer and Apexit plus sealer in absence or presence of smear layer using push out bond strength test. Materials and Methods: Sixty straight single roots of the mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments to achieve tapered canal walls, instrumentation was done with copious irrigation of 5.25% sodium hypochlorite. Roots were randomly divided into three groups according to the type of sealer used (twenty teeth for each group): Group A: Apexit plus + gutta percha, Group B: AH plus sealer + gutta percha, Group C: iRoot SP sealer + gutta percha .Then groups were subdivided according to types of final irrigation into two subgroups. Groups (A1, B1, and C1) were irrigated with 5 ml of 5.25% NaOCl for 1 minute while Groups (A2, B2, and C2), the smear layer was removed with 5 ml of 17% EDTA for 1 minute. All groups were rinsed with distilled water and then obturated with cold lateral condensation technique, the roots then stored in moist environment at 37°C for one week. The roots were embedded in clear acrylic resin and three horizontal sections were prepared at a thickness of 1 mm ±0.1 in the apical, middle and coronal parts of each root. The test specimens were subjected to the push-out test method using a Universal Test Machine that carried 1-mm, 0.5- mm and 0.3-mm plungers for coronal, middle and apical specimens, respectively. The loading speed was 0.5 mm/ min. The computer showed the higher bond force before dislodgment of the filling material. These forces were divided by the surface area to obtain the bond strength in MPa. Results: The results showed that the bond strengths of iRoot SP and AH Plus were significantly higher than those of Apexit plus, but there was no significant difference between the bond strength of iRoot SP and AH Plus.In terms of root segments, the bond strengths in the middle specimens and the apical specimens were higher compared with the bond strengths in the coronal specimens. Conclusion: The presence or absence of smear layer did not significantly affect the bond strength of Bioceramic filling materials.
The growing demand for sustainable and high-performance asphalt binders has prompted the exploration of waste-derived modifiers. This study investigates the performance enhancement of Natural Asphalt (NA) using Sugarcane Molasses (SM) and Waste Engine Oil (WEO). The modified blends were prepared by partially replacing 50 % NA with varying proportions of SM and WEO ranging from 10 % to 40 % of the total weight of NA. Comprehensive testing was conducted, including penetration, softening point, ductility, viscosity, Bending Beam Rheometer (BBR), Multiple Stress Creep Recovery (MSCR), Energy Dispersive X-ray Spectroscopy (EDX), Fourier Transform Infrared (FTIR) spectroscopy, and Scanning Electron Microscopy (SEM). The results demonstrated that
... Show MoreCocoon of larva
The main aim of this study was to molecular identification and determine the antagonistic impact of rhizosphere Trichoderma spp. against some phytopathogenic fungi, including (Magnaporthe grisea) pyricularia oryzae, Rhizoctonia solani and Macrophomina phasolina. Four Trichoderma isolates were isolated from rhizosphere soils of the different host plants in different locations of Egyptian governorates. The morphological characterization of isolated Trichoderma as well as using of (ITS1-5.8S-ITS2) ribosomal gene sequence acquisition and data analyses. By comparing the results of DNA sequences of ITS region, the fungi represented one isolate were positively identified as T. asperellum (1 isolate T1) and one as T. longibrachiatum (1 isolate T2)
... Show MoreIn this work, composite materials were prepared by mixing different concentrations of ferrites with polyacrylonitrile (PAN) polymer. Using the electrospinning technique, these composites were deposited on a p-type silicon wafer. The prepared samples demonstrated nanofibers in both pure PAN polymers and their composites with ferrite. Prior to examining the humidity sensing effectiveness with a percentage of relative humidity at a frequency of 10 kHz, based on ambient temperature and a relative humidity range of 50–100%, the composite nanofibers demonstrated stronger humidity sensing compared to the pure PAN nanofibers, which demonstrated a powerful resistance response. More precisely, the PAN@ferrite nanocomposite showed a broad adsorption
... Show MorePseudomonas aeruginosa is a Gram-negative opportunistic pathogen and a model bacterium for studying virulence and bacterial social traits. While it can be isolated in low numbers from a wide variety of environments including soil and water, it can readily be found in almost any human/animal-impacted environment. It is a major cause of illness and death in humans with immunosuppressive and chronic conditions, and infections in these patients are difficult to treat due to a number of antibiotic resistance mechanisms and the organism’s propensity to form multicellular biofilms. One hundred twenty clinical samples and forty hospital environmental samples (various sources) were collected from hospitals in Baghdad city during the period from Oc
... Show MoreThe meteorite with a single total mass of 630 gm as a visible meteorite has fallen on 22 March 2021, at 10:00 a.m. in Al-Sherqat subdistrict within Salah Al-Din, northern Iraq; and therefore, was named Al-Sherqat meteorite by the authors. It is characterized by a uniform structure of coherent and medium degree of malleability. It is of a well-crystalline structure and not homogeneous in composition. The Al-Sherqat meteorite is composed of metallic phases of 7.6 gm/cm3 density exhibiting an oriented intergrowth of kamacite (α-FeNi) with taenite showing a Widmanstätten pattern on an etched polished section with the finest octahedrite kamacite bandwidth of less than 0.2 mm. It is composed of Fe (86.9 wt%), Ni (9.63 wt%), P (1.31 wt%)
... Show More