Preferred Language
Articles
/
ijp-857
Effect ofweight percentage chopped carbon fibers on the mechanism of cracks propagation for Epoxy composites
...Show More Authors

In this research, the mechanism of cracks propagation for epoxy/ chopped carbon fibers composites have been investigated .Carbon fibers (5%, 10%, 15%, and 20%) by weight were used to reinforce epoxy resin. Bending test was carried out to evaluate the flexural strength in order to explain the mechanism of cracks propagation. It was found that, the flexural strength will increase with increasing the percentage weight for carbon fibers. At low stresses, the cracks will state at the lower surface for the specimen. Increasing the stresses will accelerate the speed of cracks until fracture accorded .The path of cracks is changed according to the distributions of carbon fibers

View Publication Preview PDF
Quick Preview PDF
Publication Date
Mon Dec 01 2014
Journal Name
Journal Of Accounting And Financial Studies ( Jafs )
The Impact of Applying the Percentage of Complete Method or the Complete Contract One on the Taxation of the Long – Term Construction Contracts: بحث تطبيقي في الهيئة العامة للضرائب – قسم الشركات
...Show More Authors

The research aims to shed light on the amount of proceeds annual tax for each of the way the contract total and percentage of completion method - see which is better - as well as the current problems arising from the application method of the contract in full in settling accounts tax - to identify problems - related to postpone settling accounts tax in accordance with the way the contract fully and determine the advantages and disadvantages of each of the methods through practical application , and then use the results as inputs to help in the decision to confirm the continuation of the GCT using a full decade in settling accounts tax for long-term construction contracts or forgo them.

Were the result of research the existence of

... Show More
View Publication Preview PDF
Publication Date
Sun Sep 05 2010
Journal Name
Baghdad Science Journal
Removal of Zinc ions from industrial wastewater with wool fibers
...Show More Authors

In this research, the efficiency of low-cost unmodified wool fibers were used to remove zinc ion from industrial wastewater. Removal of zinc ion was achieved at 99.52% by using simple wool column. The experiment was carried out under varying conditions of (2h) contact time, metal ion concentration (50mg/l), wool fibers quantity to treated water (70g/l), pH(7) & acid concentration (0.05M). The aim of this method is to use a high sensitive, available & cheep natural material which applied successfully for industrial wastewater& synthetic water, where zinc ion concentration was reduced from (14.6mg/l) to (0.07mg/l) & consequently the hazardous effect of contamination was minimized.

View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Tue Sep 10 2013
Journal Name
Nature Communications
Carbon nanotubes on a spider silk scaffold
...Show More Authors

Understanding the compatibility between spider silk and conducting materials is essential to advance the use of spider silk in electronic applications. Spider silk is tough, but becomes soft when exposed to water. Here we report a strong affinity of amine-functionalised multi-walled carbon nanotubes for spider silk, with coating assisted by a water and mechanical shear method. The nanotubes adhere uniformly and bond to the silk fibre surface to produce tough, custom-shaped, flexible and electrically conducting fibres after drying and contraction. The conductivity of coated silk fibres is reversibly sensitive to strain and humidity, leading to proof-of-concept sensor and actuator demonstrations.

View Publication Preview PDF
Scopus (139)
Crossref (137)
Scopus Clarivate Crossref
Publication Date
Sun Jan 13 2019
Journal Name
Iraqi Journal Of Physics
Dielectric properties of Ep\TiO2;Ep\MgO nano composites
...Show More Authors

The Dielectric properties of EP/TiO2 and MgO nanocomposite at
a frequency range of (102-106 Hz) were studied. The composite were
prepared with the state volume ratio (0, 0.05, 0.1) for EP/TiO2 and
MgO respectively. The impedance, dielectric constant and dielectric
loss were found decrease with frequency increase.

View Publication Preview PDF
Crossref
Publication Date
Thu Mar 14 2019
Journal Name
Al-khwarizmi Engineering Journal
Cellulose Fibers Dissolution in Alkaline Solution
...Show More Authors

In this study, NaOH dissolution method was applied to dissolve cellulose fibers which extracted from date palm fronds (type Al-Zahdi) taken from Iraqi gardens. In this process, (NaOH)-solution is brought into contact with the cellulose fibers at low temperature. Experiments were conducted with different concentrations of NaOH (4%, 6%, 8% and12%) weight percent at two cooling bath temperatures (-15 oC) and (-20oC). Maximum cellulose dissolution was 23 wt% which obtained at 8 wt% concentration of NaOH and at cooling bath temperature of -20oC. In order to enhance the cellulose fibers dissolution, the sample was pretreated with Fenton's reagent which consists of

