Background: Contact between implant material and bones must be strong and fast creation, to fulfill these properties appropriate surface modifications must apply on used implants. In this contribution; double surface modifications are applied on Ti-6Al-4V alloy to accelerate osseointegration. Materials and methods: Anodic process is utilized to create titania nanotubes (TNTs) on the screws made from Ti-6Al-4V alloy. These implants were coated with nano ZrO2 particles. Second modification was annealing anodized screws at 8000C, and implanted in tibiae of nine adult New Zealand white rabbits. Results: Physical and histological consequences of two surface modifications on Ti-6Al-4V alloy screws were studied. Scanning electron microscope (SEM) images shows inhomogeneous distribution of TNTs on screws surfaces. X-ray diffraction (XRD) patterns illustrate the covering of first group samples with ZrO2 and transformation of Ti to its oxide (Rutile phase) for second group. These pattern shows that TiO2 had higher crystallinity and larger grain size than ZrO2. Atomic Force Microscopy images (AFM) shows the increasing of roughness, grain size and internal diameter of TNTs after annealing process. Coated implant with ZrO2 at 4 month duration shows threads with newly Haversian canal feature. Annealed implant at same duration shows well developed threads, base of implant illustrates bone trabeculae filled the base of implant bed with active osteoblast cells. Conclusion: Modification of implant's surface produced an improvement of osseointegration in comparison to untreated one.
The dielectric constant of most polymers is very low; the addition of TiO2 particles into the polymers provides an attractive and promising way to reach a high dielectric constant. Polymer-based materials with a high dielectric constant show great potential for energy storage applications. Four samples were prepared, one of them was polyurethane (PU) and the other were PU with different weight percent (wt %) of TiO2 (0.1, 0.2, 0.3) powder AFM test was used to distinguish the nanoparticles. The result shows that the most shape of these nanoparticles are spherical and the roughness average is 0.798 nm. The dielectric properties were measured for all samples before and after the exposure to the UV radiation. The result illustrates that the
... Show MoreBackground: The marginal seal is essential for sealant success because penetration of bacteria under the sealant might allow caries onset or progression. The aim of the present study was to estimate and compare the microleakage of pit and fissure sealant after various methods of occlusal surface preparation. Materials and methods: Thirty non-carious premolars extracted for orthodontic reasons were equally divided into three groups. In group one, occlusal fissures were opened with round carbide bur, in group two, occlusal surfaces of the teeth were cleaned with a dry pointed bristle brush and samples of group three were cleaned with a slurry of fine flour of pumice in water using rubber cup. Then fissures of all teeth were etched using 35% p
... Show MoreThe synthesized ligand (3-(2-amino-5-(3,4,5-tri-methoxybenzyl)pyrimidin-4-ylamino)-5,5-dimethylcyclohex-2-enone] [H1L1] was characterized via fourier transform infrared spectroscopy (FTIR), 1H, 13C – NMR, Mass spectra, (CHN analysis), UV-vis spectroscopic approaches. Analytical and spectroscopic techniques like chloride content, micro-analysis, magnetic susceptibility UV-visible, conductance, and FTIR spectra were used to identify mixed ligand complexes. Its (ML13ph) mixed ligand complexes [M= Co (II), Ni (II), Cu (II), Zn (II), and Cd (II); (H1L1) = β-enaminone ligand=L1 and (3ph) =3-aminophenol= L2]. The results demonstrate that the complexes are produced with a molar ratio of M: L1:L2 (1:1:1). To generate the appropriate compl
... Show MoreBackground: In dentistry, dentist takes the advantages of soft lining materials due to the viscoelastic properties. The major problem is the adhesion of the soft liner with the denture base material. Materials and Methods: Heat cured of high impact acrylic resin specimens prepared with dimensions 75x13x13mm for shear bond strength test, soft lining material (Refit and Mollosil) with a 3-mm thickness and used to join each two acrylic blocks. Also four specimens with the same previous dimensions utilized for chemical and physical surface analysis. The specimens grouped as control (without plasma) and experiment (with oxygen plasma) treated high impact acrylic specimens. Results: Plasma treatment increased the shear bond strength for both Refi
... Show MoreAs contemporary security requires the formulation of a comprehensive strategy based on multidimensional sub-strategies (economic, developmental, social, cybersecurity, military,and diplomatic dimensions to achieve so-called sustainable security and address the unconventional challenges that worsened with the turn of the twenty-first century and concerned with violent extremism, often leading to terrorism, Iraq, despite the reversal of the terrorist group ISIS in 2017, seems urgently needed to formulate effective strategies to counter violent extremism, Violent extremism has multiple internal and external reasons. These causes have increased due to local, regional, and international causes. Violent extremist factors began with the outbreak o
... Show MoreBackground: Acne vulgaris is one of the top three most commonly encountered dermatological problems worldwide in both primary and secondary care. Human keratinocytes express functional TLR2 heterodimers. An increased expression of TLR2 was detected in the epidermis of inflammatory acne lesions, as observed in normal skin; the expression level increased with the degree of differentiation of the keratinocytes. TLR2 expression is upregulated in inflammatory acne lesions and induced by C. acnes. The current study conducted to assess the oral isotretinion treatment effect on the acne vulgaris patients by evaluated the Toll Like Receptor 2 as a major immune system marker in Acne vulgaris immune re
... Show More