Background: The treatment of dental tissues proceeding to adhesive procedures is a crucial step in the bonding protocol and decides the clinical success ofrestorations. This study was conducted in vitro, with the aim of evaluating thenanoleakage on the interface between the adhesive system and the dentine treated by five surface modalities using scanning electron microscopy and energydispersiveX-ray spectrometry. Materials and methods: Twenty five extracted premolars teeth were selected in the study. Standardized class V cavities were prepared on the buccal and lingual surfaces then the teeth divided into five main groups of (5 teeth in each group n=10) according to the type of dentine surface treatment that was used: Group (A): dentine was conditioning with Er, Cr: YSGG laser. Group (B): dentine was conditioning with (Er, Cr: YSGG laser + acid). Group (C): dentine was conditioning with (acid + Er, Cr: YSGG laser). Group (D): dentine was conditioning with acid etch. Group (E): dentine was conditioning with acid + 10% sodium hypochlorite. For All the teeth SBMP adhesive were used and restored with Z250 composite restoration then all specimens were subjected to thermocycling 500 cycles, at 5° to 55 °C. The teeth were soaked in silver nitrate suspension. Then the teeth sectioned bucco-lingually across the centre of the restorations. The specimens were characterized using scanning electron microscopy and the amount of nanoleakage was measured by EDX spectro-analysis to identify the existence of metallic silver particles. Results: Data were analysed statistically by one way ANOVA test and (LSD) Tests. The results showed that there were statistically highly significant differences among all groups of the present study.The resultshowed that the acid and laser (group III) exhibited the lowest mean value of nanoleakage at around (6.14 %), whereas the highest mean value of nanoleakage (12.83 %) was determined by the only acid (group IV). Conclusions: Treating the acid etched dentine with Er: Cr: YSGG laser showed promising results as it exhibits lowest amount of nanoleakage of the adhesive bonding system.
Background: Determination of local bone mineral density (BMD) immediately after implant insertion play an important role in implant success rate, may offer comprehensive description of the bone, and give enough information to the surgeon prior to implant insertion and at follow up status. The aim of the present study is to evaluate the changes of local bone density in the dental implant recipient sites by using computerized tomography. Material and method: The sample consisted of (20) dental implants recipient sites, bone density assessment was done twice, immediately after implants insertion and after six months. Results: The mean HU of the bone around the implant insertion site, immediately after implant placement was 552.28 HU, and inc
... Show MoreThe depletion of petroleum reserves and increasing environmental concerns have driven the development of eco-friendly asphalt binders. This research investigates the performance of natural asphalt (NA) modified with waste engine oil (WEO) as a sustainable alternative to conventional petroleum asphalt (PA). The study examines NA modified with 10%, 20%, and 30% WEO by the weight of asphalt to identify an optimal blend ratio that enhances the binder’s flexibility and workability while maintaining high-temperature stability. Comprehensive testing was conducted, including penetration, softening point, viscosity, ductility, multiple stress creep recovery (MSCR), linear amplitude sweep (LAS), energy-dispersive X-ray spectroscopy (EDX), F
... Show MoreThe present study explores the solar-induced photocatalytic degradation of reactive red (RR) and reactive turquoise (RT) dyes in a single system using TiO2 immobilized in xanthan gum (TiO2/XG), synthesized using the sol–gel dip-coating technique for direct precipitation. SEM-EDX, XRD, FTIR, and UV–Vis were used to assess the characteristics of the resulting catalyst. Moreover, the effects of different operating parameters, specifically pH, dye concentration, TiO2/XG concentration, H2O2 concentration, and contact time, were also investigated in a batch photocatalytic reactor. The immobilized TiO2/XG catalyst showed a slight adsorption degradation efficiency and then improved the RR and RT dye degradation activity (92.5 and 90.8%
... Show MoreTotal dissolved solids are at the top of the parameters list of water quality that requires investigations for planning and management, especially for irrigation and drinking purposes. If the quality of water is sufficiently predictable, then appropriate management is possible. In the current study, Multiple Linear Regression (MLR) and Artificial Neural Network (ANN) models were used as indicators of water quality and for the prediction of Total Dissolved Solids (TDS) along the Tigris River, in Baghdad city. To build these models five water parameters were selected from the intakes of four water treatment plants on the Tigris River, for the period between 2013 and 2017. The selected water parameters were Total Dissolved Solids (TDS
... Show MoreThere is a suggestion that an antidiuretic hormone-induced decrease in diuresis might contribute to the rapid relief of the acute pain in renal colic. This study was designed to evaluate the efficacy of desmopressin nasal spray compared with diclofenac given intramuscularly in patients with acute renal colic. The study included 75 patients randomized into three different groups; group A received desmopressin (40 μg, nasal spray), group B diclofenac (75 mg) intramuscularly and group C, both desmopressin and diclofenac. Pain was assessed using a visual analogue scale (a 10-cm horizontal scale ranging from `no pain' to `unbearable pain') at baseline, 10, 20 and 30 min after administering t
... Show MoreZSM-5 zeolite was synthesis under hydrothermal conditions at 175oC. The synthesis parameters have been investigated to find optimum synthesis method. Firstly, the crystallization time has been investigated to find the optimum crystallization time. Also, the ageing time was studied. The morphology, structure, and composition of the synthesized ZSM-5 zeolite were characterized using scanning electron microscopy (SEM), pH meter, viscometer, and X-ray powder diffraction (XRD). The bulk Si/Al ratio of ZSM-5 zeolite was in the range of 9.5—11.7. The synthesized ZSM-5 zeolite with appropriate ageing time could adjust crystal size and degree of the crystallinity. The crystal size of ZSM-5 zeolite obtained at an agei
... Show MoreIn this study, industrial fiber and polymer mixtures were used for high-speed impact (ballistic) applications where the effects of polymer (epoxy), polymeric
mixture (epoxy + unsaturated polyester), synthetic rubber (polyurethane), Kevlar fiber, polyethylene fiber (ultra High molecular weight) and carbon fiber.
Four successive systems of samples were prepared. the first system component made of (epoxy and 2% graphene and 20 layer of fiber), then ballistic test was
applied, the sample was successful in the test from a distance of 7 m. or more than, by using a pistol personally Glock, Caliber of 9 * 19 mm. The second
system was consisting of (epoxy, 2% graphene, 36 layers of fiber and one layer of hard rubber), it was succeeded