Background: Even the wide use of dental implants, still there is a proportion of implants are failed due to infection. Much considerable attention has been paid to modify the implant surface. Coating of dental implant with a biocomposite material of suitable properties can improve osseointegration. And this is the main concern of this study. The aim of present study was to evaluate the use of a biocomposite coating of dental implant with (ceramic nano Al2O3 and metalic AgNo3) on the bond strength at bone – implant interface and tissue reaction. Materials and methods: A total number of forty-eight screws, CpTi dental implant used in this study. Half of these screws were coated with a biocomposite material of nano (Al2O3and AgNo3), this was done by using electrophoretic deposition method (EFD). In invitro part of the study, analysis of the coated surface was done using: X ray diffraction (XRD), atomic force microscope (AFM), Energy Dispersive X-ray spectroscopy (EDX), Optical microscopy and Scanning electron microscope (SEM). In invivo part of study, 10 white male New Zealand rabbits were used, and a screw type of dental implant [uncoated and coated with nano (Al2O3and AgNo3)] were implanted in each tibia of rabbit. Then biomechanical and Histological test were performed after 2 and 4 weeks healing intervals. Results: The results of biomechanical test showed a higher torque mean values of (M+SD):(14.91N.cm+2.7)and (22.5 N.cm +5.31) after 2 and 4 weeks respectively. In histological examination of coated screws at 2 weeks, there isa bone trabeculae occupies a base of implant bed with osteoblast andosteocyte. At 4 weeks, there is a progress in the healing process around dental implant, and this includes: -new bone with haversian canals, osteoblast and osteocyte. Conclusion: Biocomposite coating of dental implant with Alumina and silver nitrate can be made by electrophoretic deposition method (EPD), and a multifunctional surface has been created. Keywords: Electrophoretic Deposition, alumina, screw Dental Implants, torque.
This research studies the effect of addition of some nanoparticles
(MgO, CuO) and grain size (30,40nm) on some physical properties
(impact strength, hardness and thermal conductivity) for a matrix
blend of epoxy resin with SBR rubber. Hand –Lay up method was
used to prepare the samples. All samples were immersed in water for
9 weeks.
The Results showed decreased in the values of impact strength and
hardness but increased the coefficient of thermal conductivity.
Background: Sealers should demonstrate adhesive properties to dentin, decreasing the chance of endodontic treatment failure. Increased adhesive properties to dentin may lead to greater strength of the restored tooth, which may provide greater resistance to tooth fracture and clinical longevity of an endodontically treated tooth. The aim of this study was to evaluate the shear bond strength of Bioceramic iRoot SP sealer, AH plus sealer and Apexit plus sealer in absence or presence of smear layer using push out bond strength test. Materials and Methods: Sixty straight single roots of the mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments to achieve tapered canal walls, instrumenta
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreThis in vivo study was conducted to investigate the effect of different concentrations of ozonated water on experimentally skin infection with some of bacterial isolates (Pseudomonas aeruginosa and Staphylococcus aureus ) which Showed dermal infection in experimental animals after 48 hours of exposure to these Microorganisms. Results revealed that ozone has the power to accelerated the healing process depending on the perfect concentration of ozonated water used and the severity of infection & nature of causative agent , in which the recovering period was 7 days for the infection caused by P. aeruginosa and 5 day for S.aureus by using the concentration 60 µg/ml . Results also indicated in this study the stimulated effect of O
... Show MoreThe compound chalcon originally is extracted form some plant and herbs, the studies of the antiviral activity of this compound were done in two cell line cultures the L2OB and RD, the compound relatively non toxic to both cell lines of the concentration of 32?g/ml or less ,the compound have significantly anti poliovirus activity in both L2OB cell line and RD cell line, we find that the concentration of 0.03 ?g/ml or more inhibit the 100TCDID50 of the poliovirus .The therapeutic index(TI)used in this study to evaluate the drug activity ,( TI is the ratio of dose of drug which is just toxic to the cells to the does which is just inhibit the viral multiplication, if this index more than one the margin of safety of drug is according great ) .In
... Show MoreABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreBackground: Pit and fissure sealant have been considered an outstanding adjunct to oral health care in the decrease of occlusal caries onset and low progression. The aims of this in vitro study were to evaluate the marginal microleakage of three different types of fissure sealants (SDI, Tg and tetric N-flow) by time interval, one day and 45 days, in the presence or absence of bonding agent among maxillary and mandibular teeth. Materials and methods: Seventy two sound human maxillary and mandibular first premolar teeth were collected which were free from obvious carious lesions. The teeth were randomly divided into two main equal groups, group (1) and group (2), each group consists of (36) teeth involving equal numbers of maxillary and mandi
... Show MoreAbstract
In this investigation, Al2O3 nano material of 50nm particles size were added to the 6061 Al aluminium alloy by using the stir casting technique to fabricate the nanocomposite of 10wt% Al2O3. The experimental results observed that the addition of 10wt% Al2O3 improved the fatigue life and strength of constant and cumulative fatigue. Comparison between the S-N curves behaviour of metal matrix (AA6061) and the nanocomposite 10wt% Al2O3 has been made. The comparison revealed that 12.8% enhancement in fatigue strength at 107cycles due to 10wt% nano reinforcement. Also cumulative fatigue l
... Show More