Background: With the increased in the demands of adult orthodontics, the challenge of direct bonding to non-enamel surface (zirconium) had been increased. The present study was carried out to compare the shear bond strength of three different brackets (stainless steel, sapphire and composite) bonded to zirconium surface and study the mode of bond failure. Materials and methods: The sample was comprised of 30 models (8mm *6mm*1.5mm) of full contour zirconium veneers. They were divided into three groups according to the brackets type; all samples were treated first by sandblast with aluminum oxide particle 50 µm then coated by z-prime plus primer. A central incisor bracket of each group was bonded to the prepared zirconium surface with light cure adhesive resin (Transbond TM XT, 3M Unitek, USA). Shear bond strength was measured by using Tinius Olsen universal testing machine at crosshead speed of 0.5\min. After debonding, each bracket and zirconium surface were examined using magnifying lens and adhesive remnant index was recorded. The difference in shear bond strength between main groups was analyzed by using ANOVA at p≤0.05. Results: The results revealed high significant difference among all tested groups and the highest value was for sapphire brackets (7.49±1.45 Mpa) of all groups followed by stainless steel brackets (6.46±1.43Mpa) and composite brackets had the least value (4.35±0.72). Non-significant difference in the site of bond failure among all groups of brackets and zirconium-adhesive interface failure (score III) was the predominant. Conclusion: the new zirconium prime plus primer can be successfully used in bonding stainless steel and sapphire brackets to zirconium surface.
Abstract
The research aims to identify the nature of the relationship between the level of debt used and economic value added of companies listed on the Iraq Stock Exchange under the Contrast sizes of these companies , The research addressed the theoretical concepts associated with each of the debt financing , economic added value and Organization size With the use of financial techniques in the practical side to measure these variables, The research community Represent of the shareholding companies listed on the Iraq Stock Exchange with a choice of intentionally sample of 24 joint stock companies representing 
... Show MoreThis paper reports the effect of Mg doping on structural and optical properties of ZnO prepared by pulse laser deposition (PLD). The films deposited on glass substrate using Nd:YAG laser (1064 nm) as the light source. The structure and optical properties were characterized by X-ray diffraction (XRD) and transmittance measurements. The films grown have a polycrystalline wurtzite structure and high transmission in the UV-Vis (300-900) nm. The optical energy gap of ZnO:Mg thin films could be controlled between (3.2eV and 3.9eV). The refractive index of ZnO:Mg thin films decreases with Mg doping. The extinction coefficient and the complex dielectric constant were also investigate.
A Schiff base ligand (L) was synthesized via condensation of N-( 1-naphthyl) ethylenediamine dihydrochloride with phthalaldehyde. The ligand was characterized by FT-IR, UV–Vis, 1H NMR, mass spectrometry, and elemental analysis (C, H, N). Five metal complexes (Co(II), Ni(II), Cu(II), Zn(II), and Cd(II)) were prepared with the ligand in a 1:1 (M:L) ratio using an aqueous ethanol solution. The complexes were characterized by FT-IR, UV–Vis, mass spectrometry, and elemental analysis (C, H, N). Additionally, 1H NMR spectroscopy was employed for Cd(II) complex. Antimicrobial activity of the ligand and its metal complexes against pathogenic bacteria (K. pneumoniae, E. coli, S. aureus, and S. epidermidis) and fungus (C. albicans) were evaluated
... Show MoreA Schiff base ligand (L) was synthesized via condensation of
In this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In additio
... Show More