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Sun Jan 02 2022
Journal Name
Al-khwarizmi Engineering Journal
Cellulose Fibers Dissolution in Alkaline Solution
...Show More Authors

In this study, NaOH dissolution method was applied to dissolve cellulose fibers which extracted from date palm fronds (type Al-Zahdi) taken from Iraqi gardens. In this process, (NaOH)-solution is brought into contact with the cellulose fibers at low temperature. Experiments were conducted with different concentrations of NaOH (4%, 6%, 8% and12%) weight percent at two cooling bath temperatures (-15 oC) and (-20oC). Maximum cellulose dissolution was 23 wt% which obtained at 8 wt% concentration of NaOH and at cooling bath temperature of -20oC. In order to enhance the cellulose fibers dissolution, the sample was pretreated with Fenton's reagent which consists of

... Show More
View Publication Preview PDF
Publication Date
Thu Mar 14 2019
Journal Name
Al-khwarizmi Engineering Journal
Cellulose Fibers Dissolution in Alkaline Solution
...Show More Authors

In this study, NaOH dissolution method was applied to dissolve cellulose fibers which extracted from date palm fronds (type Al-Zahdi) taken from Iraqi gardens. In this process, (NaOH)-solution is brought into contact with the cellulose fibers at low temperature. Experiments were conducted with different concentrations of NaOH (4%, 6%, 8% and12%) weight percent at two cooling bath temperatures (-15 oC) and (-20oC). Maximum cellulose dissolution was 23 wt% which obtained at 8 wt% concentration of NaOH and at cooling bath temperature of -20oC. In order to enhance the cellulose fibers dissolution, the sample was pretreated with Fenton's reagent which consists of hydrogen peroxide (H2O2), oxalic acid (C2H2O4) and ferrous sulfate (FeSO4). This

... Show More
Crossref (4)
Crossref
Publication Date
Sat Sep 27 2025
Journal Name
Iraqi Journal Of Science
Synthesis and characterization of some 2-sulphanyl benzimidazole derivatives and study of effect as corrosion inhibitors for carbon steel in sulfuric acid solution
...Show More Authors

This research involves the synthesis of some sulphanyl benzimidazole derivatives (Ia-c), which were prepared from reaction of 2-mercaptobenzimidazole substituted benzyl halide, and structures were identified by spectral methods[FTIR, 1H-NMR and 13C-NMR].These compounds were investigated as corrosion inhibitors for carbon steel in 1M H2SO4 solution using weight loss, potentiostatic polarization methods; obtained results showed that the sulphanyl benzimidazole derivatives retard both cathodic and anodic reactions in acidic media, by virtue of adsorption on the carbon steel surface. This adsorption obeyed Langmuir’s adsorption isotherm. The inhibition efficiency of (Ia-c) ranging between (65-92) %. By using different Ib derivative conc

... Show More
View Publication Preview PDF
Publication Date
Sat Jul 01 2017
Journal Name
Bulletin Of The Iraq Natural History Museum (p-issn: 1017-8678 , E-issn: 2311-9799)
FIRST RECORD OF MYCETOPHAGOUS NEMATODE APHELENCHUS AVENAE IN IRAQ WITH DESCRIPTION AND TESTING THEIR PROPAGATION ON DIFFERENT FUNGUS CULTURE
...Show More Authors

Aphelenchus avenae was isolated from the wheat crown in Summel distract- Duhok, Kurdistan region-Iraq infected by a crown rot disease which is caused by Fusarium spp;    wheat's crown culturing on Potato Dextrose Agar (PDA) and incubating at 25°C A. avenae was found associated with fungal culture which meant that fungal nematode was parasitic on crown rot fungi on wheat crown, this species was described for the first time in Iraq.

Fungal Nematode incubated with Fusarium graminearum, F. oxysporum and Verticillium dahliae reproduce in both solid and liquid media, best results of nematode reproduction were recorded on F. graminearum followed by F. oxy

... Show More
View Publication Preview PDF
Scopus (4)
Crossref (6)
Scopus Crossref
Publication Date
Tue Sep 01 2009
Journal Name
Al-khwarizmi Engineering Journal
Analysis of Wave Propagation in Detection of Aorta Dieses Using Lumps Analysis
...Show More Authors

In this paper a theoretical attempt is made to determine whether changes in the aorta diameter at different location along the aorta can be detected by brachial artery measurement.  The aorta is divided into six main parts, each part with 4 lumps of 0.018m length. It is assumed that a desired section of the aorta has a radius change of 100,200, 500%. The results show that there is a significant change for part 2 (lumps 5-8) from the other parts. This indicates that the nearest position to the artery gives the significant change in the artery wave pressure while other parts of the aorta have a small effect.

View Publication Preview PDF