Background: Even the wide use of dental implants, still there is a proportion of implants are failed due to infection. Much considerable attention has been paid to modify the implant surface. Coating of dental implant with a biocomposite material of suitable properties can improve osseointegration. And this is the main concern of this study. The aim of present study was to evaluate the use of a biocomposite coating of dental implant with (ceramic nano Al2O3 and metalic AgNo3) on the bond strength at bone – implant interface and tissue reaction. Materials and methods: A total number of forty-eight screws, CpTi dental implant used in this study. Half of these screws were coated with a biocomposite material of nano (Al2O3and AgNo3), this was done by using electrophoretic deposition method (EFD). In invitro part of the study, analysis of the coated surface was done using: X ray diffraction (XRD), atomic force microscope (AFM), Energy Dispersive X-ray spectroscopy (EDX), Optical microscopy and Scanning electron microscope (SEM). In invivo part of study, 10 white male New Zealand rabbits were used, and a screw type of dental implant [uncoated and coated with nano (Al2O3and AgNo3)] were implanted in each tibia of rabbit. Then biomechanical and Histological test were performed after 2 and 4 weeks healing intervals. Results: The results of biomechanical test showed a higher torque mean values of (M+SD):(14.91N.cm+2.7)and (22.5 N.cm +5.31) after 2 and 4 weeks respectively. In histological examination of coated screws at 2 weeks, there isa bone trabeculae occupies a base of implant bed with osteoblast andosteocyte. At 4 weeks, there is a progress in the healing process around dental implant, and this includes: -new bone with haversian canals, osteoblast and osteocyte. Conclusion: Biocomposite coating of dental implant with Alumina and silver nitrate can be made by electrophoretic deposition method (EPD), and a multifunctional surface has been created. Keywords: Electrophoretic Deposition, alumina, screw Dental Implants, torque.
Background: Prophylaxis methods are used to mechanically remove plaque and stain from tooth surfaces; such methods give rise to loss of superficial structure and roughen the surface of composites as a result of their abrasive action. This study was done to assess the effect of three polishing systems on surface texture of new anterior composites after storage in artificial saliva. Materials and methods: A total of 40 Giomer and Tetric®N-Ceram composite discs of 12 mm internal diameter and 3mm height were prepared using a specially designed cylindrical mold and were stored in artificial saliva for one month and then samples were divided into four groups according to surface treatment: Group A (control group):10 specimens received no surfa
... Show MoreThe aim of this study was to evaluate the effects of local application of bisphosphonate gel and recombinant human bone morphogenic protein 2 gel, on titanium dental implant stability and marginal bone level. Twenty-seven patients with upper and lower missing posterior tooth/teeth were included in the study with a total of 71 implants that were used for rehabilitation. The implants were randomly divided into 4 groups: 3 study groups and 1 control. Group1; local application of bisphosphonate gel, group 2; local application of recombinant human bone morphogenic protein 2 gel, group 3; local application of a mixed formula of both gels. The gel application was immediately preimplant insertion, group 4; implant insertion without application of a
... Show MoreIntroduction: We aimed to assess the impact of adhesive and wires types on the tensile bond strength of fixed lingual retainers. Methods: A total of 160 intact bovine teeth were collected, cleaned, stored in 25% sodium hypochlorite, and randomly assigned to two groups based on the adhesive type: a two-step adhesive and a one-step adhesive. Each group was further divided into four subgroups based on the type of lingual retainer wire, which included (A) 8-strand braided stainless steel wire, (B) three-strand titanium retainer wire, (C) stainless steel chain, and (D) fiber-reinforced retainer. A tensile bond strength test was conducted using a universal testing machine at a controlled speed of 10 mm/min. Result: The 8-strand braided stainles
... Show MoreObjective. This study aimed to evaluate and compare the force degradation of two types of elastomeric chains following different periods of immersion in zinc-containing mouthwashes. Materials and Methods. Four hundred and forty pieces of Elasto-Force and Super Elasto-Force elastomeric chains were divided into two control and eight experimental groups. The pieces were stretched to 25 mm on pins mounted on an acrylic block and stored in distilled water at 37°C. The experimental groups were immersed in four different types of mouthwash for one minute twice a day throughout the test period. Ten continuous thermocycles per day between cold and hot water baths (5–55°C) were carried out. Forces were measured at six-time intervals (in
... Show MoreBackground: Molars and premolars are considered as the most vulnerable teeth of caries attack, which is related to the morphology of their occlusal surfaces along with the difficulty of plaque removal. different methods were used for early caries detection that provide sensitive, accurate preoperative diagnosis of caries depths to establish adequate preventive measures and avoid premature tooth treatment by restoration. The aim of the present study was to evaluate the clinical sensitivity and specificity rates of DIAGNOdent and visual inspection as opposed to the ICDAS for the detection of initial occlusal caries in noncavitated first permanent molars. Materials and Methods: This study examined 139 occlusal surface of the first permanent
... Show MoreFrictional resistance occurs whenever sliding happens, negatively impacting treatment outcomes and duration. It is a clinical challenge and must be dealt with efficiently to achieve the best orthodontic results. Aims of this study: compare and evaluate the static frictional forces under the wet condition to mimic the oral environment produced by using a polycrystalline ceramic bracket, monocrystalline ceramic bracket, 0.014 of an inch nickel-titanium (Rhodium coated archwires, and ilusio aesthetic archwires), and 0.019 x 0.025 of an inch stainless steel (Rhodium coated archwires, and ilusio aesthetic archwires). Ninety-six aesthetic brackets (48 monocrystalline and 48 polycrystalline brackets) were used and stored in different incub
... Show MoreDue to the advantages over other metallic materials, such as superior corrosion resistance, excellent biocompatibility, and favorable mechanical properties, titanium, its alloys and related composites, are frequently utilized in biomedical applications, particularly in orthopedics and dentistry. This work focuses on developing novel titanium-titanium diboride (TiB2; ceramic material) composites for dental implants where TiB2 additions were estimated to be 9 wt.%. In a steel mold, Ti-TiB2 composites were fabricated using a powder metallurgy technique and sintered for five hours at 1200 °C. Microstructural and chemical properties were analyzed by energy dispersive X-ray spectroscopy (EDX), scanning electron microscopy (SEM), and X-ra
... Show More