High temperature superconductors with a nominal composition HgBa2Ca2Cu3O8+δ
for different values of pressure (0.2,0.3, 0.5, 0.6, 0.9, 1.0 & 1.1)GPa were prepared by
a solid state reaction method. It has been found that the samples were semiconductor
P=0.2GPa.while the behavior of the other samples are superconductor in the rang
(80-300) K. Also the transition temperature Tc=143K is the maximum at P is equal to
0.5GPa. X-ray diffraction showed a tetragonal structure with the decreasing of the
lattice constant c with the increasing of the pressure. Also we found an increasing of
the density with the pressure.
An experiment was conducted to study the effect of the sprayer type according to the source of power and the size of the spray nozzle concerning the quality of the spray produced and fuel consumption.Two types of sprayers were used: a conventional boom sprayer (S1) and a modified (electrified) boom sprayer (S2), along with three sizes of the XR TeeJet 110 spray nozzle (N). The following technical performance indicators were examined: Density of coverage (drops/cm2) using ImageJ software, a 600dpi business card scanner, specifically the ScanShell 800N by CSSN, Inc, and water-sensitive paper (WSP), rate of spray nozzles discharge (ml/min), and fuel consumption (liters/hectare) using a c
The effect of substitution of Ni on Cu in (Bi0.8Pb0.2)2(Sr0.9Ba0.1)2 Ca2Cu3-x Nix O10+? for (x=0,0.1….1,2,3) superconductor system and sintering time has been investigated .The samples were prepared by solid-state reaction methods. The results show that the optimum sintering temperature is equal to 850 ºC, and the sintering time is equal to 140 h. The highest transition temperature (Tc) obtained for (Bi0.8Pb0.2)2(Sr0.9Ba0.1)2 Ca2Cu3-x NixO10+? composition was 113 with x=0.8 Phase analyses of the samples by X-ray diffraction (XRD) analysis showed an orthorhombic structure with a high Tc phases (2223) as a dominant phase and low Tc phase (2212) in addition to some impurity phases.
The pure and Sb doped GeSe thin films have been prepared by thermal flash evaporation technique. Both the structural and optical measurement were carried out for as deposited and annealed films at different annealing temperatures.XRD spectra revealed that the all films have one significant broad amorphous peak except for pure GeSe thin film which annealed at 573 K, it has sharp peak belong to orthorhombic structure nearly at 2θ=33o . The results of the optical studies showed that the optical transition is direct and indirect allowed. The energy gap in general increased with increasing annealing temperature and decreased with increase the ratio of Sb dopant. The optical parameters such as refractive index, extinction coefficient and r
... Show MoreThe pure and Sb doped GeSe thin films have been prepared by thermal flash evaporation technique. Both the structural and optical measurement were carried out for as deposited and annealed films at different annealing temperatures.XRD spectra revealed that the all films have one significant broad amorphous peak except for pure GeSe thin film which annealed at 573 K, it has sharp peak belong to orthorhombic structure nearly at 2θ=33o. The results of the optical studies showed that the optical transition is direct and indirect allowed. The energy gap in general increased with increasing annealing temperature and decreased with increase the ratio of Sb dopant. The optical parameters such as refractive index, extinction coefficient and real and
... Show MoreThe aim of the present research is concerned with study the effect of UV radiation on the optical properties at wavelengths 254, 365 nm of pure PC and anthracene doping PC films prepared using the cast method for different doping ratio 10-60 mL. Films of pure PC and anthracene doping PC were aged under UV radiation for periods of up to 360 h. It found that the effect of UV radiation at wavelength 254 nm on the optical properties is great than the effect of UV radiation at wavelength 365 nm. Also, it found that the optical energy gap of pure PC and anthracene doping PC films is stable against radiation.
Vitrifications process one of the important methods to immobilize nuclear waste. In this research nuclear waste (Strontium Oxides) with molecular weight (5%) was immobilized by vitrification methods in two types of borosilicate glass (c-type) which are glass and glass-ceramics. To investigate the physical, chemical and mechanical properties of glass and glass-ceramic after immobilize nuclear waste these samples irradiated by gamma ray radiation. Co-60 was used as gamma a irradiation with dose rate 0.38 kGy/hr for different period of time. It’s found that gamma radiation affected the glass and glass-ceramic properties. From phase analysis by the x-ray diffraction for glass-ceramic samples proved that at doses 343kGy change the cry
... Show MoreMesoporous SBA-15 with nono particle size distribution, different texture properties, and morphologies have been synthesized by controlling the hydrophilic-hydrophobic character during preparation, i.e., the solubility of micelles of pluronic P123 by controlling the charge of PEO hydrophilic-inorganic silica zone using different charge surfactants CTAB (cationic), F68 (nonionic), and SDBS (anionic). Sodium silicate was used as a silica source. Eo20Po70Eo20 co-polymer was used as a template at highly acidic conditions (pH<2). The experiments were characterized using XRD, FTIR, AFM, BET, and FESEM. The XRD and FTIR tests indicated that the SBA-15 is amorphous and free from impurities. The degree of particle dispersion is sequenced
... Show MoreBackground: Dental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60
... Show MoreDental casts come into direct contact with impression materials and other items that are contaminated by saliva and blood from a patient's mouth, leaving the casts susceptible to cross-contamination. The disinfectant solutions of the impression materials cause various adverse reactions. Therefore, disinfection of dental casts may be effective in preventing cross infection. This study was carried out to evaluate the surface hardness, dimensional accuracy, reproduction of details and surface porosity of type III, type IV and type IV extra hard dental stone after immersion in and spray by using SOLO and Sodium hypochlorite disinfectant solutions. Materials and methods: 240 Stone samples were prepared in rubber rings, A total of 60 test block w