Background: Coated aesthetic archwires are currently the existing solutions for the esthetic problem, but the color of these archwires tends to change overtime. This study was aimed to evaluate the color stability of different types of esthetic archwires from four different companies at different time periods after immersion of two different staining drinks which are tea and Pepsi cola. Materials and methods: 48 specimens were prepared, each specimen contains 10 aesthetic archwires; and were divided according to type of solution into two groups: A (tea) &B (Pepsi cola); each group contained 24 specimens (12 specimens were immersed in the staining solution as 4 specimens for each time intervals and 12 specimens were immersed in distilled water as control group). Each subgroup contains one specimen from each company. Color measurements were performed by means of a computed spectrophotometer according to the Commission Internationale de I’Eclairage L*a*b* system, and color changes (ΔE*) and National Bureau of Standards units. Results: Both staining solution caused color change in variable degree and the higher amount of color instability was found for the archwires from the Hubit Company while the least amount of color change was for the archwires from the Orthotechnology Company. Conclusion: The tea caused highly significant change on the aesthetic archwires which is higher than the effect of the Pepsi cola. Key words: Color stability, aesthetic archwires, staining drinks.
This study was design to investigate the dimensional stability of heat-activated acrylic resin with different methods of flask cooling (15 minutes rapid cooling, one hour bench cooling, four hours delayed deflasking, and 24 hours delayed deflasking) at different time intervals (immediately, two days, seven days, 30 days) after deflasking. Heat-activated acrylic resin was used to prepare acrylic samples. Then, measurement of the distances where achieved between the centers of selected marks in the acrylic samples. They were measured at different time intervals for different methods of flask cooling. The results showed that the group samples of the four hours and 24 hours of delayed deflasking was insignificantly different from the control an
... Show MoreBackground: The primary stability of the dental implant is a crucial factor determining the ability to initiate temporary implant-supported prosthesis and for subsequent successful osseointegration, especially in the maxillary non-molar sites. This study assessed the reliability of the insertion torque of dental implants by relating it to the implant stability quotient values measured by the Osstell device. Material and methods: This study included healthy, non-smoker patients with no history of diabetes or other metabolic, or debilitating diseases that may affect bone healing, having non-restorable fractured teeth and retained roots in the maxillary non-molar sites. Primary dental implant stability was evaluated using a torque ratc
... Show MoreBackground: To investigate the effect of different types of storage media on enamel surface microstructure of avulsed teeth by using atomic force microscope.Materials and methods : Twelve teeth blocks from freshly extracted premolars for orthodontic treatment were selected . The study samples were divided into three groups according to type of storage media :A-egg white , B- probiotic yogurt , and C-bovine milk . All the samples were examined for changes in surface roughness and surface granularity distribution using atomic force microscope, at two periods: baseline, and after 8 hours of immersing in the three types of storage media. Results: Milk group had showed a significant increase in the mean of the roughness values at
... Show MorePlant regeneration protocols were developed for medicinally important anise (Pimpinella anisum L.) that successfully achieved from seeds. Seeds were sterilized and inoculated on Murashige and Skoog (MS) medium with and without gibberellins (GA3) until full germination. The highest percentage of germination (100%) was recorded on MS medium treated with 2.0 mg/L GA3 after 7 days. For shoot proliferation, different concentrations of 6- benzyl adenine BA (1, 1.5, 2 mg/L) were used. To enhance shoot induction, 0.1 mg/L of naphthalene acetic acid (NAA) and 0.01 mg/L of thidiazuron (TDZ) were tested along with BA. Direct regenerated shoots were obtained on MS medium supplemented with BA alone (2mg/L) which gave (7shoot/explant), while the presence
... Show MoreBackground: one of the complications of power bleaching is surface roughness of enamel which increases the possibility of post bleaching teeth discoloration. The aim of the present study is to evaluate the effect of toothpaste containing nano hydroxyapatite, NovaMin and kin sense fluoride on surface roughness of human tooth enamel after laser bleaching with 35% hydrogen peroxide bleaching gel. Materials and Methods: Twenty human enamel incisors were cleaned and their labial surface polished up to #1200, then categorized into four equal groups; first group kept without bleaching as a control group, while the remaining three experimental groups were bleached with 35% hydrogen peroxide, and each group treated with a restore paste containing o
... Show MoreObjective. This study aimed to evaluate and compare the force degradation of two types of elastomeric chains following different periods of immersion in zinc-containing mouthwashes. Materials and Methods. Four hundred and forty pieces of Elasto-Force and Super Elasto-Force elastomeric chains were divided into two control and eight experimental groups. The pieces were stretched to 25 mm on pins mounted on an acrylic block and stored in distilled water at 37°C. The experimental groups were immersed in four different types of mouthwash for one minute twice a day throughout the test period. Ten continuous thermocycles per day between cold and hot water baths (5–55°C) were carried out. Forces were measured at six-time intervals (in
... Show MoreThe study is carried out by using personal dosimeters (film badge). The films are irradiated to absorbed dose of range (0.01-10000 rad). The calibration curves are drawn by using the ordinary method taking into account the filtration effects in three regions (D (Pb/Sn),D(Du),D(300). The calibration films are stored in ambient condition. It is found that the optical density increases, which is attributed to the photodegradation of the films may induce localized states in the energy gap causing increasing in optical absorption, but optical density decreases, which attributed to the photodegradation of the films may cause some cracks at the film surface during the first month, whereas at the rest months we see clear stability in optical d
... Show MoreLeishmaniosis is a tropical neglected parasitic disease that is endemic in many countries, including Middle East, with no existing effective vaccines. The bite of female sand-fly transmits the causative agent, Leishmania spp., to humans. High toxicity, resistance and treatment failure of the available chemotherapy against visceral leishmaniosis demands the investigation of new anti-leishmanial compounds. Lupeol is a form of triterpene isolated from several medicinal plants and possesses an antimicrobial property. In this study, cytotoxic effect of lupeol was screened against the mammalian amastigotes form and insect promastigote form of Leishmania donovani, following three cycles of incubation at different concentrations by MTT assay. Resul
... Show MoreBackground: Even the wide use of dental implants, still there is a proportion of implants are failed due to infection. Much considerable attention has been paid to modify the implant surface. Coating of dental implant with a biocomposite material of suitable properties can improve osseointegration. And this is the main concern of this study. The aim of present study was to evaluate the use of a biocomposite coating of dental implant with (ceramic nano Al2O3 and metalic AgNo3) on the bond strength at bone – implant interface and tissue reaction. Materials and methods: A total number of forty-eight screws, CpTi dental implant used in this study. Half of these screws were coated with a biocomposite material of nano (Al2O3and AgNo3), thi
... Show MoreObjective: In order to evaluate the effect of different typed of Separating Medium on the roughness of the fitted
tissue surface of acrylic denture base.
Methodology: Chosen three types of separating medium (Group A Tin foil), (Group B Detery Isolant),(Group C
Cold Mould Seal),used 30 samples of hot cure acrylic resin ,10 samples for each group, after complete curing of
these samples , Profilometer device was used to measure the surface roughness of each sample in all groups.
Results: Using One Way ANOVA Test and LSD test, the results were highly significant in differences among all
groups. Although (Group A) showing lest roughness, (Group B) showing a satisfactory result of roughness, While
(Group C) Showing the hig